daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tuning the Electronic and Mechanical Properties of Two-Dimensional Diamond through N and B Doping Tuning the Electronic and Mechanical Properties of Two-Dimensional Diamond through N and B Doping AITranslate

Universidade de São Paulo; Universidade de São Paulo; Uppsala University; Universidade de São Paulo
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper examines the structural, thermodynamic, dynamic, elastic, and electronic properties of doped 2D diamond C4X2 (X = B or N) nanosheets in both AA′A″ and ABC stacking configurations, by first-principles calculations. Those systems consist of three diamond-like graphene sheets with an undoped graphene layer between two 50% doped ones. Our results, based on the analysis of ab initio molecular dynamics simulations, phonon dispersion spectra, and Born’s criteria for mechanical stability, revealed that all four structures are stable. Additionally, their standard enthalpy of formation values are similar to that of pristine 2D diamonds, recently synthesized by compressing three graphene layers together. The C4X2 (X = B or N) systems exhibit high elastic constant values and stiffness comparable to that of bulk diamond. The C4N2 nanosheets present wide indirect band gaps that could be advantageous for applications similar to those of the hexagonal boron nitride (h-BN), such as a substrate for high-mobility 2D devices. On the other hand, the C4B2 systems are semiconductors with direct band gaps, in the 1.6–2.0 eV range, and small effective masses, which are favorable characteristics to high carrier mobility and optoelectronics applications.

KeyWords AITranslate

2D diamond diamane ultrathin diamond films functionalization DFT firstprinciples calculations
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01398

Chinese Library Classification Number:

Citation Information:

This paper examines the structural, thermodynamic, dynamic, elastic, and electronic properties of doped 2D diamond C4X2 (X = B or N) nanosheets in both AA′A″ and ABC stacking configurations, by first-principles calculations. Those systems consist of three diamond-like graphene sheets with an undoped graphene layer between two 50% doped ones. Our results, based on the analysis of ab initio molecular dynamics simulations, phonon dispersion spectra, and Born’s criteria for mechanical stability, revealed that all four structures are stable. Additionally, their standard enthalpy of formation values are similar to that of pristine 2D diamonds, recently synthesized by compressing three graphene layers together. The C4X2 (X = B or N) systems exhibit high elastic constant values and stiffness comparable to that of bulk diamond. The C4N2 nanosheets present wide indirect band gaps that could be advantageous for applications similar to those of the hexagonal boron nitride (h-BN), such as a substrate for high-mobility 2D devices. On the other hand, the C4B2 systems are semiconductors with direct band gaps, in the 1.6–2.0 eV range, and small effective masses, which are favorable characteristics to high carrier mobility and optoelectronics applications.

quote

GB/T 7714-2015 [1] Bruno Ipaves, João F. Justo, Biplab Sanyal, et al. ACS Applied Electronic Materials, 2024(6). DOI:10.1021/acsaelm.3c01398.
MLA [1] Bruno Ipaves, et al., ACS Applied Electronic Materials, no. 6, 2024, https://doi.org/10.1021/acsaelm.3c01398.
APA [1] Bruno Ipaves, João F. Justo, Biplab Sanyal, & Lucy V. C. Assali. (2024). ACS Applied Electronic Materials(6). https://doi.org/10.1021/acsaelm.3c01398
IEEE [1] Bruno Ipaves, João F. Justo, Biplab Sanyal, and Lucy V. C. Assali, ACS Applied Electronic Materials, no. 6, 2024, doi: 10.1021/acsaelm.3c01398. keywords: {2D diamond diamane ultrathin diamond films functionalization DFT firstprinciples calculations}