daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Liquid Metal Hybrid Composites with High-Sensitivity and Large Dynamic Range Enabled by Micro- and Macrostructure Engineering AITranslate

University of Science and Technology of China; University of Birmingham; University of Wollongong; University of Birmingham; University of Science and Technology of China; University of Science and Technology of China; University of Birmingham; University of Wollongong; University of Science and Technology of China; North Carolina State University; University of Wollongong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Conductive elastic composites composed of conductive fillers and polymer matrices are showing an increasing number of applications in the fields of flexible sensors, wearable devices, and stretchable electronics. Under mechanical deformation, the conductive filler network in the matrix shifts to change the conductive pathway among particles and thus, electrical conductivity of the composite. For most conductive composites, their conductivity changes monotonically with strain. Here, we report a composite that exhibits an unconventional strain response; its electrical conductivity increases sharply under both compressive and tensile loads. The Ecoflex-based composite contains spike-shaped nickel microparticles and liquid metal microdroplets. Because of the elastomeric mechanical properties of Ecoflex, the composite has an extremely high stretchability and pressure sensitivity, which is ideal for tactile sensing and mechanical responsiveness. On the basis of a composite film with a grooved or pyramidal surface structure, we demonstrate a pressure-controlled intelligent heating film and a pressure sensor with extremely high sensitivity and dynamic range.

KeyWords AITranslate

conductive elastomer liquid metal multiscale structure design high sensitivity flexible sensor stretchable electronics
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01111

Chinese Library Classification Number:

Citation Information:

Conductive elastic composites composed of conductive fillers and polymer matrices are showing an increasing number of applications in the fields of flexible sensors, wearable devices, and stretchable electronics. Under mechanical deformation, the conductive filler network in the matrix shifts to change the conductive pathway among particles and thus, electrical conductivity of the composite. For most conductive composites, their conductivity changes monotonically with strain. Here, we report a composite that exhibits an unconventional strain response; its electrical conductivity increases sharply under both compressive and tensile loads. The Ecoflex-based composite contains spike-shaped nickel microparticles and liquid metal microdroplets. Because of the elastomeric mechanical properties of Ecoflex, the composite has an extremely high stretchability and pressure sensitivity, which is ideal for tactile sensing and mechanical responsiveness. On the basis of a composite film with a grooved or pyramidal surface structure, we demonstrate a pressure-controlled intelligent heating film and a pressure sensor with extremely high sensitivity and dynamic range.

quote

GB/T 7714-2015 [1] Guolin Yun, ShiYang Tang, Hongda Lu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01111.
MLA [1] Guolin Yun, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01111.
APA [1] Guolin Yun, ShiYang Tang, Hongda Lu, Tim Cole, Shuaishuai Sun, Jian Shu, Jiahao Zheng, Qingtian Zhang, Shiwu Zhang, Michael D. Dickey, & Weihua Li. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01111
IEEE [1] Guolin Yun, ShiYang Tang, Hongda Lu, Tim Cole, Shuaishuai Sun, Jian Shu, Jiahao Zheng, Qingtian Zhang, Shiwu Zhang, Michael D. Dickey, and Weihua Li, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01111. keywords: {conductive elastomer;liquid metal;multiscale structure design;high sensitivity flexible sensor;stretchable electronics}