Study of RE Mo Alloy Microstructure AITranslate
Abstract AITranslate
Based on TZM molybdenum alloy,new alloys can be produced by addition of cerium,which have the excellent high temperature properties,meanwhile,process can be controlled more easily.Their microstructure is discussed in detail in the paper.It indicates that disperse particles exist not only at grain boundary but also in grain,so they can strengthen both boundary and grain simultaneously.But coarse disperse particles and Mo-Ti solid solution are disadvantageous to alloy properties.The disperse phase in the alloys can be enriched by chemical treatment,the phase structures are identified by XRD and EDS technique.Rare earth elements of yttrium and cerium are proved that they can form composite oxides together with titanium and zirconium.In the alloys titanium presents three possible states:the composite oxides mentioned above,composite particles as Ti(CN)or Mo-Ti solid solution.
KeyWords AITranslate
1《稀有金属手册》编辑委员会.稀有金属手册[M].北京:冶金工业出版社,1992..
1段素红,张国赏,魏世忠,彭光辉,徐流杰,侯书增.液-液掺杂Mo-La_2O_3板材的室温力学性能[J].稀有金属与硬质合金,2011,39(2):29-32. 被引量:2
2刘强,魏世忠,徐流杰.钼合金的发展概况及研究现状[J].稀有金属与硬质合金,2011,39(4):50-52. 被引量:11
3曹冬,朱琦.低氧TZM合金的制备机理研究[J].中国钼业,2011,35(6):57-60. 被引量:2
4杨锋,王快社,刘仁智,王鹏洲.掺杂镧对TZM合金组织与性能的影响[J].机械工程材料,2012,36(3):43-45. 被引量:4
5刘强,魏世忠,徐流杰,张丹丹.黏液乳头型室管膜瘤9例临床病理分析[J].热加工工艺,2012,41(6):70-72. 被引量:1
6王鹏洲,王快社,张郑,胡平,刘仁智,康轩齐,何欢承.掺镧TZM合金的组织结构[J].金属热处理,2012,37(8):80-82. 被引量:4
7史振琦,黄晓玲,易永鹏.影响钼合金顶头使用寿命因素浅析[J].中国钼业,2014,38(5):57-60. 被引量:6
8宗立君,周海涛,丁洪波,高风雷,刘克明.热机械处理对TZM合金组织和性能的影响[J].热处理技术与装备,2016,37(4):34-39. 被引量:1
9李世磊,胡平,段毅,左烨盖,邢海瑞,李辉,邓洁,冯鹏发,王快社,胡卜亮.掺杂方式对钼合金组织与力学性能影响的研究进展[J].材料导报,2020,34(9):132-142. 被引量:3
10任雪婷,王广达,熊宁,周武平.氧化物强化钼合金的研究进展[J].粉末冶金工业,2022,32(4):131-138. 被引量:3
1胡平,王快社,康轩齐,何欢承,杨锋,王鹏洲,王华.轧制方式对La-TZM合金板材力学性能的影响[J].金属热处理,2013,38(4):37-39. 被引量:4
2胡平,王快社,何欢承,杨帆,杨锋,康轩齐,王鹏洲,王华.TZM合金板材的制备及其再结晶行为[J].金属热处理,2013,38(7):70-72. 被引量:6
3何欢承,王快社,胡平,康轩齐,王鹏洲,刘仁智.La_2O_3对TZM合金再结晶温度的影响[J].金属热处理,2014,39(2):12-15. 被引量:1
4于志涛,王快社,胡平,杨帆,谭江飞,何欢承,康轩齐,王华.低氧TZM合金研究进展[J].材料导报,2015,29(1):92-98. 被引量:11
5何欢承,王快社,胡平,康轩齐,王鹏洲,刘仁智.掺杂稀土元素镧对TZM合金板材再结晶行为的影响[J].稀有金属材料与工程,2015,44(5):1297-1300. 被引量:5
6曾毅,付小俊,王娜,刘秋萍.小粒度钼粉氧含量的影响因素研究[J].铸造技术,2015,36(7):1672-1675. 被引量:6
7居炎鹏,王爱琴.钼合金研究现状[J].粉末冶金工业,2015,25(4):58-62. 被引量:29
8宗立君,周海涛,丁洪波,高风雷,刘克明.热机械处理对TZM合金组织和性能的影响[J].热处理技术与装备,2016,37(4):34-39. 被引量:1
9王瑞雪,陈岁元,马雪耻,梁京,刘常升.激光直接沉积制备Mo-Ni-ZrO2高温耐磨复合合金梯度涂层[J].复合材料学报,2017,34(9):1989-1996. 被引量:4
10李红.钼及钼合金的冶炼技术现状及研究进展[J].中国金属通报,2019,0(6):18-18.
