Development & Application of Portable Horizontal Rubber Removal Furnaces AITranslate
Abstract AITranslate
The structures of portable horizontal rubber removal furnaces are described.Contrast experiments are made between the two for the comparision of their effect.The result shows portable horizontal disintegrated furnaces have the advantage of energy saving resources?even tempeature and long service life,as can meet the requirements for quality JY·1 cemented carbide production.
KeyWords AITranslate
1杨碧华,周建华.立式、卧式排胶炉及其排胶效果的对比试验[J].稀有金属与硬质合金,1996,24(2):30-35. 被引量:1
1周建华,卢伟民.YJ_(2.1),YJ_(1.1)矿山凿岩硬质合金的开发与应用[J].粉末冶金材料科学与工程,2001,6(1):73-77.
2周建华,卢伟民.YJ2.1、YJ1.1矿山凿岩硬质合金的开发与应用[J].稀有金属与硬质合金,2001,29(4):10-12. 被引量:4
3李燕,刘绍君.可倾翻式球磨机[J].湖南冶金,2000,28(2):17-20.
Basic Information:
DOI:
Chinese Library Classification Number:TF37[冶金工程—冶金机械及自动化]
Citation Information:
The structures of portable horizontal rubber removal furnaces are described.Contrast experiments are made between the two for the comparision of their effect.The result shows portable horizontal disintegrated furnaces have the advantage of energy saving resources?even tempeature and long service life,as can meet the requirements for quality JY·1 cemented carbide production.
quote
| GB/T 7714-2015 | [1] ZHOU Jian-hua, YANG Bi-hua, LU Wei-min. Development & Application of Portable Horizontal Rubber Removal Furnaces[J]. Rare Metals and Cemented Carbides, 2002(1): 48-50. |
| MLA | [1] ZHOU Jian-hua, et al., "Development & Application of Portable Horizontal Rubber Removal Furnaces." Rare Metals and Cemented Carbides, no. 1, 2002, pp. 48-50. |
| APA | [1] ZHOU Jian-hua, YANG Bi-hua, & LU Wei-min. (2002). Development & Application of Portable Horizontal Rubber Removal Furnaces. Rare Metals and Cemented Carbides(1), 48-50. |
| IEEE | [1] ZHOU Jian-hua, YANG Bi-hua, and LU Wei-min, "Development & Application of Portable Horizontal Rubber Removal Furnaces," Rare Metals and Cemented Carbides, no. 1, pp. 48-50, 2002. keywords: {cemented carbide;portable rubber removal furnace;development and application.} |