Analysis of Influencing Factors on Friction Properties of WC Coarse-grained Cemented Carbide AITranslate
Abstract AITranslate
The effects of carbon content,WC grain size,microporous structure,sintering temperature,heat treatment process,etc.on the friction properties of WC coarse-grained cemented carbide are reviewed.Through analysis,it is found that as the carbon content gradually increases,the friction properties of WC coarse-grained cemented carbide firstly increases and then decreases.When the WC coarse-grained cemented carbide has a microporous structure,excellent friction properties can be obtained.Appropriately increasing the sintering temperature can increase the free path of Co and contribute to the stability of the coarse-grained WC framework.The lower the Co content,and the larger the size of the coarse WC grains,the better the friction properties of the WC coarse-grained cemented carbide.Based on analysis,it is also found that the heat treatment process can effectively improve the friction properties of WC coarse-grained cemented carbide.
KeyWords AITranslate
1龙郑易,刘咏,贺跃辉,肖逸锋,周永贵,李芳.渗碳时间对梯度硬质合金显微组织和抗弯强度的影响[J].中国有色金属学报,2007,17(2):326-330. 被引量:9
2肖仲文,杨慧敏,白佳声.硬质合金气氛烧结过程中碳含量调整[J].硬质合金,2003,20(4):204-207. 被引量:7
3吴悦梅,熊计,赖人铭.碳含量对WC-Co硬质合金显微组织的影响及其控制[J].硬质合金,2008,25(3):179-185. 被引量:25
4周新华,王力民,赵声志,肖可俊.碳含量对粗晶硬质合金性能的影响[J].硬质合金,2009,26(2):82-86. 被引量:13
5陈明,吝楠,贺跃辉.碳含量对WC-Co-Ni-Fe-Cr硬质合金组织与性能的影响[J].硬质合金,2019,36(6):434-439. 被引量:4
6吴迪,熊志翔,白英龙,果世驹,杨霞,徐红霞.铸造碳化钨反应烧结制备粗晶硬质合金[J].粉末冶金材料科学与工程,2011,16(4):471-477. 被引量:3
7Haibin Wang,Mark Gee,Qingfan Qiu,Hannah Zhang,Xuemei Liu,Hongbo Nie,Xiaoyan Song,Zuoren Nie.Grain size effect on wear resistance of WC-Co cemented carbides under different tribological conditions[J].材料科学技术:英文版,2019,35(11):2435-2446. 被引量:5
8杨力,熊计,郭智兴,杨微,杨天恩,万维财,林子皓.WC晶粒度对硬质合金/不锈钢钎焊接头微观组织与性能的影响[J].硬质合金,2015,32(4):234-241. 被引量:6
9易怀星,王臣菊,孙斌,顾建兵.高温高压下碳化钨晶体的结构、力学、电子、光学以及热力学性能的第一性原理计算[J].原子与分子物理学报,2020,37(2):239-249. 被引量:3
10曹瑞军,林晨光,马旭东,谢兴铖,林中坤.钴含量对粗晶硬质合金磨损性能的影响[J].粉末冶金材料科学与工程,2015,20(6):860-864. 被引量:4
1曹瑞军,李开深,李腾飞,何盛亚.金刚石含量对金刚石强化硬质合金耐磨性影响[J].硬质合金,2022,39(3):165-171. 被引量:1
2张云龙,牛楚涵,牛广津,张宇民,李启荣,高志杨,张唯一.La_(2)O_(3)掺杂量对WC-12Co硬质合金微观结构和硬度的影响[J].中国钨业,2022,37(2):53-59.
1刘靖忠,窦明见,向天翔,吴建国.液相烧结法制备金刚石-WC-Co硬质合金复合材料性能影响因素的研究[J].硬质合金,2023,40(1):59-65.
1麻乐,袁彦超,刘诗博,王振汉,井长友,刘述梅,赵建青.可循环回收利用的本征导热聚六氢三嗪树脂研究[J].高分子学报,2021,52(9):1156-1164. 被引量:2
2牛玉杰,褚晨,庞雅贤,沈亚欣,李立鹏,刘清萍,张荣.大学生血清金属水平与抑郁、焦虑关联的横断面研究[J].环境与职业医学,2021,38(10):1069-1076. 被引量:2
3张德银,韦鹏辉,黄语瑄,陈心达.一种新型抗干扰复合智能火警探测器研制[J].中国科技信息,2021(21):76-78.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The effects of carbon content,WC grain size,microporous structure,sintering temperature,heat treatment process,etc.on the friction properties of WC coarse-grained cemented carbide are reviewed.Through analysis,it is found that as the carbon content gradually increases,the friction properties of WC coarse-grained cemented carbide firstly increases and then decreases.When the WC coarse-grained cemented carbide has a microporous structure,excellent friction properties can be obtained.Appropriately increasing the sintering temperature can increase the free path of Co and contribute to the stability of the coarse-grained WC framework.The lower the Co content,and the larger the size of the coarse WC grains,the better the friction properties of the WC coarse-grained cemented carbide.Based on analysis,it is also found that the heat treatment process can effectively improve the friction properties of WC coarse-grained cemented carbide.
quote
| GB/T 7714-2015 | [1] QIN Qin, WANG Nan, YAN Zi-yi, et al. Analysis of Influencing Factors on Friction Properties of WC Coarse-grained Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2021(5): 82-86. |
| MLA | [1] QIN Qin, et al., "Analysis of Influencing Factors on Friction Properties of WC Coarse-grained Cemented Carbide." Rare Metals and Cemented Carbides, no. 5, 2021, pp. 82-86. |
| APA | [1] QIN Qin, WANG Nan, YAN Zi-yi, TIAN Jin-xing, TANG Shi-jia, YANG Hao-dong, & HUANG Tai-bo. (2021). Analysis of Influencing Factors on Friction Properties of WC Coarse-grained Cemented Carbide. Rare Metals and Cemented Carbides(5), 82-86. |
| IEEE | [1] QIN Qin, WANG Nan, YAN Zi-yi, TIAN Jin-xing, TANG Shi-jia, YANG Hao-dong, and HUANG Tai-bo, "Analysis of Influencing Factors on Friction Properties of WC Coarse-grained Cemented Carbide," Rare Metals and Cemented Carbides, no. 5, pp. 82-86, 2021. keywords: {coarse-grained cemented carbide;WC;friction property;carbon content;binder;microporous structure} |