1王鹏洲,王快社,张郑,胡平,刘仁智,康轩齐,何欢承.掺镧TZM合金的组织结构[J].金属热处理,2012,37(8):80-82. 被引量:4
2童治安.稀土钼合金板坯的研制[J].中国钼业,2000,24(3):35-37. 被引量:4
3代宝珠,魏世忠,彭光辉,徐流杰.钼合金的强韧化机理与研究现状[J].热加工工艺,2009,38(14):51-54. 被引量:16
4蔡宗玉.TZM钼合金强化机理分析[J].钼业经济技术,1991(3):70-73. 被引量:5
5廖璐,周张健,李明.14CrODS铁素体钢的制备及其拉伸性能[J].材料工程,2012,40(4):42-46. 被引量:5
6杨银辉,翟传鑫,段素红.稀土钼合金的制备与性能研究[J].铸造技术,2014,35(7):1444-1446. 被引量:2
7郭磊,宋瑞,淡新国,金波,赵娟,张清,胡平.稀土钼合金制备工艺及强韧化机理研究现状[J].中国钼业,2017,41(2):45-51. 被引量:6
8张久兴,周美玲,周文元,王金淑,聂祚仁,左铁镛.稀土钼合金力学和热发射性能的研究[J].稀有金属,2002,26(2):124-128. 被引量:11
9成会朝,范景莲,刘涛,陈玉柏,田家敏.TZM钼合金制备技术及研究进展[J].中国钼业,2008,32(6):40-45. 被引量:33
10杨峥,田耘,柳光祖.MGH956合金冷轧薄板粗大再结晶晶粒形成机理[J].材料热处理学报,2010,31(5):1-4. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.412[金属学及工艺—金属材料]
Citation Information:
Based on TZM molybdenum alloy,new alloys can be produced by addition of cerium,which have the excellent high temperature properties,meanwhile,process can be controlled more easily.Their microstructure is discussed in detail in the paper.It indicates that disperse particles exist not only at grain boundary but also in grain,so they can strengthen both boundary and grain simultaneously.But coarse disperse particles and Mo-Ti solid solution are disadvantageous to alloy properties.The disperse phase in the alloys can be enriched by chemical treatment,the phase structures are identified by XRD and EDS technique.Rare earth elements of yttrium and cerium are proved that they can form composite oxides together with titanium and zirconium.In the alloys titanium presents three possible states:the composite oxides mentioned above,composite particles as Ti(CN)or Mo-Ti solid solution.
quote
| GB/T 7714-2015 | [1] YU Wei-qiang, WEN Xian-zhe, CHEN Xiang-ming, et al. Study of RE Mo Alloy Microstructure[J]. Rare Metals and Cemented Carbides, 2002(3): 33-37. |
| MLA | [1] YU Wei-qiang, et al., "Study of RE Mo Alloy Microstructure." Rare Metals and Cemented Carbides, no. 3, 2002, pp. 33-37. |
| APA | [1] YU Wei-qiang, WEN Xian-zhe, CHEN Xiang-ming, LIU Wu-sheng, & QIU Li-fen. (2002). Study of RE Mo Alloy Microstructure. Rare Metals and Cemented Carbides(3), 33-37. |
| IEEE | [1] YU Wei-qiang, WEN Xian-zhe, CHEN Xiang-ming, LIU Wu-sheng, and QIU Li-fen, "Study of RE Mo Alloy Microstructure," Rare Metals and Cemented Carbides, no. 3, pp. 33-37, 2002. keywords: {molybdenum alloy;rare earth;microstructure} |