daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Understanding and Control of Polymer Distribution in Photoresists Using Liquid Chromatography for Enhanced Lithography Performance AITranslate

Samsung Advanced Institute of Technology (SAIT);Samsung Advanced Institute of Technology (SAIT);Samsung Advanced Institute of Technology (SAIT);Paul Scherrer Institut, 5232 Villigen-PSI;Paul Scherrer Institut, 5232 Villigen-PSI;Paul Scherrer Institut, 5232 Villigen-PSI;Samsung Advanced Institute of Technology (SAIT)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The introduction of extreme ultraviolet lithography in high-volume manufacturing has once again ensured further progress in semiconductor technology. As we journey toward future technology nodes with smaller features, the quest for photoresists that meet these stringent specifications becomes increasingly challenging. Stochastic effects, such as the compositional dispersion of molecules in photoresists, have become a limiting factor in the lithography performance of photoresists. Here, we report on chromatographic techniques to separate random copolymers within photoresist materials according to chemical composition. We present a systematic study aimed at providing a fundamental understanding of how the molecular weight distribution and chemical composition of polymers included in photoresists influence lithography performance. Compared to other conventional methods, such as size exclusion chromatography, the approach in this study offers superior accuracy and resolution. It presents a promising approach to accurately identify and quantify the organic polymers within photoresists. Improved molecular dispersion of the polymers leads to an enhancement of the resist’s performance in EUV lithography. Our approach sets a standard in photoresist analysis and offers a viable approach to reduce stochastic effects, paving the way for photoresists with better performance for future technology nodes.

KeyWords AITranslate

EUV photoresist polymer HPLC chemical composition distribution critical dimension LER
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01953

Chinese Library Classification Number:

Citation Information:

The introduction of extreme ultraviolet lithography in high-volume manufacturing has once again ensured further progress in semiconductor technology. As we journey toward future technology nodes with smaller features, the quest for photoresists that meet these stringent specifications becomes increasingly challenging. Stochastic effects, such as the compositional dispersion of molecules in photoresists, have become a limiting factor in the lithography performance of photoresists. Here, we report on chromatographic techniques to separate random copolymers within photoresist materials according to chemical composition. We present a systematic study aimed at providing a fundamental understanding of how the molecular weight distribution and chemical composition of polymers included in photoresists influence lithography performance. Compared to other conventional methods, such as size exclusion chromatography, the approach in this study offers superior accuracy and resolution. It presents a promising approach to accurately identify and quantify the organic polymers within photoresists. Improved molecular dispersion of the polymers leads to an enhancement of the resist’s performance in EUV lithography. Our approach sets a standard in photoresist analysis and offers a viable approach to reduce stochastic effects, paving the way for photoresists with better performance for future technology nodes.

quote

GB/T 7714-2015 [1] Kyuhyun Im, Chang Heon Lee, Minsang Kim, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01953.
MLA [1] Kyuhyun Im, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01953.
APA [1] Kyuhyun Im, Chang Heon Lee, Minsang Kim, Iason Giannopoulos, Dimitrios Kazazis, Yasin Ekinci, & Yoonhyun Kwak. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01953
IEEE [1] Kyuhyun Im, Chang Heon Lee, Minsang Kim, Iason Giannopoulos, Dimitrios Kazazis, Yasin Ekinci, and Yoonhyun Kwak, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01953. keywords: {EUV photoresist;polymer;HPLC;chemical composition distribution;critical dimension;LER}