Real-Time Personal Fever Alert Monitoring by Wearable Detector Based on Thermoresponsive Hydrogel AITranslate

King Abdullah University of Science and Technology; Northwestern Polytechnical University; Northwestern Polytechnical University; Northwestern Polytechnical University; Northwestern Polytechnical University; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology; Northwestern Polytechnical University; Northwestern Polytechnical University; Saudi Arabia|Hong Kong Polytechnic University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Quick fever screening at a mass scale is proven effective during a pandemic to single out the ones with suspected symptoms of infectious diseases. However, achieving affordable and real-time fever alert at an individual level, although more preferable, remains elusive. Herein, we report an inexpensive and highly sensitive fever detector, which possesses a sharp color transition temperature window tailor-tuned for fever screening. The sensing component of the detector is rationally designed thermoresponsive agarose@poly(N-isopropylacrylamide)-co-acrylamide hydrogel. The hydrogel turns from transparent to opaque white when its temperature is higher than its cloud point. As a proof of concept of its practical applicability, a wearable fever monitoring device was fabricated in the form of a wristband. When the wrist temperature is higher than the threshold of a human fever, the device shows a remarkable color change, alerting an elevated body temperature. The wearable detector provides a promising strategy for real-time fever alert monitoring and is capable of making contributions to inhibit the spread of infectious diseases during a pandemic.

KeyWords AITranslate

fever Screening body temperature monitoring thermal sensitive hydrogel wearable device PNIPAM hydrogel
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01275

Chinese Library Classification Number:

Citation Information:

Quick fever screening at a mass scale is proven effective during a pandemic to single out the ones with suspected symptoms of infectious diseases. However, achieving affordable and real-time fever alert at an individual level, although more preferable, remains elusive. Herein, we report an inexpensive and highly sensitive fever detector, which possesses a sharp color transition temperature window tailor-tuned for fever screening. The sensing component of the detector is rationally designed thermoresponsive agarose@poly(N-isopropylacrylamide)-co-acrylamide hydrogel. The hydrogel turns from transparent to opaque white when its temperature is higher than its cloud point. As a proof of concept of its practical applicability, a wearable fever monitoring device was fabricated in the form of a wristband. When the wrist temperature is higher than the threshold of a human fever, the device shows a remarkable color change, alerting an elevated body temperature. The wearable detector provides a promising strategy for real-time fever alert monitoring and is capable of making contributions to inhibit the spread of infectious diseases during a pandemic.

quote

GB/T 7714-2015 [1] Wenbin Wang, Chen Wu, Kai Zhu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01275.
MLA [1] Wenbin Wang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01275.
APA [1] Wenbin Wang, Chen Wu, Kai Zhu, Fang Chen, Jingjing Zhou, Yusuf Shi, Chenlin Zhang, Renyuan Li, Mengchun Wu, Sifei Zhuo, Hepeng Zhang, & Peng Wang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01275
IEEE [1] Wenbin Wang, Chen Wu, Kai Zhu, Fang Chen, Jingjing Zhou, Yusuf Shi, Chenlin Zhang, Renyuan Li, Mengchun Wu, Sifei Zhuo, Hepeng Zhang, and Peng Wang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01275. keywords: {fever Screening;body temperature monitoring;thermal sensitive hydrogel;wearable device;PNIPAM;hydrogel}