Research of Leaching and Separation Experiment on Gallium from Gallium-rich Material AITranslate

Zijin Mining Group Co., Ltd. State Key Laboratory of Comprehensive Utilization of Low-Grade Refractory Gold Resources
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The experimental study was conducted on NaOH leaching and ion exchange separation of gallium -rich material obtained by concentrate roasting-calcine sulfuric acid selective enriching of alunite. The re- sults show that during the NaOH leaching, the gallium leaching rate can reach 98.84% under the conditions of 75 % NaOH concentration, 15 rain leaching time, 3 : 1 liquid-solid ratio, 300 r/min agitating velocity. During the ion exchange,the gallium adsorption rate is 71.4% under the conditions of the NaOH concentration of 150 g/L in adsorbed solution,Rexp-31 resin dosage of 150 g/L,spray rate of 5 mL/min,resin bed height of 15 cm. The gallium desorption rate can is 88.16% ,under the conditions of NaOH and Na2S concentration in the desorption agent of 160 g/L and 50 g/L,respectively, liquid-solid ratio of 10 :1, de- sorption duration of 1 h.

KeyWords AITranslate

gallium-rich material gallium NaOH leaching ion exchange adsorption desorption

1王金超.镓生产工艺及用途[J].四川有色金属,2003(4):14-19. 被引量:8

2赵秦生.镓的市场、生产、价格与发展[J].稀有金属与硬质合金,2001,29(4):42-44. 被引量:8

3KIDA A, SIROHASE T, KAWAGUCHI M. Metals con- tents including precious metals in waste personal com- puters[J]. Material Cyeles & Waste Management Re- search, 2009,20 (2) : 59-69.

4KATRAK F E, AGARWAL J C. Gallium: Long-run supply[J]. Journal of Metals,1981,33(9) :33-36.

5翟秀静,吕子剑.镓冶金[M].北京:冶金工业出版社,2010:51-52.

6PUVVADA G V K, CHANDRASEKHAR K, RAM- ACHANDRARAO P. Solvent extraction of gallium from an Indian Bayer process liquor using Kelex-100 [J]. Minerals Engineering, 1996,9 (10) . 1 049-1 058.

7KEKESI T. Gallium extraction from synthetic Bayer liq- uors using Ke!ex 100-kerosene,the effect of loading and stripping conditions on selectivity[J]. Hydrometallurgy, 2007,88(1/4) . 170-179.

8芦小飞,王磊,王新德,牛学坤.金属镓提取技术进展[J].有色金属,2008,60(4):105-108. 被引量:21

9苏毅,李国斌,罗康碧.金属镓提取研究进展[J].湿法冶金,2003,22(1):9-13. 被引量:12

10梁祥济,王福生.明矾石矿床中钒、镓萃取实验和综合利用的建议[J].矿床地质,1999,18(3):276-284. 被引量:9

1魏娟,王亚雄,张丽,郎春燕.聚氨酯泡沫塑料分离富集攀枝花钒钛磁铁矿尾矿中镓[J].广州化工,2018,46(2):59-62.

2郭文超,李望,朱晓波,张治国,张传祥.P507萃取煤矸石硫酸浸出液中镓的实验研究[J].稀有金属与硬质合金,2022,50(4):28-32. 被引量:2

1甘胤,禄瑜.利用煤矸石提取有价元素技术的研究进展[J].煤炭加工与综合利用,2023(5):85-91.

2康超,乔金鹏,杨胜超,彭超,付元鹏,刘斌,刘建荣,Tatiana Aleksandrova,段晨龙.煤矸石中有价关键金属活化提取研究进展[J].化工学报,2023,74(7):2783-2799.

1牟文宁,翟玉春,刘岩,刘娇.高浓度NaOH浸出红土镍矿中SiO_2的研究[J].东北大学学报:自然科学版,2009,30(5):708-711. 被引量:7

2张力,李光强,隋智通.由改性高钛渣浸出制备富钛料的研究[J].矿产综合利用,2002(6):6-9. 被引量:17

3路辉,谢刚,俞小花,谢红艳.电炉钛渣碱浸除硅、铝与碱浸渣的预氧化焙烧动力学[J].过程工程学报,2010,10(3):513-521. 被引量:8

4易小祥,李亚伟,杨大兵.含钛高炉渣选择性析出分离技术研究进展[J].矿产保护与利用,2007,27(6):42-46. 被引量:4

5王瑞永.明矾石精矿水浸—结晶法制备硫酸钾试验研究[J].有色冶金设计与研究,2014,35(3):14-16. 被引量:2

6李玉海,娄太平,隋智通.含钛高炉渣中钛组分选择性富集及钙钛矿结晶行为[J].中国有色金属学报,2000,10(5):719-722. 被引量:45

7邓慧东,任燕,张建国,刘国宏,舒祖骏,周志全,支梅峰,张海燕.离子交换法从含磷溶液中提取钼的研究[J].铀矿冶,2015,34(1):12-16. 被引量:5

8吴辛友.离子交换分离氯代磺酚C光度法测定氟钽酸钾中微量铌[J].有色金属分析通讯,1992(1):17-19.

9张力,李光强,娄太平,隋智通.高钛渣中钛组分的选择性富集与长大[J].金属学报,2002,38(4):400-402. 被引量:18

10卢新宇,许曼.从废钼催化剂中回收有价金属试验研究[J].湿法冶金,2013,32(5):319-322. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF843.1[冶金工程—有色金属冶金]

Citation Information:

The experimental study was conducted on NaOH leaching and ion exchange separation of gallium -rich material obtained by concentrate roasting-calcine sulfuric acid selective enriching of alunite. The re- sults show that during the NaOH leaching, the gallium leaching rate can reach 98.84% under the conditions of 75 % NaOH concentration, 15 rain leaching time, 3 : 1 liquid-solid ratio, 300 r/min agitating velocity. During the ion exchange,the gallium adsorption rate is 71.4% under the conditions of the NaOH concentration of 150 g/L in adsorbed solution,Rexp-31 resin dosage of 150 g/L,spray rate of 5 mL/min,resin bed height of 15 cm. The gallium desorption rate can is 88.16% ,under the conditions of NaOH and Na2S concentration in the desorption agent of 160 g/L and 50 g/L,respectively, liquid-solid ratio of 10 :1, de- sorption duration of 1 h.

quote

GB/T 7714-2015 [1] HUANG Zhong-sheng. Research of Leaching and Separation Experiment on Gallium from Gallium-rich Material[J]. Rare Metals and Cemented Carbides, 2016(4): 5-10.
MLA [1] HUANG Zhong-sheng. "Research of Leaching and Separation Experiment on Gallium from Gallium-rich Material." Rare Metals and Cemented Carbides, no. 4, 2016, pp. 5-10.
APA [1] HUANG Zhong-sheng. (2016). Research of Leaching and Separation Experiment on Gallium from Gallium-rich Material. Rare Metals and Cemented Carbides(4), 5-10.
IEEE [1] HUANG Zhong-sheng, "Research of Leaching and Separation Experiment on Gallium from Gallium-rich Material," Rare Metals and Cemented Carbides, no. 4, pp. 5-10, 2016. keywords: {gallium-rich material;gallium;NaOH leaching;ion exchange;adsorption;desorption}