Method for Reducting NonRE Impurities in Pure Tb AITranslate
Abstract AITranslate
NonRE impurities in pure Tb obtained by tradition process are high. Additional steps have been taken to reduce the impurities. Experiment results are satisfactory
KeyWords AITranslate
1金贵铸.稀土火法冶炼工艺学[M].北京:中国有色金属工业总公司教材编审办,1986.270.
2张长鑫.稀土火法冶炼冶金原理与工艺(上)[M].北京:北京科技大学,1991.2.
1张世荣.金属镝的制备、提纯及应用[J].稀有金属与硬质合金,2000,28(3):53-59. 被引量:12
1刘永林,李国云,李国栋.用熔盐萃取法制备低氧金属镝的研究[J].中国稀土学报,2002,20(z2):33-35. 被引量:2
2李国云,李国栋,刘永林.熔盐萃取法制备低氧、低氟金属镝的机制研究[J].中国稀土学报,2002,20(z2):263-265. 被引量:1
3王中磊,唐惠庆,郭占成,叶伟,蔡卓飞.直接电解法制取金属镝的阴极制备工艺研究[J].稀有金属,2010,34(5):755-763. 被引量:6
4云月厚,黄焦宏,刘文生,邰显康,李国栋.钙热还原及熔盐萃取联合法一次性制备低氧低氟金属镝[J].稀土,2006,27(3):91-93. 被引量:6
5刘宝忠.高纯金属镝的制备[J].稀有金属快报,2008,27(7):39-42. 被引量:7
6刘永林,云月厚.LiF-YF_3熔盐萃取提纯金属钇的研究[J].稀土,2010,31(1):92-94. 被引量:4
7金炳勋,谢宏伟,毛景,翟玉春.1-乙基-3-甲基-咪唑四氟硼酸盐离子液体中镝电沉积行为[J].稀有金属材料与工程,2012,41(5):881-884. 被引量:7
8郝占忠,王斌,张海玲.新型固定床气体氟化法制备低氧氟化钆[J].稀土,2013,34(5):16-21. 被引量:6
9李中华,朱伟长.氧化镝纳米粉体材料的制备[J].甘肃冶金,2013,35(6):56-57. 被引量:2
10刘木根,王薪鹏,吴英.金属镝生产工艺的改良[J].中国稀土学报,2014,32(3):354-362. 被引量:1
1田荣花,吴红.ICP-AES法测定金属铽中钽[J].江西冶金,2003,23(2):44-45. 被引量:3
2刘鹏宇.电感耦合等离子体质谱法测定金属钇中非稀土杂质的研究[J].现代科学仪器,2000,17(5):37-39. 被引量:3
3江祖成,陈建国,赖志远,廖振超,陈浩,廖振环.ICP光谱法直接测定高纯氧化钇中痕量非稀土杂质[J].稀土,1990,11(6):63-65. 被引量:2
4刘鹏宇.ICP-MS法测定金属镝中的非稀土杂质[J].分析试验室,2002,21(3):64-66. 被引量:2
5伊萨推出新款Weld M 308LSi不锈钢焊丝进一步完善焊丝产品线[J].电焊机,2015,45(5).
6洪广言.中科院“八五”重大项目——稀土新材料研究及其开发应用通过验收[J].稀土信息,1996,2(8):6-6.
7江西两项稀土行业标准通过预审[J].中国粉体工业,2015,0(5):30-30.
8江西两项稀土行业标准通过预审[J].稀土信息,2015,21(9):15-15.
9余丽萍,何为.ICP-AES法测定锌合金中的稀土杂质[J].江西冶金,1998,18(5):26-28. 被引量:1
10伍星,郑永章,刘湘生,李继东.高纯金属铕及其氧化物中14个稀土杂质的ICP-MS测定[J].现代仪器,2001,37(4):35-38. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]
Citation Information:
NonRE impurities in pure Tb obtained by tradition process are high. Additional steps have been taken to reduce the impurities. Experiment results are satisfactory
quote
| GB/T 7714-2015 | [1] WU Jian-she, CHEN Hai-quan, ZUO Jian-xin. Method for Reducting NonRE Impurities in Pure Tb[J]. Rare Metals and Cemented Carbides, 1999(2): 43-45. |
| MLA | [1] WU Jian-she, et al., "Method for Reducting NonRE Impurities in Pure Tb." Rare Metals and Cemented Carbides, no. 2, 1999, pp. 43-45. |
| APA | [1] WU Jian-she, CHEN Hai-quan, & ZUO Jian-xin. (1999). Method for Reducting NonRE Impurities in Pure Tb. Rare Metals and Cemented Carbides(2), 43-45. |
| IEEE | [1] WU Jian-she, CHEN Hai-quan, and ZUO Jian-xin, "Method for Reducting NonRE Impurities in Pure Tb," Rare Metals and Cemented Carbides, no. 2, pp. 43-45, 1999. keywords: {RE;metal Tb;nonRE impurity} |