Recent Development and Application of Surface Treatment and Coating Technology AITranslate

Northwest Nonferrous Metal Research Institute;Northwest Nonferrous Metal Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Physical vapor deposit ion coating are widely used in industry.New coating technology,such as duplex treatment,TiN deposition at low temperature and Ti2N coatings,are still under investigation and their field of application is not yet fully known.This paper describes the description,properties and future application of these coating systems

KeyWords AITranslate

Duplex treatment coating technology low temperature PVD

1艾兴,陈元春,李久立,黄传真,王宝友.陶瓷粉末涂层硬质合金刀具的切削性能[J].工具技术,1999,33(8):3-4. 被引量:2

2杨玫,王立华.表面涂层的制备工艺与测试技术[J].武汉科技大学学报,2003,26(3):241-244. 被引量:3

3傅小明,吴晓东.硬质合金刀具涂层技术的研究进展[J].江西冶金,2004,24(2):32-36. 被引量:4

1罗来龙,王贵学,尹铁英.药物洗脱性血管内支架药物涂层的研究进展[J].中国医疗器械杂志,2006,30(2):117-119. 被引量:4

2王泉国.数控机床上高速切削时的刀具选择分析[J].煤矿机械,2012,33(7):140-143. 被引量:2

3郭杰,徐看,刘利国,张盼盼.刀具涂层技术现状与发展趋势[J].工具技术,2014,48(3):3-7. 被引量:20

4艾兴,刘战强,赵军,邓建新,宋世学.高速切削刀具材料的进展和未来[J].制造技术与机床,2001(8):21-25. 被引量:62

5张锋刚,王永善,宋佩维,李文虎.硬质合金表面改性研究现状与展望[J].陕西理工学院学报:自然科学版,2015,31(3):8-13. 被引量:3

6陈威,吕政琳,高东强,艾旭.涂层硬质合金刀具加工碳钢切削性能及磨损机理研究[J].陕西科技大学学报:自然科学版,2015,35(5):146-152.

7高东强,艾旭,陈威,吕政琳.涂层硬质合金刀具对奥氏体不锈钢的切削特性[J].材料科学与工程学报,2016,34(3):437-444. 被引量:13

8乔宏霞,王鹏辉,巩位,王旭峰,张家畅.基于EIS研究镁水泥混凝土中涂层钢筋的耐腐蚀性[J].材料科学与工程学报,2017,35(6):987-992. 被引量:2

9姚世睿,陈永才.火炮身管内膛涂层制备技术的研究进展[J].热加工工艺,2018,47(6):41-44. 被引量:2

1宋勇敏,朱敦伦,魏振华.过共晶铝硅合金新型细化剂的研究[J].兵器材料科学与工程,1994,17(2):37-40. 被引量:6

2黄金昌.低温沉积Ti—6Al—4V合金上的(Ti,Al,V)N涂层生物相容和机械性能[J].稀有金属快报,1997(7):14-15.

3高晓明,孙嘉奕,胡明,翁立军,伏彦龙,杨军,谭洪根,张良俊.低温沉积银和银铜薄膜的耐原子氧性能[J].机械工程材料,2013,37(11):55-59. 被引量:3

4高晓明,孙嘉奕,胡明,翁立军,刘维民.低温沉积Cu膜的晶体结构及摩擦磨损性能的初步研究[J].摩擦学学报,2007,27(4):308-312. 被引量:5

5周伟,曲恒磊,赵永庆,李辉,冯亮,陈军.TC4-DT合金不同热处理后的组织与性能[J].金属热处理,2006,31(6):56-57. 被引量:18

6孙嘉奕,翁立军,李陇旭,汪晓萍,于翔.LY12CZ铝合金的双重处理表面摩擦学改性研究[J].润滑与密封,2001,26(4):38-40. 被引量:1

7黄美东,孙超,林国强,董闯,闻立时.脉冲偏压电弧离子低温沉积TiN硬质薄膜的力学性能[J].金属学报,2003,39(5):516-520. 被引量:34

8周伟,葛鹏,赵永庆,陈军.一种新型亚稳定β钛合金的组织与性能研究[J].热加工工艺,2007,36(22):18-20. 被引量:5

9程晓敏,宫殿清,苏光浩,吴兴文.轧辊用高铬钢组织与性能的优化研究[J].中国水运:下半月,2008,8(12):148-149. 被引量:2

10魏馥铭,黄峥,朱雅年,余荷英,徐挺,姚勇,刘锋.4Cr5MoV1Si钢的热疲劳性能研究[J].上海大学学报:自然科学版,1997,3(4):400-408. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG174.44[金属学及工艺—金属表面处理]

Citation Information:

Physical vapor deposit ion coating are widely used in industry.New coating technology,such as duplex treatment,TiN deposition at low temperature and Ti2N coatings,are still under investigation and their field of application is not yet fully known.This paper describes the description,properties and future application of these coating systems

quote

GB/T 7714-2015 [1] HUANG Jin-chang, XU Xiu-ru. Recent Development and Application of Surface Treatment and Coating Technology[J]. Rare Metals and Cemented Carbides, 1997(3): 60-62.
MLA [1] HUANG Jin-chang, and XU Xiu-ru. "Recent Development and Application of Surface Treatment and Coating Technology." Rare Metals and Cemented Carbides, no. 3, 1997, pp. 60-62.
APA [1] HUANG Jin-chang, & XU Xiu-ru. (1997). Recent Development and Application of Surface Treatment and Coating Technology. Rare Metals and Cemented Carbides(3), 60-62.
IEEE [1] HUANG Jin-chang and XU Xiu-ru, "Recent Development and Application of Surface Treatment and Coating Technology," Rare Metals and Cemented Carbides, no. 3, pp. 60-62, 1997. keywords: {Duplex treatment,coating technology, low temperature PVD}