daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Light-Responsive Crosslinked Polymer Particles from Heterogeneous Polymerization of an Asymmetric Divinyl Azobenzene Monomer AITranslate

Ehime University; Ehime University; Ehime University; Ehime University; Ehime University; Ehime University; Ehime University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Azobenzene polymer particles have been investigated for over two decades, owing to their interesting light-responsive properties. Crosslinking is a promising solution for improving the reusability of azobenzene polymer particles for practical use; however, the production of crosslinked azobenzene particles remains challenging. In this study, crosslinked azobenzene polymer particles were developed to achieve light responsiveness, recoverability, and reusability. The precipitation polymerization and dispersion polymerization of an azobenzene monomer, (E)-6-(4-((4-(allyloxy)phenyl)diazenyl)phenoxy)hexyl methacrylate bearing asymmetric divinyl groups, successfully endowed crosslinked azobenzene polymer particles with a unique oblate shape and narrow size distribution. Polarized optical microscope studies indicated that the azobenzene groups were aligned in the particles and had a bipolar configuration. The particles exhibited recoverable light-responsive shape changes upon irradiation with ultraviolet (365 nm) and white light. Hydrophobic and hydrophilic particles prepared by precipitation and dispersion polymerizations yielded water-in-oil and oil-in-water Pickering emulsions, respectively, which were both reversibly formed and deformed upon light irradiation. Furthermore, the reusability of the particles in light-responsive liquid marbles was achieved. Consequently, the asymmetric divinyl azobenzene monomer successfully produced recoverable and reusable light-responsive polymer particles.

KeyWords AITranslate

photochromic azobenzenebased polymer particles anisotropicshaped crosslinked polymer particles Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00031

Chinese Library Classification Number:

Citation Information:

Azobenzene polymer particles have been investigated for over two decades, owing to their interesting light-responsive properties. Crosslinking is a promising solution for improving the reusability of azobenzene polymer particles for practical use; however, the production of crosslinked azobenzene particles remains challenging. In this study, crosslinked azobenzene polymer particles were developed to achieve light responsiveness, recoverability, and reusability. The precipitation polymerization and dispersion polymerization of an azobenzene monomer, (E)-6-(4-((4-(allyloxy)phenyl)diazenyl)phenoxy)hexyl methacrylate bearing asymmetric divinyl groups, successfully endowed crosslinked azobenzene polymer particles with a unique oblate shape and narrow size distribution. Polarized optical microscope studies indicated that the azobenzene groups were aligned in the particles and had a bipolar configuration. The particles exhibited recoverable light-responsive shape changes upon irradiation with ultraviolet (365 nm) and white light. Hydrophobic and hydrophilic particles prepared by precipitation and dispersion polymerizations yielded water-in-oil and oil-in-water Pickering emulsions, respectively, which were both reversibly formed and deformed upon light irradiation. Furthermore, the reusability of the particles in light-responsive liquid marbles was achieved. Consequently, the asymmetric divinyl azobenzene monomer successfully produced recoverable and reusable light-responsive polymer particles.

quote

GB/T 7714-2015 [1] Tomomichi Itoh, Moeka Kimoto, Natsumi Kuroda, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00031.
MLA [1] Tomomichi Itoh, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00031.
APA [1] Tomomichi Itoh, Moeka Kimoto, Natsumi Kuroda, Keisuke Ishizaki, Eiji Yukihiro, Hiroaki Shimomoto, & Eiji Ihara. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00031
IEEE [1] Tomomichi Itoh, Moeka Kimoto, Natsumi Kuroda, Keisuke Ishizaki, Eiji Yukihiro, Hiroaki Shimomoto, and Eiji Ihara, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00031. keywords: {photochromic azobenzenebased polymer particles;anisotropicshaped crosslinked polymer particles;Show More}