daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on the Catalytic Performance of Copper-Based Composite Oxides for CO Oxidation AITranslate

School of Energy and Environment,Inner Mongolia University of Science and Technology;School of Energy and Environment,Inner Mongolia University of Science and Technology;School of Energy and Environment,Inner Mongolia University of Science and Technology;School of Energy and Environment,Inner Mongolia University of Science and Technology;School of Energy and Environment,Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Copper-based composite oxide catalysts were prepared by impregnation method usingγ-Al2O3 spheres as carrier and Cu-Ce,Cu-Mn,Cu-Zr or Cu-Co as active components.The influence of different components,doping ratio and reaction temperature on the catalytic performance of copper-based composite oxides for CO oxidation was studied.The surface properties,reducibility,surface morphology and phase composition of the catalysts were analyzed by BET,CO-TPR,SEM and XRD.The results show that under the optimal doping ratio,the order of catalytic activity of copper-based composite oxides with different active components is as follows:Cu-Ce composite oxide>Cu-Mn composite oxide>Cu-Zr composite oxide>Cu-Co composite oxide.Among them,the Cu-Ce composite oxide exhibits the best performance,and the optimal doping ratio is n(Cu)∶n(Ce)=1∶0.1.This catalyst achieves a CO conversion rate of over 80%at 150~200℃and maintains a CO conversion rate of over 90%above 200℃.Characterization results indicate that the excellent catalytic activity of the Cu-Ce composite oxide is attributed to the uniform dispersion of active components,large specific surface area,good pore structure and strong redox ability.

KeyWords AITranslate

copper-based complex oxide catalytic oxidation of CO impregnation method γ-Al2O3
No data

Basic Information:

DOI:

Chinese Library Classification Number:TQ426.6[化学工程]

Citation Information:

Copper-based composite oxide catalysts were prepared by impregnation method usingγ-Al2O3 spheres as carrier and Cu-Ce,Cu-Mn,Cu-Zr or Cu-Co as active components.The influence of different components,doping ratio and reaction temperature on the catalytic performance of copper-based composite oxides for CO oxidation was studied.The surface properties,reducibility,surface morphology and phase composition of the catalysts were analyzed by BET,CO-TPR,SEM and XRD.The results show that under the optimal doping ratio,the order of catalytic activity of copper-based composite oxides with different active components is as follows:Cu-Ce composite oxide>Cu-Mn composite oxide>Cu-Zr composite oxide>Cu-Co composite oxide.Among them,the Cu-Ce composite oxide exhibits the best performance,and the optimal doping ratio is n(Cu)∶n(Ce)=1∶0.1.This catalyst achieves a CO conversion rate of over 80%at 150~200℃and maintains a CO conversion rate of over 90%above 200℃.Characterization results indicate that the excellent catalytic activity of the Cu-Ce composite oxide is attributed to the uniform dispersion of active components,large specific surface area,good pore structure and strong redox ability.

quote

GB/T 7714-2015 [1] ZHANG Yu-xuan, YIN Yi-zhen, JIA Zhi-yuan, et al. Study on the Catalytic Performance of Copper-Based Composite Oxides for CO Oxidation[J]. Rare Metals and Cemented Carbides, 2025(2): 69-76.
MLA [1] ZHANG Yu-xuan, et al., "Study on the Catalytic Performance of Copper-Based Composite Oxides for CO Oxidation." Rare Metals and Cemented Carbides, no. 2, 2025, pp. 69-76.
APA [1] ZHANG Yu-xuan, YIN Yi-zhen, JIA Zhi-yuan, JIANG Ming-ming, & GONG Zhi-jun. (2025). Study on the Catalytic Performance of Copper-Based Composite Oxides for CO Oxidation. Rare Metals and Cemented Carbides(2), 69-76.
IEEE [1] ZHANG Yu-xuan, YIN Yi-zhen, JIA Zhi-yuan, JIANG Ming-ming, and GONG Zhi-jun, "Study on the Catalytic Performance of Copper-Based Composite Oxides for CO Oxidation," Rare Metals and Cemented Carbides, no. 2, pp. 69-76, 2025. keywords: {copper-based complex oxide;catalytic oxidation of CO;impregnation method;γ-AlO}