Review of Process and Equipment in Tungsten Smelting Industry AITranslate

School of Materials Science and Engineering, Guilin University of Technology;School of Materials Science and Engineering, Guilin University of Technology;School of Materials Science and Engineering, Guilin University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development is reviewed of process and equipment in domestic tungsten smelting industry.The process development is oriented towards energy saving and environmental protection.Guided by the market and policy,the new process and equipment would be gradually applied to further improve environment-friendly production level in tungsten smelting industry.

KeyWords AITranslate

scheelite tungsten smelting new process and equipment energy saving and environmental protection environmental-friendly production

1姜瑞,曾红云,王强.氨氮废水处理技术研究进展[J].环境科学与管理,2013,38(6):131-134. 被引量:65

2路辉,谢刚,俞小花,李荣兴.仲钨酸铵结晶母液处理技术研究进展[J].稀有金属与硬质合金,2009,37(4):44-47. 被引量:5

3杨晓峰,刘全军.我国白钨矿的资源分布及选矿的现状和进展[J].矿业快报,2008,24(4):6-9. 被引量:27

4张贵清,尚广浩,肖连生.纳滤法处理仲钨酸铵结晶母液的研究[J].稀有金属,2007,31(3):346-350. 被引量:7

5姚丽华,陈树茂,杨红.钨冶炼离子交换工艺废水的治理[J].湖南有色金属,2007,23(1):42-44. 被引量:8

6赵中伟.用于处理高浓度钨酸钠溶液的离子交换新工艺[J].中国钨业,2005,20(1):33-35. 被引量:17

7黄长庚.钨冶炼产业现状与建议[J].中国钨业,2004,19(6):14-15. 被引量:2

8万林生,晏慧娟,肖学有,陈帮明,王辉.我国钨冶炼离子交换工艺的技术发展与工艺评价[J].中国钨业,2003,18(6):31-33. 被引量:20

9陈树茂,郭永忠.离子交换法处理仲钨酸铵结晶母液试验与实践[J].中国钨业,2001,16(3):22-24. 被引量:14

1杨亮,万林生,舒柳飞.(NH_4)_3PO_4-NH_3·H_2O-H_2O体系中磷酸铵溶解度[J].有色金属科学与工程,2016,7(2):39-42. 被引量:1

2易贤荣,徐双.高纯仲钨酸铵萃取法清洁生产工艺应用研究[J].中国钨业,2016,31(6):54-59. 被引量:3

3叶田田,刘立,谌建宇,刘钢,王振兴.钨冶炼行业清洁生产评价指标体系探讨[J].中国钨业,2020,35(4):45-51.

4黄国蕾,陈云嫩,朱春.钨冶炼含砷和氨氮废水处理的研究进展[J].应用化工,2023,52(3):844-850.

5杨坤,高亮,陈浩林.云南省钨产业现状及展望[J].有色金属设计,2023,50(1):16-19.

1何艺,徐双,靳晓勤,林晓,陶莉,许海青.中国钨渣产生特性及资源化利用技术研究现状[J].中国钨业,2018,33(5):51-56. 被引量:8

2薛祥,杨亮,万林生,何人桂.氟化钙在磷酸铵-氨水溶液中的溶解行为研究[J].江西冶金,2019,39(4):7-11.

3但宁宁,李江涛.高纯仲钨酸铵产品制备工艺现状及发展前景[J].粉末冶金材料科学与工程,2020,25(5):363-368. 被引量:2

4张威,徐双,余春荣.仲钨酸铵冶炼中金属平衡管理研究[J].有色冶金设计与研究,2022,43(3):18-21.

1姚珍刚.论中国钨冶炼工业的技术升级[J].中国钨业,2004,19(6):16-18. 被引量:10

2林金嘉.宝钢高炉工艺技术和装备的演变[J].炼铁,2005,24(B09):88-91.

3杨阳,付东升,郑化安,张云.电炉炼钢与针状焦发展现状及市场分析[J].燃料与化工,2014,45(5):5-8. 被引量:9

4庄福礼,陈学刚,俞兵,邢国华,马绍兵.锌浸渣的侧吹熔炼技术与装备研究[J].中国有色冶金,2013,42(6):5-10. 被引量:1

5杨敏陔.我国钨冶炼工业的进展[J].中国钨业,1989(10):13-17.

6许继芳,盛敏奇,万康,龚柳,张捷宇.CaO-5%MgO-Al_2O_3-SiO_2-0.5%‘FeO’体系低SiO_2区域熔化性能[J].钢铁,2014,49(2):24-28. 被引量:2

7许继芳,张捷宇,翁文凭,李建朝,盛敏奇.硅-锰脱氧产物对精炼渣凝固特性的影响[J].上海金属,2016,38(2):46-50.

8张丽娜.双床平炉供连铸钢水的冶炼操作探讨[J].鞍钢技术,1994(6):14-17.

9王海燕,侯利华.钨精矿提钨工艺中硫化除钼条件的控制[J].中国钨业,2002,17(2):33-33. 被引量:1

10陈建新,张雪萍.韶钢350m^3高炉供料及上料系统的设计[J].钢铁,1999,34(9):16-18. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]

Citation Information:

The latest development is reviewed of process and equipment in domestic tungsten smelting industry.The process development is oriented towards energy saving and environmental protection.Guided by the market and policy,the new process and equipment would be gradually applied to further improve environment-friendly production level in tungsten smelting industry.

quote

GB/T 7714-2015 [1] LI Yi-bing, LIU Kai-zhong, ZHANG Da-zeng. Review of Process and Equipment in Tungsten Smelting Industry[J]. Rare Metals and Cemented Carbides, 2015(3): 1-4.
MLA [1] LI Yi-bing, et al., "Review of Process and Equipment in Tungsten Smelting Industry." Rare Metals and Cemented Carbides, no. 3, 2015, pp. 1-4.
APA [1] LI Yi-bing, LIU Kai-zhong, & ZHANG Da-zeng. (2015). Review of Process and Equipment in Tungsten Smelting Industry. Rare Metals and Cemented Carbides(3), 1-4.
IEEE [1] LI Yi-bing, LIU Kai-zhong, and ZHANG Da-zeng, "Review of Process and Equipment in Tungsten Smelting Industry," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2015. keywords: {scheelite;tungsten smelting;new process and equipment;energy saving and environmental protection;environmental-friendly production}