Abstract AITranslate

Manufacturing technologies and refinement methods for dysprosium metal were reviewed. The application of dysprosium in NdFeB permanent magnet,rare earth giant magnetostrictive material,magneto optical recording media and other rare earth functional materials were introduced. Some suggestions were given on further research and development as well as mass production of dysprosium metal.

KeyWords AITranslate

rare erath dysprosium metal manufacture refinement rare earth functional materials

1杜挺,张洪平,朱厚卿.Tb_1-_xDy_x(Fe_1-_yMn_y)_(1.95)合金的磁致伸缩和声学性质及在水声换能器中的应用[J].中国稀土学报,1999,17(2):107-110. 被引量:2

2胡华业.高纯金属钪的制备[J].稀土,1999,20(4):70-72. 被引量:10

3章复中,杨志尚,任立斌,周荣章,余宗森.Ti-Al-Dy三元系相图1000℃部分等温截面的测定[J].中国稀土学报,1996,14(3):211-214. 被引量:1

4罗广圣,贺伦燕.金属间化物(Sm_(1-x)Dy_x)_2Fe_(17)N_y中的各向异性机制探讨[J].稀土,1995,16(5):6-9. 被引量:1

5苏明忠,宋丕莹,邹天楚,路连清,刘素兰,杜森林.熔盐电解制备Al—Dy合金[J].稀土,1995,16(5):61-63. 被引量:3

6郭锋,韩允斌.金属镝中的钙与氧[J].稀土,1995,16(6):61-63. 被引量:8

7何国,周寿增,李建国,魏朋义,傅恒志.我国稀土超磁致伸缩材料的研究与应用现状[J].材料导报,1996,10(5):12-17. 被引量:5

8应启明,罗梓贤,李东培,王瑞坤,姚国庆,任世宽,张健,孙丽红.稀土大磁致伸缩材料研究[J].稀土,1999,20(1):72-74. 被引量:19

9稀土超导陶瓷[J].稀土,1999,20(2):76-78. 被引量:2

10李碚,伍虹,高军,江丽萍,刘翠兰.(TbDy)Fe_2基定向凝固磁致伸缩合金的性能与组织和成分的关系[J].中国稀土学报,1998,16(4):332-338. 被引量:16

1刘永林,李国云,李国栋.用熔盐萃取法制备低氧金属镝的研究[J].中国稀土学报,2002,20(z2):33-35. 被引量:2

2李国云,李国栋,刘永林.熔盐萃取法制备低氧、低氟金属镝的机制研究[J].中国稀土学报,2002,20(z2):263-265. 被引量:1

3王中磊,唐惠庆,郭占成,叶伟,蔡卓飞.直接电解法制取金属镝的阴极制备工艺研究[J].稀有金属,2010,34(5):755-763. 被引量:6

4云月厚,黄焦宏,刘文生,邰显康,李国栋.钙热还原及熔盐萃取联合法一次性制备低氧低氟金属镝[J].稀土,2006,27(3):91-93. 被引量:6

5刘宝忠.高纯金属镝的制备[J].稀有金属快报,2008,27(7):39-42. 被引量:7

6刘永林,云月厚.LiF-YF_3熔盐萃取提纯金属钇的研究[J].稀土,2010,31(1):92-94. 被引量:4

7金炳勋,谢宏伟,毛景,翟玉春.1-乙基-3-甲基-咪唑四氟硼酸盐离子液体中镝电沉积行为[J].稀有金属材料与工程,2012,41(5):881-884. 被引量:7

8郝占忠,王斌,张海玲.新型固定床气体氟化法制备低氧氟化钆[J].稀土,2013,34(5):16-21. 被引量:6

9李中华,朱伟长.氧化镝纳米粉体材料的制备[J].甘肃冶金,2013,35(6):56-57. 被引量:2

10刘木根,王薪鹏,吴英.金属镝生产工艺的改良[J].中国稀土学报,2014,32(3):354-362. 被引量:1

1林玉翠,张红润,刘立钧.高纯氧化镝纳米材料晶粒尺寸测试现状及标准研制[J].中国标准化,2021(S01):157-160.

