A Compact Volume-Expandable Sorbent for Oil and Solvent Capture AITranslate

Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Many sorbents demonstrate exceptionally high absorbance capacity on a per unit mass basis, with some sorbents capable of absorbing hundreds of times their own mass. However, the volumetric capacity (volume of the absorbed liquid per unit volume of the sorbent) remains close to a one-to-one ratio, making transportation and storage of sorbents intended for large volumes of liquid a challenge. A compact volume-expandable sorbent (CVES) has been developed through polymerizing the organic phase of a high internal phase emulsion (HIPE). These polymeric sorbents can transform from a collapsed state (when dry) to an expanded intermediate state (when absorbing a wetting solvent) and to a fully expanded and swollen state (when absorbing a good solvent) and are capable of absorbing a volume of organic liquid more than 20 times the original volume of the sorbent. The CVES demonstrates excellent oil–water selectivity due to a multiscale structure consisting of voids in the porous solid on the order of tens of micrometers and smaller (submicrometer scale) voids within the internal struts as a result of phase separation that occurs during curing of the HIPE. Furthermore, the CVES has a low compression hysteresis loss and retains high oil absorption performance after many cycles of use. Because of these aforementioned properties, the CVES represents a type of high-performance sorbent.

KeyWords AITranslate

polyHIPEs porous materials selective sorbents selfcompacting reusable and recyclable sorbent
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01324

Chinese Library Classification Number:

Citation Information:

Many sorbents demonstrate exceptionally high absorbance capacity on a per unit mass basis, with some sorbents capable of absorbing hundreds of times their own mass. However, the volumetric capacity (volume of the absorbed liquid per unit volume of the sorbent) remains close to a one-to-one ratio, making transportation and storage of sorbents intended for large volumes of liquid a challenge. A compact volume-expandable sorbent (CVES) has been developed through polymerizing the organic phase of a high internal phase emulsion (HIPE). These polymeric sorbents can transform from a collapsed state (when dry) to an expanded intermediate state (when absorbing a wetting solvent) and to a fully expanded and swollen state (when absorbing a good solvent) and are capable of absorbing a volume of organic liquid more than 20 times the original volume of the sorbent. The CVES demonstrates excellent oil–water selectivity due to a multiscale structure consisting of voids in the porous solid on the order of tens of micrometers and smaller (submicrometer scale) voids within the internal struts as a result of phase separation that occurs during curing of the HIPE. Furthermore, the CVES has a low compression hysteresis loss and retains high oil absorption performance after many cycles of use. Because of these aforementioned properties, the CVES represents a type of high-performance sorbent.

quote

GB/T 7714-2015 [1] Boran Zhao, Kristen Rohm, Fan Wang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01324.
MLA [1] Boran Zhao, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01324.
APA [1] Boran Zhao, Kristen Rohm, Fan Wang, Xuehui Gong, Ica ManasZloczower, & Donald L. Feke. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01324
IEEE [1] Boran Zhao, Kristen Rohm, Fan Wang, Xuehui Gong, Ica ManasZloczower, and Donald L. Feke, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01324. keywords: {polyHIPEs;porous materials;selective sorbents;selfcompacting;reusable and recyclable sorbent}