Effects of Concentration of the Alloying Element Co on the Mechanical Properties of NiAl AITranslate

Department of Mechanical and Electrical Engineering, Shaoyang Vocational and Technical College;National Key Laboratory of Advanced Design and Manufacturing of Hunan University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Calculation and analysis were made of the effects of Co concentration on the mechanical properties of NiAl alloy based on virtual crystal approximation and using the first-principles pseudopotential plane- wave method. The results from elastic modulus calculation and analysis show that after B2-NiAl crystal is alloyed with Co, its hardness is increased except x (Co) = 2%, and obviously increased in the low concentration range of x(Co)=0-0.5 %, and the increase degree is lower in the high concentration range of x(Co)=3-25%. At the same time, the ductility of B2-NiAl crystal is decreased at first and then increased,decreased only a little at x(Co) =0-0.5% and obviously at x(Co)=0.5%-4 % ,and increased gradually at x(Co) =4%-25%.

KeyWords AITranslate

B2-NiAl Co alloying Co concentration mechanical property elastic modulus first-principles cal- culation

1姚强,邢辉,孟丽君,孙坚.Ti—Mo合金β结构稳定性和弹性性质的第一性原理研究[J].金属学报,2008,44(1):19-22. 被引量:13

2李博,夏冬生,王铁利,郭建亭,李谷松.Co含量对Ni-Al机械合金化的影响[J].东北大学学报:自然科学版,1999,20(2):213-216. 被引量:4

3尚家香,喻显扬.3d过渡金属在NiAl中的占位及对键合性质的影响[J].物理学报,2008,57(4):2380-2385. 被引量:16

4郭建亭,任维丽,周健.NiAl合金化研究进展[J].金属学报,2002,38(6):667-672. 被引量:26

5陈律,文韬.B_2-NiAl弹性性质Ag合金化效应的理论研究[J].航空材料学报,2011,31(2):1-7. 被引量:8

1刘友成,周兵,刘绍忠.NiF2掺杂对MgH2解氢性能影响机制研究[J].稀有金属,2018,42(11):1193-1198. 被引量:2

1石伟和,贾陈忠,陆必旺,马志鸿.催化剂掺杂对MgH2储氢性能的改进研究[J].稀有金属,2022,46(1):87-95. 被引量:3

2王亚雄,钟顺彬,孙逢春.车载高质量密度固态储氢材料研究进展[J].稀有金属,2022,46(6):796-812. 被引量:2

1刘友成,周惦武,高丽洁,彭平.P合金化浓度对NiAl力学性能影响的第一原理计算[J].稀有金属材料与工程,2013,42(S2):578-581. 被引量:2

2徐向棋,陈子潘,王泾文,张少伍,罗来辉,王松林.800℃长期氧化过程中含铝奥氏体耐热钢中第二相的演化规律[J].机械工程材料,2016,40(12):6-8.

3桑革,李全安,陈云贵,闫康平,涂铭旌,李宁,唐定骧.CO对LaNi_(4.7)Al_(0.3)合金吸氢动力学特性的影响[J].功能材料,2000,31(6):598-600.

4刘友成,周惦武,高丽洁.基于第一性原理计算的Zr微合金化对NiAl力学性能的影响研究[J].稀有金属与硬质合金,2013,41(4):47-51. 被引量:1

5陈律.微量P对NiAl力学性能影响的理论研究[J].稀有金属材料与工程,2012,41(S2):290-294. 被引量:1

6陈律,彭平,湛建平,韩绍昌.Fe对NiAl力学性能影响的第一原理计算[J].稀有金属材料与工程,2010,39(2):229-233. 被引量:7

7陈律,文韬.B_2-NiAl弹性性质Ag合金化效应的理论研究[J].航空材料学报,2011,31(2):1-7. 被引量:8

8胡艳军,彭平,李贵发,周惦武,韩绍昌.NiAl力学性质合金化效应的第一原理计算[J].中国有色金属学报,2006,16(1):47-53. 被引量:10

9陈律.B2-NiAl力学性质Cr合金化效应的第一原理计算[J].中国材料科技与设备,2009,6(5):54-60.

10胡艳军,彭平,周惦武,李贵发,郑采星,韩绍昌.3d过渡金属在NiAl中占位的第一原理计算[J].中国有色金属学报,2004,14(12):2102-2107. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TG146.16[金属学及工艺—金属材料]

Citation Information:

Calculation and analysis were made of the effects of Co concentration on the mechanical properties of NiAl alloy based on virtual crystal approximation and using the first-principles pseudopotential plane- wave method. The results from elastic modulus calculation and analysis show that after B2-NiAl crystal is alloyed with Co, its hardness is increased except x (Co) = 2%, and obviously increased in the low concentration range of x(Co)=0-0.5 %, and the increase degree is lower in the high concentration range of x(Co)=3-25%. At the same time, the ductility of B2-NiAl crystal is decreased at first and then increased,decreased only a little at x(Co) =0-0.5% and obviously at x(Co)=0.5%-4 % ,and increased gradually at x(Co) =4%-25%.

quote

GB/T 7714-2015 [1] LIU You-cheng, GAO Li-jie. Effects of Concentration of the Alloying Element Co on the Mechanical Properties of NiAl[J]. Rare Metals and Cemented Carbides, 2013(6): 33-38.
MLA [1] LIU You-cheng, and GAO Li-jie. "Effects of Concentration of the Alloying Element Co on the Mechanical Properties of NiAl." Rare Metals and Cemented Carbides, no. 6, 2013, pp. 33-38.
APA [1] LIU You-cheng, & GAO Li-jie. (2013). Effects of Concentration of the Alloying Element Co on the Mechanical Properties of NiAl. Rare Metals and Cemented Carbides(6), 33-38.
IEEE [1] LIU You-cheng and GAO Li-jie, "Effects of Concentration of the Alloying Element Co on the Mechanical Properties of NiAl," Rare Metals and Cemented Carbides, no. 6, pp. 33-38, 2013. keywords: {B2-NiAl;Co alloying;Co concentration;mechanical property;elastic modulus;first-principles cal- culation}