Coral-Inspired Asymmetrically Porous Radiative Cooling Biofilm with Thermoplastic Polyurethane-Enhanced Mechanical Tolerance as Building Energy-Saving Envelope AITranslate
Abstract AITranslate
Passive radiative cooling (PRC) is an emerging energy-free cooling strategy that reflects solar radiation and emits heat into outer space to achieve a cooling temperature below ambient. Despite notable progress, large-scale commercialization of PRC films for practical applications still remains a challenge, specifically in terms of their ability to envelope complex surfaces and the mechanical tolerance for prolonged utilization. Herein, we fabricated an asymmetrically coral-like porous cellulose acetate/thermoplastic polyurethane (CA/TPU) film with controllable size and thickness inspired by natural coral. The asymmetrical structure with coral-shaped pores enhances the scattering of sunlight across the apertures, and the introduction of hydroxyapatite nanorods (HAP NRs) strengthens the infrared emission. Additionally, the cross-linking between the polymer molecular chains of CA and elastomer TPU enables the PRC biofilm outstanding mechanical tolerance and flexibility which can be stretched to 236.2%. As a result, the PRC biofilm exhibits high solar reflectivity of 97.26% and infrared emissivity of 97.22%, contributing to a subambient temperature drop of 9.2 °C under solar radiation of 1550 W/m2. The PRC biofilm is expected to be utilized as an energy-saving envelope structure for buildings, vehicles, and textiles in practical applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01914
Chinese Library Classification Number:
Citation Information:
Passive radiative cooling (PRC) is an emerging energy-free cooling strategy that reflects solar radiation and emits heat into outer space to achieve a cooling temperature below ambient. Despite notable progress, large-scale commercialization of PRC films for practical applications still remains a challenge, specifically in terms of their ability to envelope complex surfaces and the mechanical tolerance for prolonged utilization. Herein, we fabricated an asymmetrically coral-like porous cellulose acetate/thermoplastic polyurethane (CA/TPU) film with controllable size and thickness inspired by natural coral. The asymmetrical structure with coral-shaped pores enhances the scattering of sunlight across the apertures, and the introduction of hydroxyapatite nanorods (HAP NRs) strengthens the infrared emission. Additionally, the cross-linking between the polymer molecular chains of CA and elastomer TPU enables the PRC biofilm outstanding mechanical tolerance and flexibility which can be stretched to 236.2%. As a result, the PRC biofilm exhibits high solar reflectivity of 97.26% and infrared emissivity of 97.22%, contributing to a subambient temperature drop of 9.2 °C under solar radiation of 1550 W/m2. The PRC biofilm is expected to be utilized as an energy-saving envelope structure for buildings, vehicles, and textiles in practical applications.
quote
| GB/T 7714-2015 | [1] Haoran Cai, Shuangjiang Feng, Mingxin Feng, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01914. |
| MLA | [1] Haoran Cai, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01914. |
| APA | [1] Haoran Cai, Shuangjiang Feng, Mingxin Feng, Xu He, Chenghuan Liu, Man He, Xiaohai Bu, Jun Huang, & Yuming Zhou. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01914 |
| IEEE | [1] Haoran Cai, Shuangjiang Feng, Mingxin Feng, Xu He, Chenghuan Liu, Man He, Xiaohai Bu, Jun Huang, and Yuming Zhou, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01914. keywords: {radiative cooling;corallike porous film;asymmetrically structure;mechanical tolerance;energysaving envelope} |