Influence of Sintering Temperature on WC-TiC-Co Double-phase Alloy AITranslate

Zhuzhou Hard Alloy Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Overall inspection and analysis are made of the structure of WC-TiC-Co double-phase alloys. sintered at different temperatures.Cutting tests are carried out on their related tips. The results show that regardless of the sintering temperature, free WC phases are found in all the double-phase alloys made from WC-TiC 70: 30 by mass saturated solid solution and Co powder. Its relative amount varies inversely with the sintering temperature, while the grain size of the carbide varies directly. The cutting life of the specimen sintered at 1480℃ is the longest.

KeyWords AITranslate

sintering temperature WC-TiC-Co structure cutting life influence

1罗军明,廖佳,陆磊,徐吉林.微波烧结制备WC-TiC-Co硬质合金的组织和性能研究[J].材料导报,2013,27(20):103-105. 被引量:5

2郭鸿镇,姚泽坤,花田修治,吉见享祜.快速凝固Nb_3Al-Nb固溶体两相合金的组织与性能[J].中国有色金属学报,1998,8(3):472-476. 被引量:7

3Lapt.,AV,唐丹.孔隙度对两相合金抗弯强度和断裂韧性的影响[J].国外难熔金属与硬质材料,1997,13(1):29-34.

4QU Xuanhui, GAO Jianxiang, QIN Mingli, and LEI Changming.Rheologic behavior and PIM processing of WC-TiC-Co powder feedstock[J].稀有金属:英文版,2004,23(3):240-240.

5熊继,羊建高,李懿,张静静.稀土对硬质合金中WC晶粒度和碳的影响[J].硬质合金,1994,11(3):134-137. 被引量:14

6TomaVasile,李仁琼,陈满元.通过添加(Ta,Nb)C来提高WC-TiC-Co合金的性能[J].国外难熔金属与硬质材料,2003,19(2):1-3. 被引量:1

7范志康,梁淑华,肖鹏.Cu W假两相合金的熔渗参数[J].中国有色金属学报,2001,11(z1):102-104. 被引量:9

8贺从训,汪有明,马福康.稀土在硬质合金中的应用研究[J].硬质合金,1994,11(3):129-133. 被引量:15

9XuanhuiQu,JianxiangGao,MingliQin,ChangmingLei.Rheologic behavior and PIM processing of WC-TiC-Co powder feedstock[J].北京科技大学学报:英文版,2004,11(4):334-337.

10胡焕校,刘静.金刚石锯片胎体的耐磨性[J].中国有色金属学报,2000,10(3):400-403. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

Overall inspection and analysis are made of the structure of WC-TiC-Co double-phase alloys. sintered at different temperatures.Cutting tests are carried out on their related tips. The results show that regardless of the sintering temperature, free WC phases are found in all the double-phase alloys made from WC-TiC 70: 30 by mass saturated solid solution and Co powder. Its relative amount varies inversely with the sintering temperature, while the grain size of the carbide varies directly. The cutting life of the specimen sintered at 1480℃ is the longest.

quote

GB/T 7714-2015 [1] WEN Hong-wei. Influence of Sintering Temperature on WC-TiC-Co Double-phase Alloy[J]. Rare Metals and Cemented Carbides, 1996(3): 28-32.
MLA [1] WEN Hong-wei. "Influence of Sintering Temperature on WC-TiC-Co Double-phase Alloy." Rare Metals and Cemented Carbides, no. 3, 1996, pp. 28-32.
APA [1] WEN Hong-wei. (1996). Influence of Sintering Temperature on WC-TiC-Co Double-phase Alloy. Rare Metals and Cemented Carbides(3), 28-32.
IEEE [1] WEN Hong-wei, "Influence of Sintering Temperature on WC-TiC-Co Double-phase Alloy," Rare Metals and Cemented Carbides, no. 3, pp. 28-32, 1996. keywords: {sintering temperature;WC-TiC-Co;structure;cutting life;influence}