Study on Extraction of Vanadium from Stone Coal Vanadium Ore by Barium Salt Roasting-Low Acid Leaching Method AITranslate
Abstract AITranslate
In this paper,stone coal vanadium ore was used as raw material,and the vanadium was extracted by barium salt roasting-low acid leaching process from the concentrate after tailing discarding and enrichment.The effects of concentrate roasting and leaching conditions on the leaching rate of vanadium were studied.The results show that the average vanadium leaching rate can reach 87.93%under the optimal conditions of stone coal vanadium concentrate fineness of 70%passing 74μm,roasting temperature of 925℃,roasting time of 6 h,barium sulfate dosage of 4%concentrate quality,liquid-solid ratio in leaching process of 2∶1,sulfuric acid dosage of 5%calcine quality,leaching temperature of 50℃and leaching time of 1 h.The process has the advantages of high vanadium leaching rate,low acid dosage,low extraction cost and simplified subsequent vanadium extraction process.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程]
Citation Information:
In this paper,stone coal vanadium ore was used as raw material,and the vanadium was extracted by barium salt roasting-low acid leaching process from the concentrate after tailing discarding and enrichment.The effects of concentrate roasting and leaching conditions on the leaching rate of vanadium were studied.The results show that the average vanadium leaching rate can reach 87.93%under the optimal conditions of stone coal vanadium concentrate fineness of 70%passing 74μm,roasting temperature of 925℃,roasting time of 6 h,barium sulfate dosage of 4%concentrate quality,liquid-solid ratio in leaching process of 2∶1,sulfuric acid dosage of 5%calcine quality,leaching temperature of 50℃and leaching time of 1 h.The process has the advantages of high vanadium leaching rate,low acid dosage,low extraction cost and simplified subsequent vanadium extraction process.
quote
| GB/T 7714-2015 | [1] WANG Yong, LIANG Xiao, WANG Xu, et al. Study on Extraction of Vanadium from Stone Coal Vanadium Ore by Barium Salt Roasting-Low Acid Leaching Method[J]. Rare Metals and Cemented Carbides, 2025(3): 18-24. |
| MLA | [1] WANG Yong, et al., "Study on Extraction of Vanadium from Stone Coal Vanadium Ore by Barium Salt Roasting-Low Acid Leaching Method." Rare Metals and Cemented Carbides, no. 3, 2025, pp. 18-24. |
| APA | [1] WANG Yong, LIANG Xiao, WANG Xu, & NING Xin-xia. (2025). Study on Extraction of Vanadium from Stone Coal Vanadium Ore by Barium Salt Roasting-Low Acid Leaching Method. Rare Metals and Cemented Carbides(3), 18-24. |
| IEEE | [1] WANG Yong, LIANG Xiao, WANG Xu, and NING Xin-xia, "Study on Extraction of Vanadium from Stone Coal Vanadium Ore by Barium Salt Roasting-Low Acid Leaching Method," Rare Metals and Cemented Carbides, no. 3, pp. 18-24, 2025. keywords: {stone coal vanadium ore;vanadium extraction;barium salt roasting;low acid leaching;sulfuric acid} |