Electric Field Induced Schottky to Ohmic Contact Transition in Fe3GeTe2/TMDs Contacts Electric Field Induced Schottky to Ohmic Contact Transition in Fe3GeTe2/TMDs Contacts AITranslate

Nanjing Tech University; Nanjing Tech University; Southeast University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Although the two-dimensional transition metal dichalcogenides (TMDs) present excellent electrical properties, the contact resistance at the interface of metal/TMDs limits the device performance. Herein, we use 2D metallic Fe3GeTe2 (FGT) as an electrode in contact with TMDs semiconductors MX2 (M = Mo, W; X = S, Se, Te) and investigate the contact properties of FGT/MX2 based on density functional theory calculations. We demonstrated that FGT/MX2 presents n-type Schottky contacts, and their n-type Schottky barrier heights are lower than that of the most common bulk metal contacts with MX2, suggesting that FGT can be used as an efficient metallic electrode for MX2. The transitions from n-type Schottky contact to p-type Schottky contact and from Schottky contact to Ohmic contact can be achieved in FGT/MX2 under the electric field. This work not only illustrates an effective method to modulate the contact types and Schottky barrier heights of FGT/MX2 contacts but also provides a route for designing the nanodevices based on FGT/MX2 electrical contacts.

KeyWords AITranslate

transition metal dichalcogenides Fe3GeTe2 Schottky barrier electric field density functional theory
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00151

Chinese Library Classification Number:

Citation Information:

Although the two-dimensional transition metal dichalcogenides (TMDs) present excellent electrical properties, the contact resistance at the interface of metal/TMDs limits the device performance. Herein, we use 2D metallic Fe3GeTe2 (FGT) as an electrode in contact with TMDs semiconductors MX2 (M = Mo, W; X = S, Se, Te) and investigate the contact properties of FGT/MX2 based on density functional theory calculations. We demonstrated that FGT/MX2 presents n-type Schottky contacts, and their n-type Schottky barrier heights are lower than that of the most common bulk metal contacts with MX2, suggesting that FGT can be used as an efficient metallic electrode for MX2. The transitions from n-type Schottky contact to p-type Schottky contact and from Schottky contact to Ohmic contact can be achieved in FGT/MX2 under the electric field. This work not only illustrates an effective method to modulate the contact types and Schottky barrier heights of FGT/MX2 contacts but also provides a route for designing the nanodevices based on FGT/MX2 electrical contacts.

quote

GB/T 7714-2015 [1] Guotao Jiang, Xiaohui Hu, Litao Sun. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00151.
MLA [1] Guotao Jiang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00151.
APA [1] Guotao Jiang, Xiaohui Hu, & Litao Sun. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00151
IEEE [1] Guotao Jiang, Xiaohui Hu, and Litao Sun, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00151. keywords: {transition metal dichalcogenides Fe3GeTe2 Schottky barrier electric field density functional theory}