Metal–Organic-Framework-Based Polymers for Effective Water Harvesting in Arid Areas AITranslate
Abstract AITranslate
This study used a postsynthetic modification strategy to amidate UIO-66-NH2 to synthesize a functional copolymer monomer by free radical polymerization with acrylic acid (AA) and acrylamide (AM) to form hygroscopic polymer materials based on UIO-66-NH2 (UPHMs). The experiments show that the uptake capacity of UIO-66-NH2-self-polymerization products and UPHMs for water vapor is 11.1 and 18.6 times that of pure UIO-66-NH2, respectively. And UPHMs can be adsorbed in a wide range of adsorption humidity (relative humidity (RH) from 50 to 90%) and with high adsorption of liquid water (salt), rapid water vapor capture (at 90% RH and 25 °C, 10 h adsorption efficiency reaches 1.9 g/g), low desorption temperature, and higher water release rate. The method offers a promising route for the development of atmospheric water recovery materials based on adsorbents, and it opens horizons for the controllable preparation of soft MOF hydrogels and functional materials for many promising applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01656
Chinese Library Classification Number:
Citation Information:
This study used a postsynthetic modification strategy to amidate UIO-66-NH2 to synthesize a functional copolymer monomer by free radical polymerization with acrylic acid (AA) and acrylamide (AM) to form hygroscopic polymer materials based on UIO-66-NH2 (UPHMs). The experiments show that the uptake capacity of UIO-66-NH2-self-polymerization products and UPHMs for water vapor is 11.1 and 18.6 times that of pure UIO-66-NH2, respectively. And UPHMs can be adsorbed in a wide range of adsorption humidity (relative humidity (RH) from 50 to 90%) and with high adsorption of liquid water (salt), rapid water vapor capture (at 90% RH and 25 °C, 10 h adsorption efficiency reaches 1.9 g/g), low desorption temperature, and higher water release rate. The method offers a promising route for the development of atmospheric water recovery materials based on adsorbents, and it opens horizons for the controllable preparation of soft MOF hydrogels and functional materials for many promising applications.
quote
| GB/T 7714-2015 | [1] Xiaomei Liu, Tao Feng, Wenbin Ding, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01656. |
| MLA | [1] Xiaomei Liu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01656. |
| APA | [1] Xiaomei Liu, Tao Feng, Wenbin Ding, Zhenshi Zhang, Huaiwu Peng, Cailing Yang, Jing Li, Pengbo Liu, Qi Li, Li Zhang, & Ziqiang Lei. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01656 |
| IEEE | [1] Xiaomei Liu, Tao Feng, Wenbin Ding, Zhenshi Zhang, Huaiwu Peng, Cailing Yang, Jing Li, Pengbo Liu, Qi Li, Li Zhang, and Ziqiang Lei, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01656. keywords: {atmospheric water harvesting;polymer monomer;fresh water resources;postsynthetic modification;function materials} |
