Catechol End-Capped Poly(arylene sulfide) as a High-Refractive-Index “TiO2/ZrO2-Nanodispersible” Polymer AITranslate

Waseda University; Waseda University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Poly(arylene sulfide)s (PASs) with a functional group at one terminus were successfully prepared by end functionalization of a disulfide end in a precursor PAS obtained via oxidative polymerization. End functionalization of methoxy-substituted PAS (OMePPS) with a carboxylic acid or catechol unit afforded not only high refractive indices up to 1.7 but also a high dispersivity of TiO2/ZrO2 nanoparticles with a size of a few 30 nm, owing to the high affinity of the end group for inorganic oxide nanoparticles. In particular, the catechol-functionalized OMePPS showed remarkably high dispersivity of inorganic nanoparticles, and the hybrid film of this polymer with 30 wt % of ZrO2 nanoparticles exhibited a higher refractive index of 1.82 at the D line (589.3 nm).

KeyWords AITranslate

poly(phenylene sulfide) end functionalization high refractive index polymer−inorganic nanohybrid materials composites polymers
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00536

Chinese Library Classification Number:

Citation Information:

Poly(arylene sulfide)s (PASs) with a functional group at one terminus were successfully prepared by end functionalization of a disulfide end in a precursor PAS obtained via oxidative polymerization. End functionalization of methoxy-substituted PAS (OMePPS) with a carboxylic acid or catechol unit afforded not only high refractive indices up to 1.7 but also a high dispersivity of TiO2/ZrO2 nanoparticles with a size of a few 30 nm, owing to the high affinity of the end group for inorganic oxide nanoparticles. In particular, the catechol-functionalized OMePPS showed remarkably high dispersivity of inorganic nanoparticles, and the hybrid film of this polymer with 30 wt % of ZrO2 nanoparticles exhibited a higher refractive index of 1.82 at the D line (589.3 nm).

quote

GB/T 7714-2015 [1] Seigo Watanabe, Kenichi Oyaizu. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00536.
MLA [1] Seigo Watanabe, and Kenichi Oyaizu. ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00536.
APA [1] Seigo Watanabe, & Kenichi Oyaizu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00536
IEEE [1] Seigo Watanabe and Kenichi Oyaizu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00536. keywords: {poly(phenylene sulfide);end functionalization;high refractive index;polymer−inorganic nanohybrid materials;composites;polymers}