daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Enhanced Energy Storage Performance of Doped Modified PC/PVDF Coblended Flexible Composite Films Enhanced Energy Storage Performance of Doped Modified PC/PVDF Coblended Flexible Composite Films AITranslate

Harbin University of Science and Technology; Harbin University of Science and Technology; Harbin University of Science and Technology; Zhejiang University of Water Resources and Electric Power; Harbin University of Science and Technology; Harbin University of Science and Technology; Harbin University of Science and Technology; Harbin University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The rapid development of the clean energy industry has given great impetus to energy-efficient storage and conversion technologies. Film capacitors have attracted much attention because of their higher charge and release rates, greater energy density, and extended life cycle. But the lower recharging and discharging efficiency and insulation properties pertaining to the electricity used in capacitors limit the improvement of their energy storage performance. In this paper, the addition of the linear polymer polycarbonate (PC) to polyvinylidene fluoride (PVDF) through a blending strategy and the subsequent acquisition of the high-dielectric nanofiller titanium dioxide (TiO2) to the blended matrix is expected to achieve synergistic optimization of the insulation and polarization properties, thereby enhancing the energy storage performance of the mixed media. The findings show that great storage of energy productivity (Ue ≈ 11.43 J/cm3, η ≈ 57.08%) is obtained for 40 vol % PC/PVDF-x wt %-TiO2 at an optimum field strength of 450 kV/mm when the TiO2 doping amount x is 0.9 wt %. Compared with pure PVDF, its Ue is improved by 2.3 times, η by 1.2 times, and Eb by 1.5 times. This research presents a viable answer for applying PVDF-based high-energy-storage film capacitors.

KeyWords AITranslate

Blended composite media TiO2 Dielectric properties Energy storage density
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00537

Chinese Library Classification Number:

Citation Information:

The rapid development of the clean energy industry has given great impetus to energy-efficient storage and conversion technologies. Film capacitors have attracted much attention because of their higher charge and release rates, greater energy density, and extended life cycle. But the lower recharging and discharging efficiency and insulation properties pertaining to the electricity used in capacitors limit the improvement of their energy storage performance. In this paper, the addition of the linear polymer polycarbonate (PC) to polyvinylidene fluoride (PVDF) through a blending strategy and the subsequent acquisition of the high-dielectric nanofiller titanium dioxide (TiO2) to the blended matrix is expected to achieve synergistic optimization of the insulation and polarization properties, thereby enhancing the energy storage performance of the mixed media. The findings show that great storage of energy productivity (Ue ≈ 11.43 J/cm3, η ≈ 57.08%) is obtained for 40 vol % PC/PVDF-x wt %-TiO2 at an optimum field strength of 450 kV/mm when the TiO2 doping amount x is 0.9 wt %. Compared with pure PVDF, its Ue is improved by 2.3 times, η by 1.2 times, and Eb by 1.5 times. This research presents a viable answer for applying PVDF-based high-energy-storage film capacitors.

quote

GB/T 7714-2015 [1] Changhai Zhang, Weidong Yan, Yue Zhang, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00537.
MLA [1] Changhai Zhang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00537.
APA [1] Changhai Zhang, Weidong Yan, Yue Zhang, Yang Cui, Tiandong Zhang, Chao Tang, Xianli Liu, & Qingguo Chi. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00537