Abstract AITranslate

Brief introduction is made to the domestic vacuum sintering integral furnace.The furnace functions and related testing data showed that the furnace is close to or has come up to the international advanced standard.

KeyWords AITranslate

vacuum-sintering integral furnace structure property

1凌云,刘颖慧,王兵.基于S7-200的真空烧结炉模糊控制系统设计[J].电气自动化,2007,29(5):21-23. 被引量:1

2杨伟,胡元安,张杞芳,田峰.真空脱蜡-烧结一体炉的改造设计与实践[J].粉末冶金工业,2012,22(3):44-50. 被引量:2

1叶景明,王建华,金鑫.烧结炉温度控制中专家协调系统的设计[J].东南大学学报:自然科学版,2010,40(S1):312-315. 被引量:1

2周媛,周李蕾.高密度钨合金可控微气氛真空烧结工艺研究[J].四川有色金属,2018(1):41-45. 被引量:2

3郄程飞,刘双林,魏智才.立式脱蜡预烧结炉的研发与应用[J].电器工业,2019,0(11):76-78. 被引量:1

1薛朝云.国外高炉喷吹废塑料简况[J].炼铁,1997,16(2):57-58. 被引量:26

2邵维裘,叶枫.上钢五厂转炉厂引进意大利特钢小方坯连铸机调试简况[J].上海冶金情报,1989(4):7-12.

3陈伟庆.德国氧气转炉钢的冶炼技术[J].钢铁,1996,31(8):79-84. 被引量:2

4姜文革.武钢2号高炉大修改造简况[J].炼铁,1999,18(6):44-45.

5宰文新,赵继宇,何金平.武钢第一炼钢厂方坯高效连铸机装备及投产简况[J].炼钢,2000,16(1):60-62. 被引量:1

6王维兴.日本高炉工艺节能简况[J].炼铁,1997,16(5):52-53.

7黄海民.工业硅电炉使用自焙炭砖简况[J].铁合金,1989(4):29-30.5.

8李凤喜,李具中,萧忠敏,曹维,王雪冬,陈清泉,张文辉.武钢二炼钢KR铁水脱硫生产实践[J].炼钢,2005,21(5):1-4. 被引量:24

9严维源,陈德富,袁济国.特殊钢小方坯连铸机工艺设备特点和热调试简况[J].炼钢,1990,6(4):27-31.

102010年1~3月韩国进口铝锭简况[J].建材发展导向,2010,8(3):72-72.

Basic Information:

DOI:

Chinese Library Classification Number:TF806.1[冶金工程—有色金属冶金]

Citation Information:

Brief introduction is made to the domestic vacuum sintering integral furnace.The furnace functions and related testing data showed that the furnace is close to or has come up to the international advanced standard.

quote

GB/T 7714-2015 [1] LI Zhong-ding. Brief Introduction to Domestic Vacuum Sintering Integral Furnace[J]. Rare Metals and Cemented Carbides, 2003(1): 39-42.
MLA [1] LI Zhong-ding. "Brief Introduction to Domestic Vacuum Sintering Integral Furnace." Rare Metals and Cemented Carbides, no. 1, 2003, pp. 39-42.
APA [1] LI Zhong-ding. (2003). Brief Introduction to Domestic Vacuum Sintering Integral Furnace. Rare Metals and Cemented Carbides(1), 39-42.
IEEE [1] LI Zhong-ding, "Brief Introduction to Domestic Vacuum Sintering Integral Furnace," Rare Metals and Cemented Carbides, no. 1, pp. 39-42, 2003. keywords: {vacuum-sintering integral furnace;structure;property}