daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Narrow Bandgap-Conjugated Polymers Incorporating Thieno[3,2-c]pyridine-4,6-Dione-Derived Isoindigo for Organic Field-Effect Transistor Applications AITranslate

Donghua University; Donghua University; Hunan University; Donghua University; Donghua University; Donghua University; Hunan University; Donghua University; Donghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A building block of thieno[3,2-c]pyridine-4,6-dione-derived isoindigo (TPyI) was designed and synthesized. TPyI has a planar structure with strong S···O noncovalent interactions according to both quantum chemistry simulations and single-crystal structure information. Two TPyI-based D–A polymers, including regioirregular and regioregular versions (ri-PTPyI2T and rr-PTPyI2T), were synthesized since TPyI is geometrically asymmetrical. The polymer thin films exhibited narrow bandgaps of approximately 1.19 eV and p-type charge transport characteristics, with maximum hole mobilities of 0.14 cm2/(V s) for ri-PTPyI2T and 0.32 cm2/(V s) for rr-PTPyI2T, respectively. This study highlights the design and synthesis of TPyI-based narrow band gap-conjugated polymers that are promising for organic electronics.

KeyWords AITranslate

conjugated polymers isoindigo narrow bandgap regioregular hole mobility
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01532

Chinese Library Classification Number:

Citation Information:

A building block of thieno[3,2-c]pyridine-4,6-dione-derived isoindigo (TPyI) was designed and synthesized. TPyI has a planar structure with strong S···O noncovalent interactions according to both quantum chemistry simulations and single-crystal structure information. Two TPyI-based D–A polymers, including regioirregular and regioregular versions (ri-PTPyI2T and rr-PTPyI2T), were synthesized since TPyI is geometrically asymmetrical. The polymer thin films exhibited narrow bandgaps of approximately 1.19 eV and p-type charge transport characteristics, with maximum hole mobilities of 0.14 cm2/(V s) for ri-PTPyI2T and 0.32 cm2/(V s) for rr-PTPyI2T, respectively. This study highlights the design and synthesis of TPyI-based narrow band gap-conjugated polymers that are promising for organic electronics.

quote

GB/T 7714-2015 [1] FangLiang Dong, Yu Zhang, Huan Wei, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01532.
MLA [1] FangLiang Dong, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01532.
APA [1] FangLiang Dong, Yu Zhang, Huan Wei, Chang Li, Zheng Li, Jiaxing Gao, Yuanyuan Hu, Zheng Tang, & Ming Wang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01532