Unconventional Superconductivity at LaVO3/SrTiO3 Interfaces Unconventional Superconductivity at LaVO3/SrTiO3 Interfaces AITranslate

Indian Institute of Science Education and Research (IISER); Indian Institute of Science Education and Research (IISER); Indian Institute of Science Education and Research (IISER); Institute of Nano Science and Technology;Indian Institute of Science;Indian Institute of Science; Institute of Nano Science and Technology; Indian Institute of Science Education and Research (IISER)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The conducting interfaces of perovskite oxides are fertile playgrounds of diverse quantum phenomena, and they are potentially important for applications in superconducting nanoelectronic devices. We discovered that the interfaces between the Mott-insulator LaVO3 and the band-insulator SrTiO3 host two-dimensional superconductivity below Tc ≈ 250 mK. Our band structure calculations indicate that for these interfaces, multiple bands (the V and the Ti d bands) cross the Fermi energy where the V d electrons also carry a magnetic moment, thereby raising the possibility of an unconventional order parameter (OP) of the superconducting phase. We have fabricated subsurface soft metallic point-contacts at the LaVO3/SrTiO3 interfaces to probe the OP symmetry spectroscopically through the measurement of Andreev reflection. The spectroscopic features strongly deviate from the expectations within the conventional Bardeen–Cooper–Schriefer framework and support the existence of an unconventional order parameter.

KeyWords AITranslate

oxide 2DEGs Mott insulator unconventional superconductivity multiband superconductivity Andreev reflection spectroscopy
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01027

Chinese Library Classification Number:

Citation Information:

The conducting interfaces of perovskite oxides are fertile playgrounds of diverse quantum phenomena, and they are potentially important for applications in superconducting nanoelectronic devices. We discovered that the interfaces between the Mott-insulator LaVO3 and the band-insulator SrTiO3 host two-dimensional superconductivity below Tc ≈ 250 mK. Our band structure calculations indicate that for these interfaces, multiple bands (the V and the Ti d bands) cross the Fermi energy where the V d electrons also carry a magnetic moment, thereby raising the possibility of an unconventional order parameter (OP) of the superconducting phase. We have fabricated subsurface soft metallic point-contacts at the LaVO3/SrTiO3 interfaces to probe the OP symmetry spectroscopically through the measurement of Andreev reflection. The spectroscopic features strongly deviate from the expectations within the conventional Bardeen–Cooper–Schriefer framework and support the existence of an unconventional order parameter.

quote

GB/T 7714-2015 [1] Soumyadip Halder, Mona Garg, Nikhlesh Singh Mehta, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01027.
MLA [1] Soumyadip Halder, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01027.
APA [1] Soumyadip Halder, Mona Garg, Nikhlesh Singh Mehta, Anamika Kumari, Rajesh Sharma, Tanmoy Das, Suvankar Chakraverty, & Goutam Sheet. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01027
IEEE [1] Soumyadip Halder, Mona Garg, Nikhlesh Singh Mehta, Anamika Kumari, Rajesh Sharma, Tanmoy Das, Suvankar Chakraverty, and Goutam Sheet, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01027. keywords: {oxide 2DEGs Mott insulator unconventional superconductivity multiband superconductivity Andreev reflection spectroscopy}