daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Digital Light Processing 3D Printing of PDMS-Based Soft and Elastic Materials with Tunable Mechanical Properties AITranslate

CSIRO Manufacturing;CSIRO Manufacturing;CSIRO Manufacturing;CSIRO Manufacturing;CSIRO Manufacturing;CSIRO Data61;CSIRO Manufacturing
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, a family of thiourea containing silicone-based photoresins suitable for creating silicone objects with excellent elasticity was developed for use in conventional digital light processing 3D printers. Rapid manufacturing of silicone products is highly desirable for small-volume manufacturing, especially for the application of customer-specific medical devices. However, because of their intrinsic high viscosity and lack of intermolecular interactions, 3D printing with silicone remains an ongoing challenge as suitable resins are not commercially available. To improve the elasticity of 3D-printed silicones, dynamic noncovalent intermolecular interactions between polymer chains were increased through the introduction of thiourea groups. Furthermore, a molecular design strategy was implemented based on utilizing “oligomeric” and “polymeric” PDMS units to adjust the ratio of thiourea segments. The cured silicone elastomer developed here displayed a maximum elongation of up to 1000% under tensile load and excellent cyclic compression durability. Moreover, this approach allowed for the 3D printing of PDMS-based objects with complex microarchitectures, high resolution, excellent surface finishing, and low cytotoxicity. The silicone thiourea resins have potential application in medical devices, wearable devices, and soft robotics.

KeyWords AITranslate

additive manufacturing digital light processing rapid prototyping silicone siloxane dynamic bonding noncytotoxic cyclic loading
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00260

Chinese Library Classification Number:

Citation Information:

Herein, a family of thiourea containing silicone-based photoresins suitable for creating silicone objects with excellent elasticity was developed for use in conventional digital light processing 3D printers. Rapid manufacturing of silicone products is highly desirable for small-volume manufacturing, especially for the application of customer-specific medical devices. However, because of their intrinsic high viscosity and lack of intermolecular interactions, 3D printing with silicone remains an ongoing challenge as suitable resins are not commercially available. To improve the elasticity of 3D-printed silicones, dynamic noncovalent intermolecular interactions between polymer chains were increased through the introduction of thiourea groups. Furthermore, a molecular design strategy was implemented based on utilizing “oligomeric” and “polymeric” PDMS units to adjust the ratio of thiourea segments. The cured silicone elastomer developed here displayed a maximum elongation of up to 1000% under tensile load and excellent cyclic compression durability. Moreover, this approach allowed for the 3D printing of PDMS-based objects with complex microarchitectures, high resolution, excellent surface finishing, and low cytotoxicity. The silicone thiourea resins have potential application in medical devices, wearable devices, and soft robotics.

quote

GB/T 7714-2015 [1] Ke Du, Johan Basuki, Veronica Glattauer, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00260.
MLA [1] Ke Du, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00260.
APA [1] Ke Du, Johan Basuki, Veronica Glattauer, Caroline Mesnard, Anh Tuan Nguyen, David L. J. Alexander, & Timothy C. Hughes. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00260
IEEE [1] Ke Du, Johan Basuki, Veronica Glattauer, Caroline Mesnard, Anh Tuan Nguyen, David L. J. Alexander, and Timothy C. Hughes, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00260. keywords: {additive manufacturing;digital light processing;rapid prototyping;silicone;siloxane;dynamic bonding;noncytotoxic;cyclic loading}