2廖春发,郭超,林觉远,蔡伯清,王旭.电流密度对稀土熔盐电解影响的研究进展[J].稀土,2021(1):122-128. 被引量:4

3贾雷,严红燕,李慧,刘畅,张帅.金属铪的制备和精炼[J].热加工工艺,2020,0(1):10-15. 被引量:1

4王旭,廖春发.熔盐电解法制备金属钨粉的技术分析及发展前景[J].稀有金属,2011,35(4):587-592. 被引量:5

5成维,李宗安,陈德宏,庞思明,王志强,王祥生.锂热还原-真空蒸馏联合法制备高纯金属镧工艺研究[J].稀有金属,2011,35(5):781-785. 被引量:8

6史丽秀,朱茜.住宅主空间室内设计的思考[J].室内设计,2000(1):36-41. 被引量:2

7叶章根,陈松,李文良,吴延科,王力军.熔盐电解精炼铪的研究[J].稀有金属,2012,36(5):791-798. 被引量:13

8Ze-quan Li,Li-yue Ru,Cheng-guang Bai,Na Zhang,Hai-hua Wang.Effect of sintering temperature on the electrolysis of TiO_2[J].矿物冶金与材料学报:英文版,2012,19(7):636-641. 被引量:1

9成维,黄美松,王志坚,杨露辉.钙热还原法制备高纯金属镧的研究[J].矿冶工程,2013,33(3):104-106. 被引量:11

10武淑珍,王铁虎,许方,刘徽平.高纯稀土金属制备工艺的研究现状[J].稀有金属与硬质合金,2013,41(4):10-13. 被引量:3

1顾楠.稀土关税取消之后[J].中国有色金属,2015,0(18):42-43. 被引量:1

2魏宏亮.烧结机返矿率影响因素探索[J].浙江冶金,2010(2):23-25. 被引量:2

3袁萍,颜豪威,陶利明,徐秋华.高纯金属铽的试生产[J].江西冶金,1999,19(5):18-21.

4“中国稀土学会第二届青年学术年会”第一轮通知[J].稀有金属,2007,0(S2):96-96.

5祝爱兰.镍溶液提纯方法研究现状[J].湿法冶金,2012,31(2):71-75. 被引量:6

6李碧春,肖英龙.国内外不锈钢冶炼技术现状及相关建议[J].重钢技术,1998,41(3):45-52.

7胡志方,尹延西,江洪林,田丽森,薛红霞,王力军.金属钙及高纯钙制备技术[J].矿冶,2013,22(2):63-66. 被引量:1

8田敬龙.高炉煤气干法除尘技术发展现状及宝钢应用前景[J].冶金能源,2007,26(5):3-4. 被引量:5

9田敬龙.高炉煤气干法除尘技术发展现状及宝钢应用前景[J].冶金动力,2007(6):20-21. 被引量:10

10吴志伟.高炉煤气干法除尘技术发展现状及邯钢应用前景[J].冶金信息导刊,2008,45(4):23-25.

Basic Information:

DOI:

Chinese Library Classification Number:TF845.3[冶金工程—有色金属冶金]

Citation Information:

Manufacturing technologies and refinement methods for dysprosium metal were reviewed. The application of dysprosium in NdFeB permanent magnet,rare earth giant magnetostrictive material,magneto optical recording media and other rare earth functional materials were introduced. Some suggestions were given on further research and development as well as mass production of dysprosium metal.

quote

GB/T 7714-2015 [1] ZHANG Shi-rong. Manufacture, Refinement and Application of Dysprosium Metal[J]. Rare Metals and Cemented Carbides, 2000(3): 53-59.
MLA [1] ZHANG Shi-rong. "Manufacture, Refinement and Application of Dysprosium Metal." Rare Metals and Cemented Carbides, no. 3, 2000, pp. 53-59.
APA [1] ZHANG Shi-rong. (2000). Manufacture, Refinement and Application of Dysprosium Metal. Rare Metals and Cemented Carbides(3), 53-59.
IEEE [1] ZHANG Shi-rong, "Manufacture, Refinement and Application of Dysprosium Metal," Rare Metals and Cemented Carbides, no. 3, pp. 53-59, 2000. keywords: {rare erath;dysprosium metal;manufacture;refinement;rare earth functional materials}