Effects of Powder Mixing Processes on Mechanical Properties of Ultrafine Cemented Carbides AITranslate

School of Mechanical Engineering,Nanjing University of Science&Technology;School of Mechanical Engineering,Nanjing University of Science&Technology;School of Mechanical Engineering,Nanjing University of Science&Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of three original powder mixing methods including mechanical ball milling,dispersant dispersion and ultrasonic vibration on the mechanical properties of sintered WC-based cemented carbide samples were systematically studied.The results show that the density of the cemented carbide prepared by PEG dispersion is the lowest,while the density of the cemented carbide prepared by ultrasonic vibration is the highest and its mechanical properties are the best:relative density of 97.8%,Vickers hardness of 21.47 GPa,fracture toughness of 11.2 MPa·m1/2,bending strength of 1123.6 MPa and grain size of 258 nm.

KeyWords AITranslate

cemented carbide WC-Co ultrafine grain powder mixing process mechanical property soft agglomeration spark plasma sintering

1苗赫濯.新型陶瓷刀具的发展与应用[J].中国有色金属学报,2004,14(F01):237-242. 被引量:20

2徐德良,方层层,詹迎旭,王翰瑶,梁志瑜,吴啸,林枞.微波两步法烧结氧化铝陶瓷及对韧性的影响[J].陶瓷学报,2018,39(2):174-180. 被引量:1

3刘雪梅,王海滨,宋晓艳,王西龙,李玉玺.VC添加量对纳米晶硬质合金的制备及性能影响[J].稀有金属材料与工程,2016,45(2):477-481. 被引量:10

4吴冲浒,聂洪波,肖满斗.中国超细晶硬质合金及原料制备技术进展[J].中国材料进展,2012,31(4):39-46. 被引量:34

5崔洪梅,刘宏,王继扬,李霞,韩峰.纳米粉体的团聚与分散[J].机械工程材料,2004,28(8):38-41. 被引量:71

6季必发,田长安,谢劲松.国内放电等离子烧结技术的研究进展及展望[J].广东化工,2013,40(15):85-86. 被引量:5

7王栋,田辉,李建伟.超声震荡及化学试剂对碳纳米管分散性能的影响[J].科技情报开发与经济,2009,19(29):141-142. 被引量:10

1李云龙.氧化预处理对超细晶硬质合金材料性能的影响[J].稀有金属与硬质合金,2022,50(6):83-89.

1王晓芳,李硕.控制小麦粉粉色与麸星的技术探讨[J].现代面粉工业,2020,34(3):3-6. 被引量:3

2王书涛,牛磊.Nano-Sb2O3对PBT基复合材料力学性能的影响[J].中国材料进展,2020,39(5):391-394. 被引量:2

3王鹏,时凯华,顾金宝,曾伟,韩亚刚,董凯林.不同粘结相碳化钨基硬质合金的研究与应用(Ⅱ)[J].硬质合金,2020,37(2):152-169. 被引量:3

4陈军强,孙青竹,万桂林,吕雯,杨芮.添加剂对Ti(C,N)基金属陶瓷的力学性能影响[J].科技资讯,2020,18(4):54-54.

5彭雪伟,张淇,谢志勇.碳纳米管/聚乙烯醇/羰基铁粉复合材料的制备及吸波性能研究[J].炭素技术,2020(2):39-43. 被引量:5

6王立华.锻造“工业牙齿”的硬属性[J].中国科技奖励,2020,0(1):49-50.

7刘文彬,陈飞雄,裴新军,熊宁,王铁军.大尺寸亚微米硬质合金顶锤的热等静压研制[J].稀有金属与硬质合金,2020,48(2):82-89. 被引量:1

8李萌,弓满锋,张程煜,莫德云,李玫,韩栋,张洪军.超细、纳米晶WC-Co硬质合金烧结技术的研究现状[J].材料导报,2020,34(15):15138-15144. 被引量:8

9李世嘉,庞尔楠,郝彩红,蔡婷婷,胡胜亮.固态荧光碳点的制备[J].化学进展,2020,32(5):548-561. 被引量:2

10李之旭,范洪远,鲜广,赵海波,熊计.硬质合金基体对TiAlN/TiAlSiCrN/TiSiN多层涂层结构和机械性能的影响[J].硬质合金,2020,37(2):119-126. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

The effects of three original powder mixing methods including mechanical ball milling,dispersant dispersion and ultrasonic vibration on the mechanical properties of sintered WC-based cemented carbide samples were systematically studied.The results show that the density of the cemented carbide prepared by PEG dispersion is the lowest,while the density of the cemented carbide prepared by ultrasonic vibration is the highest and its mechanical properties are the best:relative density of 97.8%,Vickers hardness of 21.47 GPa,fracture toughness of 11.2 MPa·m1/2,bending strength of 1123.6 MPa and grain size of 258 nm.

quote

GB/T 7714-2015 [1] JIA Ji-heng, LIU Kui, WANG Zhen-hua. Effects of Powder Mixing Processes on Mechanical Properties of Ultrafine Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2020(3): 87-91.
MLA [1] JIA Ji-heng, et al., "Effects of Powder Mixing Processes on Mechanical Properties of Ultrafine Cemented Carbides." Rare Metals and Cemented Carbides, no. 3, 2020, pp. 87-91.
APA [1] JIA Ji-heng, LIU Kui, & WANG Zhen-hua. (2020). Effects of Powder Mixing Processes on Mechanical Properties of Ultrafine Cemented Carbides. Rare Metals and Cemented Carbides(3), 87-91.
IEEE [1] JIA Ji-heng, LIU Kui, and WANG Zhen-hua, "Effects of Powder Mixing Processes on Mechanical Properties of Ultrafine Cemented Carbides," Rare Metals and Cemented Carbides, no. 3, pp. 87-91, 2020. keywords: {cemented carbide;WC-Co;ultrafine grain;powder mixing process;mechanical property;soft agglomeration;spark plasma sintering}