Thermodynamic Study on Acid Decomposition Process of Cerium and Terbium Oxides AITranslate
Abstract AITranslate
Theφ-pH diagrams of acid decomposition process of oxides of cerium and terbium at 298.15 K were studied by thermodynamic calculation.The results show that CeO2 and TbO2are difficult to be directly decomposed by acid,but they can be transformed into Ce^3+and Tb^3+by acid decomposition in a reductive environment.Compared with CeO2 and TbO2,Ce2O3 and Tb2O3can be directly decomposed into Ce^3+and Tb^3+by acid with high pH value,which actualizes the extraction of cerium and terbium.
KeyWords AITranslate
1洪梅.稀土二次资源开发与循环利用任重道远[J].稀土信息,2015,21(3):26-27. 被引量:1
2李晓丽,张忠义.稀土发光材料产业现状分析[J].稀土,2010,31(2):55-59. 被引量:10
3田振宇.灯用稀土三基色荧光粉的现状[J].中国照明电器,2012(5):21-23. 被引量:7
4王伍宝,郭峰,闫世润.灯用稀土荧光粉的若干技术发展和探索(上)[J].中国照明电器,2009(6):11-16. 被引量:4
5李洪枚.从废稀土荧光粉中酸浸回收稀土的研究[J].稀有金属,2010,34(6):898-904. 被引量:32
6李雨,徐欣欣,徐林,魏涛,雷鹰.微波辅助加热浸出废荧光粉中稀土氧化物实验研究[J].矿冶工程,2015,35(4):67-69. 被引量:4
7李洪枚.用硫酸从废旧稀土荧光粉中浸出稀土[J].湿法冶金,2010,29(3):188-190. 被引量:15
8廖春发,陈静远,曾颜亮,李啊林.选择性还原浸出废旧稀土绿色荧光粉及热力学分析[J].稀土,2015,36(6):7-12. 被引量:8
1李洪枚.用硫酸从废旧稀土荧光粉中浸出稀土[J].湿法冶金,2010,29(3):188-190. 被引量:15
2廖春发,曾颜亮,焦芸芬.从废旧稀土荧光粉中回收稀土的研究现状[J].稀有金属与硬质合金,2013,41(6):7-12. 被引量:12
3王瑞祥,廖根,温功玉,郭跃东,张兆雪,熊家春,谢博毅.废旧稀土荧光粉与氢氧化钠焙烧反应动力学[J].有色金属:冶炼部分,2017(2):32-35.
4张兆雪,王瑞祥,熊家春,温功玉,廖根,谢博毅.碱熔预处理对废旧稀土荧光粉中稀土提取的影响[J].有色金属科学与工程,2016,7(6):129-135. 被引量:6
5葛星坊.溶剂萃取法从攀西稀土矿提取氧化铈新工艺[J].稀土信息,1999,5(6):11-11.
6郭斗斗,梁勇,温葆林,刘玉城,靖青秀.从废稀土荧光粉回收稀土[J].中国有色冶金,2014,43(5):79-82. 被引量:4
7白钨精矿与黑白钨混合矿碱分解方法及设备[J].中国新技术新产品,1997,0(1):42-42.
8马凯,马培华.块状磷矿石硝酸溶浸试验研究[J].矿产保护与利用,2010,30(1):30-32. 被引量:1
9刘海蛟,许延辉,孟志军,崔建国,张旭霞,王英杰.浓碱法分解包头混合稀土矿的静态工艺条件研究[J].稀土,2011,32(1):68-71. 被引量:8
10柯平超,刘志宏,刘智勇,李玉虎,刘付朋.固砷矿物臭葱石组成与结构及其浸出稳定性研究现状[J].化工学报,2016,67(11):4533-4540. 被引量:9
Basic Information:
DOI:
Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]
Citation Information:
Theφ-pH diagrams of acid decomposition process of oxides of cerium and terbium at 298.15 K were studied by thermodynamic calculation.The results show that CeO2 and TbO2are difficult to be directly decomposed by acid,but they can be transformed into Ce^3+and Tb^3+by acid decomposition in a reductive environment.Compared with CeO2 and TbO2,Ce2O3 and Tb2O3can be directly decomposed into Ce^3+and Tb^3+by acid with high pH value,which actualizes the extraction of cerium and terbium.
quote
| GB/T 7714-2015 | [1] LIANG Yong, LI Yong-kang, XUE Li-yan, et al. Thermodynamic Study on Acid Decomposition Process of Cerium and Terbium Oxides[J]. Rare Metals and Cemented Carbides, 2017(1): 8-10. |
| MLA | [1] LIANG Yong, et al., "Thermodynamic Study on Acid Decomposition Process of Cerium and Terbium Oxides." Rare Metals and Cemented Carbides, no. 1, 2017, pp. 8-10. |
| APA | [1] LIANG Yong, LI Yong-kang, XUE Li-yan, & GUO Dou-dou. (2017). Thermodynamic Study on Acid Decomposition Process of Cerium and Terbium Oxides. Rare Metals and Cemented Carbides(1), 8-10. |
| IEEE | [1] LIANG Yong, LI Yong-kang, XUE Li-yan, and GUO Dou-dou, "Thermodynamic Study on Acid Decomposition Process of Cerium and Terbium Oxides," Rare Metals and Cemented Carbides, no. 1, pp. 8-10, 2017. keywords: {waste rare earth phosphor;cerium;terbium;thermodynamics;acid decomposition;φ-pH diagram} |