Study on Process for Ni-Mo-Co Alloy Electrode Preparation AITranslate

Beijing Nonferrous Metal Research Institute of Energy Materials and Technology Research Institute;Beijing Nonferrous Metal Research Institute of Energy Materials and Technology Research Institute;Beijing Nonferrous Metal Research Institute of Energy Materials and Technology Research Institute;Beijing Nonferrous Metal Research Institute of Energy Materials and Technology Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ternary Ni-Mo-Co alloy electrode was prepared by electrodeposition.The effects of deposition current density,and temperature and pH of electroplating solution were studied on the catalytic activity for hydrogen evolution reaction of the alloy electrode.The chemical composition and microstructure of the alloy electrode were investigated by EDS and XRD.Based on the polarization curves,the optimal technological conditions can be determined,including deposition current density 15 mA/cm2,temperature 25 ℃ and electroplating solution pH 10.Under the above conditions,the prepared alloy electrode is of amorphous structure,silver bright appearance,smooth and compact surface,and the chemical composition of 34.09% Ni,59.51% Mo and 6.40% Co.Meanwhile,its overpotential of hydrogen evolution in 30% KOH solution is 112 mV,that is 352 mV lower than that of Ni electrode,showing better catalytic activity for hydrogen evolution.

KeyWords AITranslate

Ni-Mo-Co alloy electrodeposition preparation condition polarization curve hydrogen evolution reaction

1李贺,姚素薇,张卫国,王宏智.电化学技术制备析氢电极材料的研究进展[J].化工进展,2005,24(7):718-722. 被引量:16

2Han Qing, Liu Kuiren, Chen Jianshe, et al. Study of a morphous Ni-S-Co alloy used as hydrogen evolution re action cathode in alkaline medium[J]. International Jour nat of Hydrogen Energy, 2004,29:24 a-g48.

3李聪,许洪胤,杜朝军,郑盛会.电沉积Ni-Mo-P合金及其析氢电催化性能的研究[J].电镀与环保,2005,25(1):10-11. 被引量:8

4Giz M J, Bento S C, Gonzalez E R. NiFeZn codeposit as a cathode material for the production of hydrogen by water electrolysis[J].International Journal of Hydrogen Energy, 2000,25 : 621-626.

5Ramesh L, Sheshadri B S, Mayanna S M. Electrolytic preparation and characterization of Ni-Mo-Fe alloys: cathode materials for alkaline water electrolysis [J]. International Journal of Energy Research, 1999,23 (10) : 919-924.

6朱波,刘贵昌,施志聪,王华,刘伟.高析氢活性Ni-Mo-Zn合金电极的制备与表征[J].微细加工技术,2008(6):22-25. 被引量:3

7邹勇进,肖作安,费锡明.电沉积Co-Ni-W合金电极在碱性溶液中的析氢电催化活性[J].稀有金属,2004,28(5):954-957. 被引量:8

8黄令,杨防阻,许书楷,周绍民.纳米晶Ni-Mo-Co合金镀层的结构与析氢行为[J].应用化学,2001,18(10):767-771. 被引量:13

9杨静,张存中,吴仲达.非晶态Ni-Mo-Co合金电极的制备和析氢性能[J].应用化学,2000,17(5):475-478. 被引量:16

10Dolati A G,Ghorbani M,Afshar A. The electro-deposition of quaternary Fe-Cr-Ni-Mo alloys from the chloride -complexing agents electrolyte (Part I. Processing) [J]. Surface and Coatings Technology, 2003,166 ( 2-3 ) :105-110.

1周新宇,王一雍,金辉,梁智鹏,刘香琳.Ni-Co/ZrO_2复合镀层的电化学研究和性能表征[J].稀有金属与硬质合金,2018,46(5):54-58. 被引量:1

1敬双怡,侯娜,范保建,于玲红,李卫平,殷震育.稀土镨电极处理焦化尾水过程特性研究[J].现代化工,2021,41(8):139-144.

