MoS2 Nanostructures for Solar Hydrogen Generation via Membraneless Electrochemical Water Splitting MoS2 Nanostructures for Solar Hydrogen Generation via Membraneless Electrochemical Water Splitting AITranslate
Abstract AITranslate
Storing and delivering green hydrogen generated by solar energy have the potential to significantly supplement and disburse the share of promising but intermittent renewable energy. In this scenario, robust materials capable of delivering solar-driven electrochemical water splitting for hydrogen generation provide an interesting protocol that is applicable to all sectors of energy. Electrochemical water splitting is the conventional and most prevalent technique for hydrogen generation, which utilizes platinum-based materials for the hydrogen evolution reaction (HER). However, these platinum-based noble metal catalysts possess poor cyclic stability, limiting their commercial application for economical hydrogen generation. Therefore, the development of efficient non-noble metal-based electrocatalysts is urgently needed to produce cost-competitive hydrogen energy. Several kinds of non-noble metal-based heterogeneous electrocatalysts, including carbides, sulfides, selenides, oxides, and phosphides, have been developed and studied. The unique physicochemical properties of carbonaceous materials make them promising candidates to support catalysts. In this paper, molybdenum disulfide (MoS2) nanomaterial catalysts have been synthesized, deposited on carbon fiber (CF)-based materials, and then used for solar hydrogen generation by membraneless electrochemical water splitting. At 430 W/m2 irradiation and 35 °C working temperature, the solar-to-hydrogen conversion efficiency is found to be 2.46%.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01415
Chinese Library Classification Number:
Citation Information:
Storing and delivering green hydrogen generated by solar energy have the potential to significantly supplement and disburse the share of promising but intermittent renewable energy. In this scenario, robust materials capable of delivering solar-driven electrochemical water splitting for hydrogen generation provide an interesting protocol that is applicable to all sectors of energy. Electrochemical water splitting is the conventional and most prevalent technique for hydrogen generation, which utilizes platinum-based materials for the hydrogen evolution reaction (HER). However, these platinum-based noble metal catalysts possess poor cyclic stability, limiting their commercial application for economical hydrogen generation. Therefore, the development of efficient non-noble metal-based electrocatalysts is urgently needed to produce cost-competitive hydrogen energy. Several kinds of non-noble metal-based heterogeneous electrocatalysts, including carbides, sulfides, selenides, oxides, and phosphides, have been developed and studied. The unique physicochemical properties of carbonaceous materials make them promising candidates to support catalysts. In this paper, molybdenum disulfide (MoS2) nanomaterial catalysts have been synthesized, deposited on carbon fiber (CF)-based materials, and then used for solar hydrogen generation by membraneless electrochemical water splitting. At 430 W/m2 irradiation and 35 °C working temperature, the solar-to-hydrogen conversion efficiency is found to be 2.46%.
quote
| GB/T 7714-2015 | [1] Khushali Joshi, Khyati Mistry, Brijesh Tripathi, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01415. |
| MLA | [1] Khushali Joshi, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01415. |
| APA | [1] Khushali Joshi, Khyati Mistry, Brijesh Tripathi, Prakash Chandra, Satyam M. Shinde, Manoj Kumar, Dhaval Santola, Himanshu Chokshi, & Pavan Gurrala. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01415 |
| IEEE | [1] Khushali Joshi, Khyati Mistry, Brijesh Tripathi, Prakash Chandra, Satyam M. Shinde, Manoj Kumar, Dhaval Santola, Himanshu Chokshi, and Pavan Gurrala, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01415. keywords: {hydrogen evolution reaction (HER) CF−MoS2 membraneless electrolyzer hydrogen conversion efficiency stainless steel (SS)} |