Selective Adsorption Performance of Indium(Ⅲ)with P507/HZ818 Impregnated Resin in Sulfuric Acid System AITranslate

School of Chemistry and Materials Sciences of Ludong University;School of Chemistry and Materials Sciences of Ludong University;School of Chemistry and Materials Sciences of Ludong University;School of Chemistry and Materials Sciences of Ludong University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

P507/HZ818 impregnated resin was prepared with styrene-divinylbenzene copolymer (HZ818) as the carrier and 2-ethylhexyl phosphonic acid mono (2-ethylhexyl) ester (P507) as the extractant, which was characterized by scanning electron microscope (SEM) and infrared spectra (IR). The selective adsorp- tion performance of In (Ⅲ) with the impregnated resin in sulfuric acid system was studied. Static adsorp- tion experimental results show that P507/HZ818 impregnated resin has high selectivity to In ( Ⅲ ) in indi- um and gallium binary system and In/Ga separation coefficient reaches the maximum value when solution pH is 1.2. In multicomponent system of indium, gallium, zinc, iron and copper, the impregnated resin has the best adsorption selectivity to In (Ⅲ ) when solution pH is 0.9. Dynamic adsorption experimental results show that the resin column provides little adsorption capacity for Ga (Ⅲ ) and high selectivity for In ( Ⅲ ) in indium and gallium binary system of pH= 1.2,achieving indium separation from gallium. Indium can be well enriched in indium,gallium,zinc,iron and copper system by controlling solution pH at 0.9.

KeyWords AITranslate

P507 / H Z818 impregnated resin sulfuric acid system selective adsorption indium gallium

1赵婷,郑子恩,董鹏.瓦斯灰回收稀散金属铟的工艺设计[J].稀有金属与硬质合金,2014,42(4):14-16. 被引量:1

2刘军深,蔡伟民.萃淋树脂技术分离稀散金属的研究现状及展望[J].稀有金属与硬质合金,2003,31(4):36-39. 被引量:25

3王俊莲,孙春宝,徐盛明.基于稀土分离的萃淋树脂制备与应用研究[J].中国稀土学报,2015,33(2):129-145. 被引量:16

1陈晓亮,刘军深,高学珍,魏士龙,张妍.伯胺N1923溶剂浸渍树脂吸附In(Ⅲ)的性能及机理[J].鲁东大学学报:自然科学版,2020,36(4):366-370.

1李圣华.钢铁冶金用炭素材料(二)(续9)[J].炭素技术,1997,16(6):42-44.

2走科技进步道路收节能环保之果[J].节能之友,1996(2):22-24.

3蒋新宇,周春山,汤淑芳.N235萃取色谱法分离萃铟余液中锗的研究[J].稀有金属,2002,26(2):116-119. 被引量:1

4宋伟忠.合理控制化学成分 提高烧结矿质量[J].烧结球团,2002,27(3):43-45. 被引量:3

5孙洪兵.竖炉齿辊的改进[J].设备管理与维修,2010(12):34-35.

6陶德宁.提高水冶锌渣中锗的提取率[J].铀矿冶,1993,12(4):241-241.

7张晓峰,李林艳,张覃.盐酸体系中二(2-乙基己基)次膦酸(P227)萃取铁的性能研究[J].湿法冶金,2017,36(3):203-207. 被引量:2

8王红军,刘智勇,刘志宏,李玉虎,李思唯,张文海,李启厚.湿法炼锌窑渣铁精矿中有价组分浸出行为及其机理(英文)[J].中国有色金属学报:英文版,2017,27(4):901-907. 被引量:5

9郭雯,罗章林.离子型稀土矿区溪流水中稀土的回收[J].科技与创新,2017(10):12-14.

10刘向东,行开新,王翔,钟渝,姜玖辉.RH一体式浸渍管真空槽结构与优化[J].工业加热,2017,46(1):62-64. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF843.5[冶金工程—有色金属冶金]

Citation Information:

P507/HZ818 impregnated resin was prepared with styrene-divinylbenzene copolymer (HZ818) as the carrier and 2-ethylhexyl phosphonic acid mono (2-ethylhexyl) ester (P507) as the extractant, which was characterized by scanning electron microscope (SEM) and infrared spectra (IR). The selective adsorp- tion performance of In (Ⅲ) with the impregnated resin in sulfuric acid system was studied. Static adsorp- tion experimental results show that P507/HZ818 impregnated resin has high selectivity to In ( Ⅲ ) in indi- um and gallium binary system and In/Ga separation coefficient reaches the maximum value when solution pH is 1.2. In multicomponent system of indium, gallium, zinc, iron and copper, the impregnated resin has the best adsorption selectivity to In (Ⅲ ) when solution pH is 0.9. Dynamic adsorption experimental results show that the resin column provides little adsorption capacity for Ga (Ⅲ ) and high selectivity for In ( Ⅲ ) in indium and gallium binary system of pH= 1.2,achieving indium separation from gallium. Indium can be well enriched in indium,gallium,zinc,iron and copper system by controlling solution pH at 0.9.

quote

GB/T 7714-2015 [1] XU Cui-ping, LIU Jun-shen, LIU Qing-qing, et al. Selective Adsorption Performance of Indium(Ⅲ)with P507/HZ818 Impregnated Resin in Sulfuric Acid System[J]. Rare Metals and Cemented Carbides, 2017(2): 28-32.
MLA [1] XU Cui-ping, et al., "Selective Adsorption Performance of Indium(Ⅲ)with P507/HZ818 Impregnated Resin in Sulfuric Acid System." Rare Metals and Cemented Carbides, no. 2, 2017, pp. 28-32.
APA [1] XU Cui-ping, LIU Jun-shen, LIU Qing-qing, & CHEN Xiao-liang. (2017). Selective Adsorption Performance of Indium(Ⅲ)with P507/HZ818 Impregnated Resin in Sulfuric Acid System. Rare Metals and Cemented Carbides(2), 28-32.
IEEE [1] XU Cui-ping, LIU Jun-shen, LIU Qing-qing, and CHEN Xiao-liang, "Selective Adsorption Performance of Indium(Ⅲ)with P507/HZ818 Impregnated Resin in Sulfuric Acid System," Rare Metals and Cemented Carbides, no. 2, pp. 28-32, 2017. keywords: {P507 / H Z818 impregnated resin;sulfuric acid system;selective adsorption;indium;gallium}