Carbohydrate-Containing Conjugated Polymers: Solvent-Resistant Materials for Greener Organic Electronics Carbohydrate-Containing Conjugated Polymers: Solvent-Resistant Materials for Greener Organic Electronics AITranslate

University of Windsor; The University of Southern Mississippi; University of Windsor; The University of Southern Mississippi; University of Windsor
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Organic semiconducting polymers are exciting materials for electronic applications because of their good mechanical and optoelectronic properties. A major advantage of organic semiconductors is their solution processability. This allows access to a variety of simple and cost-effective device fabrication methods compared to the expensive, high-temperature processing methods required for silicon-based electronics. However, these materials often have low solubility, which limits their processing to toxic halogenated solvents. Also, their limited solubility often leads to interfacial mixing during device fabrication. This work explores the incorporation of environmentally friendly carbohydrate side chains in conjugated polymers to enhance processability in eco-friendly solvents. Moreover, a mild postprocessing treatment was designed to enable solvent resistance. Isoindigo-based polymers with varied ratios of acetyl-protected galactose side chains were synthesized to improve solubility in o-anisole in the protected state, while inducing solvent resistance through intramolecular hydrogen bonding in the deprotected state. Solvent resistance was confirmed both visually upon submersion in various solvents and using UV–visible spectroscopy. Importantly, the mild basic treatment to achieve solvent resistance has no negative impact on the electronic performance of these materials in organic field-effect transistors, even after subsequent submersion in various solvents, making them a valuable platform for the production of green processable multilayer electronics.

KeyWords AITranslate

solventresistant electronics organic electronics conjugated polymers semiconducting polymers organic fieldeffect transistors processing of πconjugated polymers
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c00932

Chinese Library Classification Number:

Citation Information:

Organic semiconducting polymers are exciting materials for electronic applications because of their good mechanical and optoelectronic properties. A major advantage of organic semiconductors is their solution processability. This allows access to a variety of simple and cost-effective device fabrication methods compared to the expensive, high-temperature processing methods required for silicon-based electronics. However, these materials often have low solubility, which limits their processing to toxic halogenated solvents. Also, their limited solubility often leads to interfacial mixing during device fabrication. This work explores the incorporation of environmentally friendly carbohydrate side chains in conjugated polymers to enhance processability in eco-friendly solvents. Moreover, a mild postprocessing treatment was designed to enable solvent resistance. Isoindigo-based polymers with varied ratios of acetyl-protected galactose side chains were synthesized to improve solubility in o-anisole in the protected state, while inducing solvent resistance through intramolecular hydrogen bonding in the deprotected state. Solvent resistance was confirmed both visually upon submersion in various solvents and using UV–visible spectroscopy. Importantly, the mild basic treatment to achieve solvent resistance has no negative impact on the electronic performance of these materials in organic field-effect transistors, even after subsequent submersion in various solvents, making them a valuable platform for the production of green processable multilayer electronics.

quote

GB/T 7714-2015 [1] Madison Mooney, Yunfei Wang, Ekaterini Iakovidis, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c00932.
MLA [1] Madison Mooney, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c00932.
APA [1] Madison Mooney, Yunfei Wang, Ekaterini Iakovidis, Xiaodan Gu, & Simon RondeauGagné. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c00932
IEEE [1] Madison Mooney, Yunfei Wang, Ekaterini Iakovidis, Xiaodan Gu, and Simon RondeauGagné, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c00932. keywords: {solventresistant electronics organic electronics conjugated polymers semiconducting polymers organic fieldeffect transistors processing of πconjugated polymers}