Study on the Absorption Extraction of Germanium with CL-N235 Extraction Resin AITranslate

Department of Chemical Engineering, College of Environmental Science and Engineering, Chang'an University;Department of Chemistry, Yan'an University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the property of absorption and extraction of germanium from acidic solution. The results show that the resin can effectively separate and enrich germanium from Ge-containing solution with H2SO4 (pH 2.0-2.5 ) medium and tartaric acid. The adsorbed germanium can be quantitatively eluted with NH4 F solution. The preliminary study proved that the absorption was an anion exchange process.

KeyWords AITranslate

germanium CL-N235 extraction resin absorption extraction

1DeniseR.Kelex100 在稀土萃取中的应用[J].国外稀有金属,1984,(1):15-15.

2Harbuck D D,et al.Lix63 solvent extraction Ge study[J].Solvent Extraction and Ion Exchange,1991,9 (3):383.

3李世平.关于N235-酒石酸体系萃取分离锗锌的研究[J].稀有金属,1996,20(5):334-337. 被引量:3

4关根达也 腾藤译.溶剂萃取化学[M].北京:原子能出版社,1981.24.

5Zygmunt Marczenko.元素的分光光度测定[M].郑用熙,等译.北京:地质出版社,1983.240.

6北川 浩,等.吸附基础设计[M].鹿政理,译.北京:化学工业出版社,1983.33.

1戴财胜,罗道成.CL-N235树脂富集-分光光度法测定粉煤灰中痕量锗[J].冶金分析,2011,31(7):72-75.

1董岁明,张理平,董西芳.CL-N235萃淋树脂吸附分离金的研究[J].有色金属:冶炼部分,2007(1):14-16. 被引量:2

2蒋新宇,周春山,汤淑芳.N235萃取色谱法分离萃铟余液中锗的研究[J].稀有金属,2002,26(2):116-119. 被引量:1

3朱吕田.VC还原吸附分离—ICP—AES法测定钢铁及高温合金中痕量硒[J].冶钢科技,1992(1):55-58.

4胡鸿儒.聚氨酯泡沫塑料吸附分离金机理的探讨[J].黄金,1995,16(1):53-55. 被引量:6

5朱吕田,柳鸿明.巯基棉吸附分离—DBC—偶氮胂光度法测定钢铁中痕量铋[J].冶钢科技,1993(2):47-50.

6刘建,闫英桃,邵海欣,陈长江.CL-TBP萃淋树脂吸附分离镓(Ga)研究[J].化学通报,2001,64(2):119-121. 被引量:10

7朱吕田,柳鸿明.巯基棉吸附分离—1CP—AES法测定高温合金中痕量银[J].冶钢科技,1991(2):53-57.

8胡小玲,岳红,管萍,苏克和.D_(001)CC强酸性树脂吸附分离金银[J].西北大学学报:自然科学版,1999,29(5):406-408. 被引量:2

9朱永萍.血粉吸附金的物理化学行为[J].贵金属,1994,15(4):10-15. 被引量:1

10吴人驹.离子交换法除钼及其树脂再生的化学原理初探[J].中国钨业,1997,0(6):18-20. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF843[冶金工程—有色金属冶金]

Citation Information:

Study is made of the property of absorption and extraction of germanium from acidic solution. The results show that the resin can effectively separate and enrich germanium from Ge-containing solution with H2SO4 (pH 2.0-2.5 ) medium and tartaric acid. The adsorbed germanium can be quantitatively eluted with NH4 F solution. The preliminary study proved that the absorption was an anion exchange process.

quote

GB/T 7714-2015 [1] DONG Sui-ming, ZHANG Li-ping. Study on the Absorption Extraction of Germanium with CL-N235 Extraction Resin[J]. Rare Metals and Cemented Carbides, 2006(3): 1-4.
MLA [1] DONG Sui-ming, and ZHANG Li-ping. "Study on the Absorption Extraction of Germanium with CL-N235 Extraction Resin." Rare Metals and Cemented Carbides, no. 3, 2006, pp. 1-4.
APA [1] DONG Sui-ming, & ZHANG Li-ping. (2006). Study on the Absorption Extraction of Germanium with CL-N235 Extraction Resin. Rare Metals and Cemented Carbides(3), 1-4.
IEEE [1] DONG Sui-ming and ZHANG Li-ping, "Study on the Absorption Extraction of Germanium with CL-N235 Extraction Resin," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2006. keywords: {germanium;CL-N235 extraction resin;absorption extraction}