1孔亚鹏,陈建设,刘奎仁,韩庆.脉冲镀Ni-Mo-Co合金镀层及其析氢性能[J].东北大学学报:自然科学版,2016,37(6):815-819. 被引量:2

2陈良木,陈范才,李文军,吴道明,徐超,王子天.电沉积镍-钼-钴泡沫合金析氢电极的工艺研究[J].电镀与涂饰,2010,29(8):1-3. 被引量:7

3范宏义.硬Ni—P镀层[J].材料保护,2002,35(11):65-66.

4姚素薇,刘春松,张卫国,王宏智,张溪.双脉冲电沉积制备Ni-聚苯胺复合电极及其析氢性能的研究[J].电镀与涂饰,2006,25(2):1-4. 被引量:6

5许兴欣,康丹苗,刘庆雷,张荻.电极制备工艺对褐藻多孔碳双电层电容性能的影响[J].材料科学与工艺,2016,24(1):51-57.

6李宁,丁大勇,黎德育.非晶态Ni-Co-P膜层在碱性介质中的电催化析氢性能[J].哈尔滨工业大学学报,2005,37(9):1185-1188. 被引量:6

7李远会,王海峰,黄碧芳,张晓燕,郭忠诚.电镀Cu-Mo-Co合金的热力学分析[J].电镀与精饰,2013,35(8):12-14.

8李玉敏,王海南,王日杰,张继炎,张鎏.Mo-Co-Mg/Al_2O_3工业耐硫变换催化剂的失活[J].应用化学,1999,16(1):42-45. 被引量:1

9脉冲电镀纳米镍[J].材料保护,2003,36(8):78-79.

10辜敏,杨防祖,黄令,姚士冰,周绍民.高择优取向Cu电沉积层的XRD研究[J].电化学,2002,8(3):282-287. 被引量:35

Basic Information:

DOI:

Chinese Library Classification Number:TQ153.2[化学工程—电化学工业]

Citation Information:

Ternary Ni-Mo-Co alloy electrode was prepared by electrodeposition.The effects of deposition current density,and temperature and pH of electroplating solution were studied on the catalytic activity for hydrogen evolution reaction of the alloy electrode.The chemical composition and microstructure of the alloy electrode were investigated by EDS and XRD.Based on the polarization curves,the optimal technological conditions can be determined,including deposition current density 15 mA/cm2,temperature 25 ℃ and electroplating solution pH 10.Under the above conditions,the prepared alloy electrode is of amorphous structure,silver bright appearance,smooth and compact surface,and the chemical composition of 34.09% Ni,59.51% Mo and 6.40% Co.Meanwhile,its overpotential of hydrogen evolution in 30% KOH solution is 112 mV,that is 352 mV lower than that of Ni electrode,showing better catalytic activity for hydrogen evolution.

quote

GB/T 7714-2015 [1] WANG Guo-qing, WEI Hai-jun, ZHU Lei, et al. Study on Process for Ni-Mo-Co Alloy Electrode Preparation[J]. Rare Metals and Cemented Carbides, 2011(1): 21-24.
MLA [1] WANG Guo-qing, et al., "Study on Process for Ni-Mo-Co Alloy Electrode Preparation." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 21-24.
APA [1] WANG Guo-qing, WEI Hai-jun, ZHU Lei, & JIAN Xu-yu. (2011). Study on Process for Ni-Mo-Co Alloy Electrode Preparation. Rare Metals and Cemented Carbides(1), 21-24.
IEEE [1] WANG Guo-qing, WEI Hai-jun, ZHU Lei, and JIAN Xu-yu, "Study on Process for Ni-Mo-Co Alloy Electrode Preparation," Rare Metals and Cemented Carbides, no. 1, pp. 21-24, 2011. keywords: {Ni-Mo-Co alloy;electrodeposition;preparation condition;polarization curve;hydrogen evolution reaction}