daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Green High Barrier Solution for Paperboard Packaging based on Potato Fruit Juice, Poly(lactic acid), and Poly(butylene adipate terephthalate) AITranslate

Tampere University; Tampere University; Tampere University; Tampere University; KTH Royal Institute of Technology; Tampere University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The potential of using potato fruit juice (PFJ), a byproduct from the potato starch industry, was investigated as a barrier paper-coating material. The paperboard was initially hand-coated with PFJ (with and without glycerol as plasticizer) and then extrusion-coated with poly(lactic acid) (PLA) or a blend of PLA and poly(butylene adipate terephthalate) (PBAT). The multilayer coated paperboard was homogeneous in appearance with a glossy finish. The coated paperboard showed, at the most, a ca. 95% reduction in specific water vapor transmission rate compared to the uncoated paperboard. In the presence of the PFJ layer, the extrusion-coated paperboard experienced, at the most, a 98% reduction in oxygen permeability. The grease resistance of the paperboard was also improved significantly with this multilayer coating. PLA- and PFJ-coated samples showed better barrier properties, whereas PFJ with PLA/PBAT layers exhibited better adhesion and heat-sealing properties. The peel strength of the coated samples was moderately good for paper converting applications. The developed coated paperboard also exhibited good creasing properties which is yet again an advantage for packaging applications. The presented barrier properties make the developed multilayer coatings on paperboards a sustainable competitive alternative to several of today’s coatings.

KeyWords AITranslate

paper coating barrier coating biobased coating potato fruit juice poly(lactic acid) poly(butylene adipate terephthalate) Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00153

Chinese Library Classification Number:

Citation Information:

The potential of using potato fruit juice (PFJ), a byproduct from the potato starch industry, was investigated as a barrier paper-coating material. The paperboard was initially hand-coated with PFJ (with and without glycerol as plasticizer) and then extrusion-coated with poly(lactic acid) (PLA) or a blend of PLA and poly(butylene adipate terephthalate) (PBAT). The multilayer coated paperboard was homogeneous in appearance with a glossy finish. The coated paperboard showed, at the most, a ca. 95% reduction in specific water vapor transmission rate compared to the uncoated paperboard. In the presence of the PFJ layer, the extrusion-coated paperboard experienced, at the most, a 98% reduction in oxygen permeability. The grease resistance of the paperboard was also improved significantly with this multilayer coating. PLA- and PFJ-coated samples showed better barrier properties, whereas PFJ with PLA/PBAT layers exhibited better adhesion and heat-sealing properties. The peel strength of the coated samples was moderately good for paper converting applications. The developed coated paperboard also exhibited good creasing properties which is yet again an advantage for packaging applications. The presented barrier properties make the developed multilayer coatings on paperboards a sustainable competitive alternative to several of today’s coatings.

quote

GB/T 7714-2015 [1] Simi Poulose, Juuso Toriseva, Johanna Lahti, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00153.
MLA [1] Simi Poulose, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00153.
APA [1] Simi Poulose, Juuso Toriseva, Johanna Lahti, Ilari Jönkkäri, Mikael S. Hedenqvist, & Jurkka Kuusipalo. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00153
IEEE [1] Simi Poulose, Juuso Toriseva, Johanna Lahti, Ilari Jönkkäri, Mikael S. Hedenqvist, and Jurkka Kuusipalo, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00153. keywords: {paper coating;barrier coating;biobased coating;potato fruit juice;poly(lactic acid);poly(butylene adipate terephthalate);Show More}