daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The Current Research and the Development Trend of Hydrogen Storage Alloy AITranslate

School of Materials Science and Engineering, Beijing University of Science and Technology;School of Materials Science and Engineering, Beijing University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Description is made of the development and latest research of hydrogen storage alloys. The developing trend of hydrogen storage alloy is predicted.

KeyWords AITranslate

hydrogen storage alloy current research development trend

1余学斌,吴铸,黄太仲,陈金舟,倪君.表面氧化层对TiMn_(1.25)Cr_(0.25)储氢合金活化性能的影响[J].稀有金属材料与工程,2004,33(11):1191-1194. 被引量:1

2陈东,陈廉,佟敏,陈德敏,成会明,吴锋.纳米复合储氢材料的研究[J].电池,2002,32(z1):94-97. 被引量:2

3刘红,白金兰.A组分变化对AB_5型储氢合金组织结构及电化学性能的影响[J].沈阳航空工业学院学报,2004,21(4):42-44. 被引量:2

4高嵘岗,涂江平,王秀丽,张孝彬,陈长聘.纳米TiO_2对Mg-15%Mg_2Ni复相合金吸放氢性能的影响[J].太阳能学报,2004,25(1):52-55. 被引量:4

5王方香,闫晓琦,高学平,袁华堂,宋德瑛.镁基复合储氢材料[J].化学通报,2002,65(2):85-89. 被引量:20

6李静明.储氢合金的研究进展[J].安庆师范学院学报:自然科学版,2004,10(3):15-17. 被引量:8

7黄太仲,吴铸,余学斌,陈金舟,夏保佳,徐乃欣.合金化对Ti-Cr基储氢合金性能的影响[J].稀有金属,2004,28(4):744-749. 被引量:8

8王毅,邱晓航,申泮文.镁基储氢材料研究新进展[J].化学通报,2004,67(5):327-332. 被引量:4

9李全安,陈云贵,王丽华,涂铭旌.贮氢合金的开发与应用[J].材料开发与应用,1999,14(3):33-36. 被引量:13

10Haiyan LENG, Demin CHEN, Manqi LU, Haifeng ZHANG, Huiming CHENG and Ke YANGInstitute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China.Mg AmorphousZr_(0.9)Ti_(0.1)(Ni_(0.57)Mn_(0.28)V_(0.1)Co_(0.05))_(2.1)Composite for Hydrogen Storage[J].材料科学技术:英文版,2003,19(2):141-144. 被引量:2

1胥锴,刘徽平,吴子平.贮氢合金材料的开发及应用[J].冶金丛刊,2008(6):32-36. 被引量:2

1周怀营,倪成员,王仲民,颜瑞,王殿辉.金属储氢材料与材料设计研究进展[J].桂林电子科技大学学报,2010,30(5):363-373. 被引量:3

2朱来成.发展氢能源的技术问题探讨[J].计算机与应用化学,2011,28(8):1079-1081. 被引量:6

1李惠萍.日本大力开发改良型镍钛系记忆合金[J].上海钢研,2003(2):53-53. 被引量:1

2高泽生.铝-钛系晶粒细化剂与第三元素[J].轻合金加工技术,1994,22(10):28-33. 被引量:2

3日本大力开发改良型镍-钛系记忆合金[J].金属材料研究,2004,30(3):51-51.

4曾泉浦,伍本德,毛小南.钛系多元储氢合金的研究[J].稀有金属材料与工程,1990(2):21-25. 被引量:2

5郭继伟,刘钦雷,荣守范,宋春梅.碳化钛系钢结硬质合金的研究现状[J].铸造设备与工艺,2010(1):48-54. 被引量:8

6陈泽民,宋勇朝,程志民.铝材表面制备钼锰钛系化学转化膜的研究[J].电镀与涂饰,2015,34(8):454-457. 被引量:3

7龚建勋,李丹,肖逸锋.铁-碳-铬-钒-钛系药芯焊丝堆焊层的显微组织及耐磨性能[J].机械工程材料,2010,34(11):42-45. 被引量:7

8陈泽民,宋勇朝,程志民.铝材表面制备钼锰钛系化学转化膜的影响因素分析[J].电镀与环保,2016,36(3):42-44. 被引量:3

9张爱文,郑磊.汽车用低合金高强度钢成分及控冷工艺[J].机械工程材料,2006,30(12):11-13. 被引量:13

10李健美,肖飞.钛系表面调整磷化膜的SEM和XRD研究[J].化学通报,1995(9):31-33. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TG139.7[一般工业技术—材料科学与工程]

Citation Information:

Description is made of the development and latest research of hydrogen storage alloys. The developing trend of hydrogen storage alloy is predicted.

quote

GB/T 7714-2015 [1] LIU Sheng-lin, SUN Dong-bai. The Current Research and the Development Trend of Hydrogen Storage Alloy[J]. Rare Metals and Cemented Carbides, 2005(4): 46-51.
MLA [1] LIU Sheng-lin, and SUN Dong-bai. "The Current Research and the Development Trend of Hydrogen Storage Alloy." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 46-51.
APA [1] LIU Sheng-lin, & SUN Dong-bai. (2005). The Current Research and the Development Trend of Hydrogen Storage Alloy. Rare Metals and Cemented Carbides(4), 46-51.
IEEE [1] LIU Sheng-lin and SUN Dong-bai, "The Current Research and the Development Trend of Hydrogen Storage Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 46-51, 2005. keywords: {hydrogen storage alloy;current research;development trend}