Preparation and Properties of Ce0.8Gd0.2O2-δ AITranslate
Abstract AITranslate
Ce0.8Gd0.2O2-δ electrolyte for solid oxide fuel cellI (IT-SOFC)δ was prepared by co-precipitation method. Its properties are tested. The XRD measurement shows that the powder from precursor calcination is of mono-cubic fluorite-type structure. SEM testing shows that the calcination temperature has important influence on powder morphology and density of the sintered body,relative density of which reached 96.4% upon sintering at 1 350 ℃. And the results of impedance spectroscopy showed that ionic conduction of the said electrolyte reached 0. 003 S/cm at 700℃.
KeyWords AITranslate
1罗绍华,唐子龙,尧巍华,张中太,李杰,闫俊萍.低温燃烧合成钛酸钡及其陶瓷介电性能研究[J].硅酸盐学报,2003,31(6):560-565. 被引量:41
2李艳华,于战华,冷静,刘晓梅.溶胶-凝胶法制备两种中温SOFC电解质材料[J].中国稀土学报,2005,23(S2):182-184. 被引量:6
3刘晓梅,苏文辉,梁路光,郭天才,冷静.稀土电解质Ce_(0.9)M_(0.1)O_(2-δ)(M=Pr,Nd,Sm,Gd,Dy)的制备与性能[J].中国稀土学报,2003,21(4):476-477. 被引量:4
4蒋凯,彭程,李五聚,王琳,王鸿燕,梁宏伟,孟健.Ce_(1-x)Gd_xO_(2-x/2)的溶胶-凝胶法合成及其性质[J].高等学校化学学报,2001,22(8):1279-1282. 被引量:24
5尹艳红,杨书廷,夏长荣,孟广耀.不同方法制备的Ce_(0.8)Sm_(0.2)O_(1.9)(SDC)性能对比[J].河南师范大学学报:自然科学版,2005,33(2):56-59. 被引量:5
1刘润泽,周芬,王青春,郜建全,包金小,宋希文.固体氧化物燃料电池用CeO_(2)基电解质的研究进展[J].材料导报,2021,35(S01):29-32. 被引量:5
1姜晓峰,周芬,张永和,郜建全,宋希文.Sm、Nd、Ca多掺杂铈基固体电解质的制备及性能研究[J].电子元件与材料,2022,41(6):587-594.
2赵建军,甄文龙,吕功煊.固体氧化物电解CO_(2)技术现状与前景[J].燃料化学学报,2022,50(10):1237-1258. 被引量:1
3杨琛宇,周芬,包金小,郜建全,宋希文.Ce_(0.8)Gd_(0.15-x)Nd_(x)Ca_(0.05)O_(2-δ)电解质的制备及性能研究[J].陶瓷学报,2022,43(5):908-916.
4吕超,殷宏鑫,刘艳龙,陈绪鑫,孙铭赫.微波热解法制备氧化铈过程的可视化研究[J].工程科学学报,2023,45(7):1238-1245.
5朱志刚,宋琛,胡永俊,邓畅光,刘太楷,文魁,董东东,毛杰,刘敏.粉末粒径对等离子喷涂固体氧化物燃料电池阳极微观结构及性能的影响[J].材料研究与应用,2023,17(2):329-337.
1刘晓梅,苏文辉,梁路光,郭天才,冷静.稀土电解质Ce_(0.9)M_(0.1)O_(2-δ)(M=Pr,Nd,Sm,Gd,Dy)的制备与性能[J].中国稀土学报,2003,21(4):476-477. 被引量:4
2李艳华,于战华,刘晓梅.甘氨酸-硝酸盐法制备中温SOFC电解质材料[J].稀土,2008,29(1):13-15. 被引量:1
3王峰.锰(Ⅱ)配位聚合物的水热合成和晶体结构[J].河南教育学院学报:自然科学版,2009,18(1):25-27.
4郝红霞,刘瑞泉.天然气中温SOFC阳极材料铒掺杂的氧化铈的制备与性能研究[J].无机化学学报,2009,25(10):1842-1847. 被引量:2
5王亚楠,周和平.Gd_(1-x)Sr_xCoO_(3-δ)和Gd_(0.8)Sr_(0.2)Co_(1-y)Fe_yO_(3-δ)系阴极材料的制备和性能[J].无机化学学报,2008,24(10):1558-1563. 被引量:1
6刘毅.YBaCo_2O_(5+δ)阴极材料的微观结构和热膨胀及电性能(英文)[J].硅酸盐学报,2009,37(3):373-377. 被引量:1
7李双保,盛建军,林峰,张小林.钙钛矿型复合氧化物La_(0.8)Sr_(0.2)Mn_(1-y)Co_yO_(3-δ)的合成与性能研究[J].深圳职业技术学院学报,2009,8(1):66-70. 被引量:2
8陈国荣,史鹏飞,白永平,范太炳.新型复合聚合物电解质离子导电行为的研究[J].化学学报,2004,62(4):377-380. 被引量:1
9Longfei Luo,Hongwei Cheng,Guangshi Li,Xionggang Lu,Bo Jiang.Oxygen permeability and CO_2-tolerance of Ce_(0.8)Gd_(0.2)O_(2-δ)-Ln BaCo_2O_(5+δ) dual-phase membranes[J].能源化学:英文版,2015,24(1):15-22. 被引量:3
10谢光远,郭密,谢育涛,李平生.复合掺杂固体电解质氧离子导电性的回归模型[J].华中科技大学学报:自然科学版,2006,34(9):66-68.
Basic Information:
DOI:
Chinese Library Classification Number:O614.33[理学—无机化学]
Citation Information:
Ce0.8Gd0.2O2-δ electrolyte for solid oxide fuel cellI (IT-SOFC)δ was prepared by co-precipitation method. Its properties are tested. The XRD measurement shows that the powder from precursor calcination is of mono-cubic fluorite-type structure. SEM testing shows that the calcination temperature has important influence on powder morphology and density of the sintered body,relative density of which reached 96.4% upon sintering at 1 350 ℃. And the results of impedance spectroscopy showed that ionic conduction of the said electrolyte reached 0. 003 S/cm at 700℃.
quote
| GB/T 7714-2015 | [1] SHI Qian, ZHENG Feng, CHEN Yu. Preparation and Properties of Ce0.8Gd0.2O2-δ[J]. Rare Metals and Cemented Carbides, 2007(3): 1-4. |
| MLA | [1] SHI Qian, et al., "Preparation and Properties of Ce0.8Gd0.2O2-δ." Rare Metals and Cemented Carbides, no. 3, 2007, pp. 1-4. |
| APA | [1] SHI Qian, ZHENG Feng, & CHEN Yu. (2007). Preparation and Properties of Ce0.8Gd0.2O2-δ. Rare Metals and Cemented Carbides(3), 1-4. |
| IEEE | [1] SHI Qian, ZHENG Feng, and CHEN Yu, "Preparation and Properties of Ce0.8Gd0.2O2-δ," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2007. keywords: {co-precipitation method;SOFC;RE electrolyte;high-temperature conductivity} |