daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Quasi-Solid-State Flexible Zn–Air Batteries with a Hydrophilic-Treated Co@NCNTs Array Electrocatalyst and PEO–PANa Electrolyte AITranslate

China Three Gorges University; China Three Gorges University; China Three Gorges University; China Three Gorges University; China Three Gorges University; China Three Gorges University; Wuhan Institute of Technology; China Three Gorges University; China Three Gorges University; China Three Gorges University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this work, we report an efficient and stable electrocatalyst (MoS2–Co@NCNTs) with a dense layer of MoS2 nanosheets compounded on the surface of Co@NCNTs. When tested in an oxygen-saturated electrolyte, MoS2–Co@NCNTs undergoes electrochemical reconfiguration (MoS2–Co@NCNTs–ER) and the MoS2 nanosheets are oxidized, resulting in some high-valence molybdenum–oxygen compounds (MoOx). The oxidized MoS2–ER nanoparticles significantly enhanced the hydrophilicity of the Co@NCNTs. Hydrophilicity improvement increased the electrochemical active surface area (ECSA) of MoS2–Co@NCNTs–ER and promoted the ion transport between the catalyst and electrolyte, which led to the enhanced OER/ORR catalytic performance compared with Co@NCNTs. Meanwhile, a PEO–PANa GPE with high electrical conductivity and excellent electrolyte absorption and retention capacity was reported. QSS-F-ZABs assembled with MoS2–Co@NCNTs and PEO–PANa GPE exhibit enhanced charge/discharge performance and long-cycle stability with a stable cycle of 200 h at a current density of 2 mA cm–2 and 160 h at a current density of 5 mA cm–2.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c01089

Chinese Library Classification Number:

Citation Information:

In this work, we report an efficient and stable electrocatalyst (MoS2–Co@NCNTs) with a dense layer of MoS2 nanosheets compounded on the surface of Co@NCNTs. When tested in an oxygen-saturated electrolyte, MoS2–Co@NCNTs undergoes electrochemical reconfiguration (MoS2–Co@NCNTs–ER) and the MoS2 nanosheets are oxidized, resulting in some high-valence molybdenum–oxygen compounds (MoOx). The oxidized MoS2–ER nanoparticles significantly enhanced the hydrophilicity of the Co@NCNTs. Hydrophilicity improvement increased the electrochemical active surface area (ECSA) of MoS2–Co@NCNTs–ER and promoted the ion transport between the catalyst and electrolyte, which led to the enhanced OER/ORR catalytic performance compared with Co@NCNTs. Meanwhile, a PEO–PANa GPE with high electrical conductivity and excellent electrolyte absorption and retention capacity was reported. QSS-F-ZABs assembled with MoS2–Co@NCNTs and PEO–PANa GPE exhibit enhanced charge/discharge performance and long-cycle stability with a stable cycle of 200 h at a current density of 2 mA cm–2 and 160 h at a current density of 5 mA cm–2.

quote

GB/T 7714-2015 [1] Minghui Lv, Chan Luo, Jiale Li, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01089.
MLA [1] Minghui Lv, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01089.
APA [1] Minghui Lv, Chan Luo, Jiale Li, Yulin Zhang, Qin Zeng, Niu Huang, Shenggao Wang, Yong Zheng, Wei Liu, & Liqun Ye. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01089
IEEE [1] Minghui Lv, Chan Luo, Jiale Li, Yulin Zhang, Qin Zeng, Niu Huang, Shenggao Wang, Yong Zheng, Wei Liu, and Liqun Ye, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01089.