Development and Application of Forging Technology in Processing of the New Materials AITranslate
Abstract AITranslate
Brief analysis is made of tendency for the development of the forging equipment and its control system. The paper describes the powder forging, precision forging, isothermal forging techniques and their applications in the processing of steel-bonded cemented carbide,Nb-Ti high-temperature alloy steel,etc.
KeyWords AITranslate
1张宝玮.中国锻压技术及装备的现状与发展[J].机械工人:热加工,2003(4):41-43. 被引量:1
2张会,张昌明.浅议锻压加工技术的发展[J].包钢科技,2004,30(5):14-15. 被引量:1
3林永新.锻造设备制造技术的发展[J].稀有金属快报,2004,23(12):7-9. 被引量:9
4王荣滨,海波.钢结硬质合金锻压形变工艺研究[J].硬质合金,1997,14(2):87-91. 被引量:6
1姚汝君.锻压设备构件生产中的工艺优化措施[J].能源与节能,2017(5):130-131.
2胡景蓉,陈保家,严文超.锻压温度对钢制机械扣件性能的影响[J].热加工工艺,2018,47(3):170-173.
3董海涛,张治民,杨占尧.锻造工艺对铝合金轴承盖性能的影响[J].热加工工艺,2018,47(19):151-154. 被引量:1
4梅耀云.关于材料成型技术的现状与发展趋势的研究[J].商业故事,2015,0(27):96-97. 被引量:3
1胡景蓉,陈保家,严文超.锻压温度对钢制机械扣件性能的影响[J].热加工工艺,2018,47(3):170-173.
2马红超.简析新型金属材料成型加工技术[J].山东工业技术,2016(21):45-45. 被引量:7
3张会斌.新型材料成型加工技术分析[J].科学与信息化,2018,0(3):103-103.
4魏冠义,杨峰,齐晓华.基于QForm的6082铝合金吊耳锻造工艺优化[J].热加工工艺,2019,48(17):113-116. 被引量:2
1李连方.在摩擦压力机上精密锻压[J].锻压机械,1992,27(4):15-16.
2汪诚.高温精密锻压模的设计[J].湘潭大学自然科学学报,1990,12(3):77-82.
3陶建明,宋爱平,易旦萍,杨益,田德云.基于SuperForge的直齿锥齿轮精密锻压模具设计[J].机械工程与自动化,2013(1):122-124. 被引量:2
4大连高合金棒线材公司成功轧制8825高温合金钢[J].不锈:市场与信息,2015,0(8):6-6.
5E.W.Kelloy,吴鼎.高温合金钢与工具钢的轧制[J].一重技术,1994(4):112-115.
6王守伟,尉少荣.某筒座30CrMnSi合金结构钢毛坯锻压工艺[J].精密成形工程,2012,4(5):48-50. 被引量:1
7廖国防,易幼平,王少辉.航空接头锻件等温锻压成形工艺[J].材料科学与工艺,2012,20(1):6-10. 被引量:11
8重庆五九精密锻压有限责任公司[J].精密成形工程,2010(1).
9重庆五九精密锻压有限责任公司[J].精密成形工程,2009,0(3).
10重庆五九精密锻压有限责任公司[J].精密成形工程,2010,0(4).
Basic Information:
DOI:
Chinese Library Classification Number:TG306[金属学及工艺—金属压力加工]
Citation Information:
Brief analysis is made of tendency for the development of the forging equipment and its control system. The paper describes the powder forging, precision forging, isothermal forging techniques and their applications in the processing of steel-bonded cemented carbide,Nb-Ti high-temperature alloy steel,etc.
quote
| GB/T 7714-2015 | [1] YU Xiao-jun. Development and Application of Forging Technology in Processing of the New Materials[J]. Rare Metals and Cemented Carbides, 2007(1): 57-60. |
| MLA | [1] YU Xiao-jun. "Development and Application of Forging Technology in Processing of the New Materials." Rare Metals and Cemented Carbides, no. 1, 2007, pp. 57-60. |
| APA | [1] YU Xiao-jun. (2007). Development and Application of Forging Technology in Processing of the New Materials. Rare Metals and Cemented Carbides(1), 57-60. |
| IEEE | [1] YU Xiao-jun, "Development and Application of Forging Technology in Processing of the New Materials," Rare Metals and Cemented Carbides, no. 1, pp. 57-60, 2007. keywords: {forging technique;equipment and control;powder forging;precision forging;isothermal forging material processing} |