Influence of Oxygen Content on the Formation of Anode Oxide Film and Leakage Current of Ta Electrolytic Capacitor AITranslate
Abstract AITranslate
In view of the importance of anode oxide film in Ta electrolytic capacitor,comparative analysis is made of the influence of oxygen content in Ta anode sheet. Related influence mechanism is described. Resuits show that the oxygen content is dependant on the impurity oxygen content of the in Ta powder and is related to the anode sheet compaction, sintering and property. Impurity oxygen is unfavorable for the formation of anode oxide film and is one of the main factors for higher leakage current of the capacitor.
KeyWords AITranslate
1欧阳一凤,李荐,姜翠玲,钟海云,刘建清,王德全.钽、铌电解电容器工艺研究进展[J].稀有金属与硬质合金,2003,31(4):32-35. 被引量:3
2郭书霞.固体钽电解电容器对产品性能的影响及其形成[J].焦作师范高等专科学校学报,1995,0(1):55-58. 被引量:2
3揣荣岩,孟丽囡,韦春才.钽阳极氧化膜的防晶化研究[J].沈阳工业大学学报,2004,26(4):433-434. 被引量:7
1刘勇刚,易金锋.成形烧结过程对固体电解质钽电容器电性能的影响[J].稀有金属与硬质合金,2008,36(4):17-19. 被引量:6
2李仲香,郑金风,张健康,包玺芳.影响电容器钽阳极漏电流因素分析[J].宁夏工程技术,2010,9(2):108-110. 被引量:7
3刘莲云,马春红,黄凯,朱鸿民.热处理时间和压制密度对氮化钽粉电性能的影响[J].有色金属:冶炼部分,2012(10):34-37. 被引量:6
4高路.掺氮及氮化钽粉的研究进展[J].广州化工,2013,41(3):15-17. 被引量:1
5李军义,孙本双,王东新,任晓,何季麟.氧含量对FFC法制备钽粉形貌和电容的影响[J].稀有金属材料与工程,2013,42(4):849-852. 被引量:3
6帅柱军,余琨,何坤池.电容器钽粉镁处理降氧工艺探究[J].硬质合金,2013,30(2):86-90. 被引量:2
7石维,杨邦朝,张选红,方鸣,马建华,李玮,王兴伟.电化学Ta_2O_5薄膜漏电流机理的研究进展[J].化工进展,2013,32(4):832-836.
8高路,刘莲云,黄凯,朱鸿民.纳米氮化钽粉末的后处理[J].有色金属工程,2013,3(6):27-29.
9张学清,郭顺,杨国启,谢群力,左婧懿,罗文.煅烧工艺对钽粉微观结构和电性能的影响[J].稀有金属,2018,42(1):67-74. 被引量:3
10王晓明,雒国清,杨国启,赵春霞.包装对钽粉碳含量影响的研究[J].湖南有色金属,2018,34(2):48-50. 被引量:1
1高路.掺氮及氮化钽粉的研究进展[J].广州化工,2013,41(3):15-17. 被引量:1
2李军义,孙本双,王东新,任晓,何季麟.氧含量对FFC法制备钽粉形貌和电容的影响[J].稀有金属材料与工程,2013,42(4):849-852. 被引量:3
3鄢波,阳元江,肖毅,王安玖,杨槐香,王刚.中压大容量新型高能非固体电解质钽电容器研制[J].材料导报:纳米与新材料专辑,2014,28(1):180-182. 被引量:1
4张卜升,许万祥,陈姝晖,马光.含钽合金渣中钽的回收[J].有色金属:冶炼部分,2014(9):47-50. 被引量:2
5张学清,郭顺,杨国启,谢群力,左婧懿,罗文.煅烧工艺对钽粉微观结构和电性能的影响[J].稀有金属,2018,42(1):67-74. 被引量:3
6赵春霞,赵勇刚,王晓明,王小明,颜景熠.金属杂质含量对钽粉电性能影响的研究[J].湖南有色金属,2019,35(1):48-50. 被引量:3
7许宁辉,刘军,魏春霞.阳极氧化形成工艺对一氧化铌电性能的影响[J].粉末冶金工业,2019,29(3):23-26. 被引量:3
8李福成,张学清,柳金洲,包富贵.FTW150K高比容钽粉研制钽电容器电介质膜形成工艺的研究[J].宁夏大学学报:自然科学版,2020,41(2):164-167.
9刘建清,袁艳丰,徐震宇.一种高压大容量非固体电解质钽电容器的研究[J].电子元件与材料,2020,39(8):96-100. 被引量:2
10李丽君,雒国清,刘建伟,纪保军.降低钠还原钽粉中铁、镍质量分数的工艺探讨[J].宁夏工程技术,2020,19(3):223-225. 被引量:1
1归振兴,沈华勤,沈晖.宽条阳极的管板式放电电极[J].科技开发动态,2005(1):43-43.
2甘权,周淑娟.核电站海水相关系统防腐措施探讨[J].科技信息,2014,0(4):49-49. 被引量:6
3刘勇刚,易金锋.成形烧结过程对固体电解质钽电容器电性能的影响[J].稀有金属与硬质合金,2008,36(4):17-19. 被引量:6
4陈德显,王述昌.微波炉(九)——电源的设计考虑(下)[J].家用电器科技,1989(1):39-40.
5那日苏.PLC在桥式托盘翻转机控制系统中的应用[J].青海经济研究,2008(5):83-84.
6蒋春强,陆胜,吕林兴.高频、低ESR钽电解电容器新工艺的开发[J].材料导报,2008,22(4):135-137.
7李福成.聚合物银浆在钽电解电容器阴极上的应用研究[J].陕西理工学院学报:自然科学版,2013,29(1):42-46. 被引量:3
8马强.三工位片式钽电容器真空预烧炉的研制[J].真空,2001,38(5):33-36. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TM535.1[电气工程—电器]
Citation Information:
In view of the importance of anode oxide film in Ta electrolytic capacitor,comparative analysis is made of the influence of oxygen content in Ta anode sheet. Related influence mechanism is described. Resuits show that the oxygen content is dependant on the impurity oxygen content of the in Ta powder and is related to the anode sheet compaction, sintering and property. Impurity oxygen is unfavorable for the formation of anode oxide film and is one of the main factors for higher leakage current of the capacitor.
quote
| GB/T 7714-2015 | [1] WU Zun-zhong, YAO Wei-dong, YUAN Kun-yang. Influence of Oxygen Content on the Formation of Anode Oxide Film and Leakage Current of Ta Electrolytic Capacitor[J]. Rare Metals and Cemented Carbides, 2006(2): 32-34. |
| MLA | [1] WU Zun-zhong, et al., "Influence of Oxygen Content on the Formation of Anode Oxide Film and Leakage Current of Ta Electrolytic Capacitor." Rare Metals and Cemented Carbides, no. 2, 2006, pp. 32-34. |
| APA | [1] WU Zun-zhong, YAO Wei-dong, & YUAN Kun-yang. (2006). Influence of Oxygen Content on the Formation of Anode Oxide Film and Leakage Current of Ta Electrolytic Capacitor. Rare Metals and Cemented Carbides(2), 32-34. |
| IEEE | [1] WU Zun-zhong, YAO Wei-dong, and YUAN Kun-yang, "Influence of Oxygen Content on the Formation of Anode Oxide Film and Leakage Current of Ta Electrolytic Capacitor," Rare Metals and Cemented Carbides, no. 2, pp. 32-34, 2006. keywords: {oxygen content;Ta electrolytic capacitor;anode oxide film;leakage current} |