Microgels as Smart Polymer Colloids for Sensing and Environmental Remediation AITranslate

Indian Institute of Technology Patna; Indian Institute of Technology Patna; Indian Institute of Technology Patna
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Stimuli-responsive microgels are gaining a lot of attention as a result of their excellent chemical and structural integrity with easy deformability and possibilities for being incorporated into various functionalities. The characteristic chemical and physical properties of microgels result in their widespread application. Among their many applications in the current review, we will give an overview on the design principles and synthetic approaches of microgels for sensing applications and their uses for the removal of different environmental pollutants. It is important to understanding the mechanism of sensing and adsorption, which is important for exploring further advancement. In this review, we brief these aspects.

KeyWords AITranslate

functional microgels stimuliresponsive materials sensing environmental remediation detection polymer colloids nanomaterials
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01947

Chinese Library Classification Number:

Citation Information:

Stimuli-responsive microgels are gaining a lot of attention as a result of their excellent chemical and structural integrity with easy deformability and possibilities for being incorporated into various functionalities. The characteristic chemical and physical properties of microgels result in their widespread application. Among their many applications in the current review, we will give an overview on the design principles and synthetic approaches of microgels for sensing applications and their uses for the removal of different environmental pollutants. It is important to understanding the mechanism of sensing and adsorption, which is important for exploring further advancement. In this review, we brief these aspects.

quote

GB/T 7714-2015 [1] Sulbha Kumari, Mohd. Avais, Subrata Chattopadhyay. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01947.
MLA [1] Sulbha Kumari, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01947.
APA [1] Sulbha Kumari, Mohd. Avais, & Subrata Chattopadhyay. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01947
IEEE [1] Sulbha Kumari, Mohd. Avais, and Subrata Chattopadhyay, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01947. keywords: {functional microgels;stimuliresponsive materials;sensing;environmental remediation;detection;polymer colloids;nanomaterials}