Effects of Gd on Microstructure and Corrosion Resistance of Mg-Gd-Y-Sm-Zr Rare Earth Magnesium Alloys AITranslate
Abstract AITranslate
The effect of Gd content on corrosion resistance of Mg-Gd-Y-Sm-Zr rare earth magnesium alloys was investigated by weight loss method. The microstrueture and corrosion morphology of the alloys were observed by optical microscope (OM) and scanning electron microscope (SEM). And the alloys and their corrosion products were analyzed by XRD. The results show that after heat treatment, Mg-Gd-Y-Sm-Zr rare earth magnesium alloys are consisted of primary α-Mg matrix and precipitated phases of MgsGd and Mg24 Ys. With the increase of Gd content, the alloy grains become finer and the precipitated phases gradual- ly increase. The alloy corrosion rate increases at first and then decreases as Gd content increases, and Mg- 12Gd-2Y-1Sm-0.5Zr alloy has the best corrosion resistance.
KeyWords AITranslate
1陈增,张密林,吕艳卓,韩伟,唐定骧.锆在镁及镁合金中的作用[J].铸造技术,2007,28(6):820-822. 被引量:32
2王福会,杜克勤,张伟.镁合金的腐蚀与防护研究进展[J].中国材料进展,2011,30(2):29-34. 被引量:36
3LI Quan’an,LI Xiaofeng,ZHANG Qing,and CHEN Jun School of Materials Science and Engineering,Henan University of Science and Technology,Luoyang 471003,China.Effect of rare-earth element Sm on the corrosion behavior of Mg-6Al-1.2Y-0.9Nd alloy[J].稀有金属:英文版,2010,0(6):557-560. 被引量:9
4戴长松,吴宜勇,王殿龙,胡信国.镁及镁合金的化学镀镍[J].兵器材料科学与工程,1997,20(4):35-38. 被引量:44
5王萍,李建平,马群.Gd对ZK60铸造镁合金组织和耐蚀性能的影响[J].稀有金属材料与工程,2008,37(6):1056-1059. 被引量:18
6周伟,李全安,亢海娟,王耀贵.Mg-Gd-Y-Zr系耐热镁合金的研究进展[J].稀有金属与硬质合金,2012,40(5):51-56. 被引量:6
7李冠群,吴国华,樊昱,丁文江.镁合金的腐蚀研究现状与防护途径[J].材料导报,2005,19(11):60-64. 被引量:39
8齐伟光,王进华,邢志媛,吕绯,刘环恩,李冬梅.稀土钇对AZ91D镁合金微观组织和腐蚀性能影响的研究[J].兵器材料科学与工程,2009,32(4):80-83. 被引量:15
1李金宝,周古昕,杨润田,杜秀征,王生,郎玉婧,乔丽,毛华.轧态Mg-Gd-Y-Zr合金显微组织及耐腐蚀性能研究[J].兵器材料科学与工程,2020,0(2):42-47. 被引量:4
2江民华.稀土元素Sm对AM60镁合金显微组织和耐腐蚀性能的影响[J].热加工工艺,2015,44(4):86-89. 被引量:7
3张帅,李全安,朱宏喜,陈晓亚.Mg-Gd-Y系镁合金的腐蚀与防护研究进展[J].材料保护,2019,0(8):158-165. 被引量:4
4张甜甜,崔红卫,贾秋荣,崔晓丽,冯锐,潘尧坤,赵娟.Sm对铸态ZK30镁合金组织和耐腐蚀性能的影响[J].有色金属工程,2019,9(2):18-26. 被引量:6
1王文礼,张薇,雷宁宁,王杰.稀土元素Sm、Ce对Mg-Y系合金组织和性能的影响[J].稀有金属材料与工程,2016,45(6):1473-1476. 被引量:8
2李瑞红,蒋斌,陈志军,潘复生.Y和Sr对Mg-14Li-1Al合金组织及力学性能的影响[J].热加工工艺,2016,45(14):67-70. 被引量:9
3张璐,崔彤,史旭晨.生物医用镁合金耐蚀性的研究进展[J].腐蚀与防护,2016,37(8):666-670. 被引量:1
4高奇峰.稀土元素对AZ91D镁合金组织与性能的影响研究[J].热加工工艺,2016,45(18):84-86. 被引量:6
5介石磊,安红恩,温少飞.元素Y和Ca含量对车用AZ31镁合金力学性能的影响研究[J].热加工工艺,2017,46(24):140-142. 被引量:4
6陈君,张清.添加稀土Gd对Mg-6Al镁合金组织和耐蚀性的影响[J].材料保护,2019,52(3):35-39. 被引量:3
7付恩天,彭建洪,李海宾.溅射参数对合金表面硬质膜层性能影响的研究现状[J].热加工工艺,2020,49(20):15-18.
