Effect of Calcination Temperature on the Electrocatalytic Properties of La0.6Sr0.4CoO_3 AITranslate
Abstract AITranslate
La0.6Sr0.4CoO3 perovskite-type oxide was prepared with sol-gel method, and the effect of calcina- tion temperature on its electrocatalytic properities in bifunctional oxygen electrodes was particularly stud- ied. The phase and morphology of La0.6Sr0.4CoO3 perovskite-type oxide were analyzed by XRD, SEM and BET,and the steady-state polarization curves and steady-state galvanostatic curves of the cathode and an- ode of the bifunctional oxygen electrodes were plotted in a three-electrode system. The results show that increasing the calcination temperature is advantageous for decreasing the impurities in La0.6Sr0.4CoO3 per- ovskite-type oxide. When the calcination temperature reaches 800 ℃, pure La0.6Sr0.4CoO3 perovskite-type oxide is obtained with the highest catalytic activity,and the bifunctional oxygen electrode owns the lowest electrochemical polarization and the highest stability.
KeyWords AITranslate
1王瀛,张丽敏,胡天军.金属空气电池阴极氧还原催化剂研究进展[J].化学学报,2015,73(4):316-325. 被引量:23
2庄树新,吕建先,路密,刘翼民,陈晓彬.钙钛矿型氧化物的制备及其在固体氧化物燃料电池和金属-空气电池中的应用[J].化学进展,2015,27(4):436-447. 被引量:7
3朱志杰,唐有根,宋永江,罗继.pH值对钙钛矿催化剂结构和性能的影响[J].电源技术,2008,32(4):218-221. 被引量:4
1郎凤培,汪浩,张生俊,刘晶冰,严辉.基于智能变色的发射率可调型薄膜研究进展[J].材料导报,2017,31(A01):251-256. 被引量:1
2韩国成功开发第二代钙钛矿型光伏电池[J].电力建设,2018,39(6).
3史鹤鸣.市政公用工程道路路基施工技术探讨[J].工程建设与设计,2018(11):252-253. 被引量:3
4张程誉.基于计算机软件工程的数据库编程技术[J].自动化与仪器仪表,2018,0(6):186-188. 被引量:15
5韩国成功开发第二代钙钛矿型光伏电池[J].山东陶瓷,2018,41(2):7-7.
6宋珍霞,殷齐贺,穆晓斐.膨润土负载纳米零价铁去除废水中Cr(Ⅵ)的动力学特性研究[J].化工新型材料,2018,46(5):199-203. 被引量:7
7李云峰,罗传军.湿法包覆LiNi_(0.6)Co_(0.2)Mn_(0.2)O_2合成、结构与性能的研究[J].河南化工,2018,35(4):26-31.
8谭玉琪,刘立宁,关冰冰,王珅,于杰,韩松.石墨烯/TiO_2复合材料的制备及其在超级电容器中的应用[J].化学与粘合,2018,40(3):185-188. 被引量:2
9张建华,马红星,蒋玉思,程华月,刘斌.一种复合氧化物涂层钛电极的电化学性能及其在废水处理中的应用[J].化学与生物工程,2018,35(4):53-57.
10徐效梅,朱松然.Ce(Ⅲ)/Ce(Ⅳ)-H_2SO_4体系的反应动力学[J].河南大学学报:自然科学版,1985,0(4):67-77.
Basic Information:
DOI:
Chinese Library Classification Number:TM911[电气工程—电力电子与电力传动]
Citation Information:
La0.6Sr0.4CoO3 perovskite-type oxide was prepared with sol-gel method, and the effect of calcina- tion temperature on its electrocatalytic properities in bifunctional oxygen electrodes was particularly stud- ied. The phase and morphology of La0.6Sr0.4CoO3 perovskite-type oxide were analyzed by XRD, SEM and BET,and the steady-state polarization curves and steady-state galvanostatic curves of the cathode and an- ode of the bifunctional oxygen electrodes were plotted in a three-electrode system. The results show that increasing the calcination temperature is advantageous for decreasing the impurities in La0.6Sr0.4CoO3 per- ovskite-type oxide. When the calcination temperature reaches 800 ℃, pure La0.6Sr0.4CoO3 perovskite-type oxide is obtained with the highest catalytic activity,and the bifunctional oxygen electrode owns the lowest electrochemical polarization and the highest stability.
quote
| GB/T 7714-2015 | [1] YU Wen-wan, HUANG Hong-xia, WANG Cheng. Effect of Calcination Temperature on the Electrocatalytic Properties of La0.6Sr0.4CoO_3[J]. Rare Metals and Cemented Carbides, 2018(3): 23-28. |
| MLA | [1] YU Wen-wan, et al., "Effect of Calcination Temperature on the Electrocatalytic Properties of La0.6Sr0.4CoO_3." Rare Metals and Cemented Carbides, no. 3, 2018, pp. 23-28. |
| APA | [1] YU Wen-wan, HUANG Hong-xia, & WANG Cheng. (2018). Effect of Calcination Temperature on the Electrocatalytic Properties of La0.6Sr0.4CoO_3. Rare Metals and Cemented Carbides(3), 23-28. |
| IEEE | [1] YU Wen-wan, HUANG Hong-xia, and WANG Cheng, "Effect of Calcination Temperature on the Electrocatalytic Properties of La0.6Sr0.4CoO_3," Rare Metals and Cemented Carbides, no. 3, pp. 23-28, 2018. keywords: {perovskite- type oxide;La0.6Sr0.4CoO3;bifunctional oxygen electrode;calcination temperature;electrocatalytic property;stability} |