Abstract AITranslate
Flexible electronic sensors are today trending toward being smaller, lighter, and also conformal, while additive manufacturing capabilities are proving crucial in their rapid prototyping. Here, we report flexible and conformal thermocouples by printing liquid metal–organic decomposition materials, consisting of Cu and CuNi particle-free conductive inks. The printed Cu–CuNi (type T) thermocouple shows a linear temperature response with a sensitivity of 20.6 μV/°C and a response time below 2 s. In addition, the printed flexible thermocouple sensor exhibits high stability and reliability when subjected to external stimuli, such as bending, humidity, and thermal cycling. Printed conformal thermocouples using liquid metal decomposition ink materials provide a promising avenue toward miniaturized hybrid electronic devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01150
Chinese Library Classification Number:
Citation Information:
Flexible electronic sensors are today trending toward being smaller, lighter, and also conformal, while additive manufacturing capabilities are proving crucial in their rapid prototyping. Here, we report flexible and conformal thermocouples by printing liquid metal–organic decomposition materials, consisting of Cu and CuNi particle-free conductive inks. The printed Cu–CuNi (type T) thermocouple shows a linear temperature response with a sensitivity of 20.6 μV/°C and a response time below 2 s. In addition, the printed flexible thermocouple sensor exhibits high stability and reliability when subjected to external stimuli, such as bending, humidity, and thermal cycling. Printed conformal thermocouples using liquid metal decomposition ink materials provide a promising avenue toward miniaturized hybrid electronic devices.
quote
| GB/T 7714-2015 | [1] Aaron Sheng, Saurabh Khuje, Zheng Li, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01150. |
| MLA | [1] Aaron Sheng, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01150. |
| APA | [1] Aaron Sheng, Saurabh Khuje, Zheng Li, Jian Yu, & Shenqiang Ren. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01150 |
| IEEE | [1] Aaron Sheng, Saurabh Khuje, Zheng Li, Jian Yu, and Shenqiang Ren, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01150. keywords: {copper copper−nickel printed electronics thermocouple flexible sensors} |