Fundamentals and Applications of Polymer Brushes in Air AITranslate
Abstract AITranslate
For several decades, high-density, end-tethered polymers, forming so-called polymer brushes, have inspired scientists to understand their properties and to translate them to applications. While earlier research focused on polymer brushes in liquids, it was recently recognized that these brushes can find application in air as well. In this review, we report on recent progress in unraveling fundamental concepts of brushes in air, such as their vapor-swelling and solvent partitioning. Moreover, we provide an overview of the plethora of applications in air (e.g., in sensing, separations or smart adhesives) where brushes can be key components. To conclude, we provide an outlook by identifying open questions and issues that, when solved, will pave the way for the large scale application of brushes in air.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01615
Chinese Library Classification Number:
Citation Information:
For several decades, high-density, end-tethered polymers, forming so-called polymer brushes, have inspired scientists to understand their properties and to translate them to applications. While earlier research focused on polymer brushes in liquids, it was recently recognized that these brushes can find application in air as well. In this review, we report on recent progress in unraveling fundamental concepts of brushes in air, such as their vapor-swelling and solvent partitioning. Moreover, we provide an overview of the plethora of applications in air (e.g., in sensing, separations or smart adhesives) where brushes can be key components. To conclude, we provide an outlook by identifying open questions and issues that, when solved, will pave the way for the large scale application of brushes in air.
quote
| GB/T 7714-2015 | [1] Guido C. Ritsema van Eck, Leonardo Chiappisi, Sissi de Beer. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01615. |
| MLA | [1] Guido C. Ritsema van Eck, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01615. |
| APA | [1] Guido C. Ritsema van Eck, Leonardo Chiappisi, & Sissi de Beer. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01615 |
| IEEE | [1] Guido C. Ritsema van Eck, Leonardo Chiappisi, and Sissi de Beer, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01615. keywords: {polymer brush;vapor;sensing;separations;wetting;adhesion;surfaces} |