8张玺,刘刚,解芳,刘蒙恩,胡发平.表面处理对镁合金及其复合材料性能的影响[J].兵器材料科学与工程,2021,44(1):13-17. 被引量:2
9孙业成,王超宁,朱瑞,董可伟,孔见.微合金化法对高锰铝青铜合金组织和性能的影响[J].有色金属工程,2021,11(2):17-24. 被引量:3
10刘艳,冀杰.法兰磷化处理及锌系磷化膜的耐腐蚀性能研究[J].有色金属工程,2021,11(5):12-17. 被引量:1
1宋庭玉,王文川,杨晓禹,毛红奎,徐宏.Gd含量对AZ31合金组织和性能的影响[J].铸造技术,2015,36(5):1208-1210. 被引量:2
2李克杰,李全安,王小强.Gd对AZ81镁合金显微组织的影响[J].有色金属,2010,62(1):10-13. 被引量:10
3张金玲,何勇,李涛,王西涛,王艳丽.稀土元素Gd对AZ91镁合金摩擦磨损及腐蚀性能的影响[J].铸造技术,2014,35(7):1498-1501. 被引量:5
4贺峰,李建平,杨忠,郭永春,夏峰.Gd对Mg-5Sn-0.5Zn合金的显微组织及力学性能的影响[J].铸造,2008,57(2):130-133.
5牛高,陈云贵,唐永柏,肖素芬,章晓萍,魏尚海,赵源华.Mg-5Sn-xGd合金的铸态显微组织[J].特种铸造及有色合金,2008,28(2):150-152. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]
Citation Information:
The effect of Gd content on corrosion resistance of Mg-Gd-Y-Sm-Zr rare earth magnesium alloys was investigated by weight loss method. The microstrueture and corrosion morphology of the alloys were observed by optical microscope (OM) and scanning electron microscope (SEM). And the alloys and their corrosion products were analyzed by XRD. The results show that after heat treatment, Mg-Gd-Y-Sm-Zr rare earth magnesium alloys are consisted of primary α-Mg matrix and precipitated phases of MgsGd and Mg24 Ys. With the increase of Gd content, the alloy grains become finer and the precipitated phases gradual- ly increase. The alloy corrosion rate increases at first and then decreases as Gd content increases, and Mg- 12Gd-2Y-1Sm-0.5Zr alloy has the best corrosion resistance.
quote
| GB/T 7714-2015 | [1] LI Quan-an, CHEN Zhi, CHENG Bin, et al. Effects of Gd on Microstructure and Corrosion Resistance of Mg-Gd-Y-Sm-Zr Rare Earth Magnesium Alloys[J]. Rare Metals and Cemented Carbides, 2013(4): 26-29. |
| MLA | [1] LI Quan-an, et al., "Effects of Gd on Microstructure and Corrosion Resistance of Mg-Gd-Y-Sm-Zr Rare Earth Magnesium Alloys." Rare Metals and Cemented Carbides, no. 4, 2013, pp. 26-29. |
| APA | [1] LI Quan-an, CHEN Zhi, CHENG Bin, & ZHOU Wei. (2013). Effects of Gd on Microstructure and Corrosion Resistance of Mg-Gd-Y-Sm-Zr Rare Earth Magnesium Alloys. Rare Metals and Cemented Carbides(4), 26-29. |
| IEEE | [1] LI Quan-an, CHEN Zhi, CHENG Bin, and ZHOU Wei, "Effects of Gd on Microstructure and Corrosion Resistance of Mg-Gd-Y-Sm-Zr Rare Earth Magnesium Alloys," Rare Metals and Cemented Carbides, no. 4, pp. 26-29, 2013. keywords: {Mg-Gd-Y-Sm-Zr;rare earth magnesium alloy;Gd content;microstructure;corrosion resistance} |