Present Status of Beryllium Production and its Development and Application AITranslate

Beijing Nonferrous Metal Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The article introduces the distribution of mineral resource and reserve of beryllium and present status of Be production of main manufacturers in the world. It describes in details theapplication and development of Be-metal、Be-Cu、Be-alloys and Be-oxides in all the fields. Finally it analyzes and forecasts the supply and demand of Be up to 2000 year.

KeyWords AITranslate

beryllium industry mineral resource production status application and development market demand

1杨雨浓.世界和日本的铍市场[J]稀有金属与硬质合金,1988(03).

1刘晓文,毛小西,刘庄,华燕莉.羟硅铍石型铍矿的工艺矿物学研究[J].矿物学报,2010,30(S1):61-63. 被引量:8

2李爱民,蒋进光,王晖,符剑刚.含铍矿物浮选研究现状与展望[J].稀有金属与硬质合金,2008,36(3):58-61. 被引量:13

3符剑刚,蒋进光,李爱民,王晖.从含铍矿石中提取铍的研究现状[J].稀有金属与硬质合金,2009,37(1):40-44. 被引量:20

4陈希春,董超群,朱宝辉,陈林.气氛保护电渣重熔铍铜合金QBe2.0的冶金质量研究[J].稀有金属,2011,35(5):786-790. 被引量:4

5张涛.8-羟基喹啉分光光度法测定铍铜中间合金中铝[J].冶金分析,2013,33(3):60-64. 被引量:12

6刘勇,刘牡丹,刘珍珍,万丽.低品位铍精矿冶金处理新工艺的实验研究[J].稀有金属与硬质合金,2014,42(2):13-15. 被引量:6

7王仁财,邢佳韵,彭浩.美国铍资源战略启示[J].中国矿业,2014,23(10):21-24. 被引量:9

8马进,桑利,张恩玉,贡大雷,鲁兴武,邵传兵.高氟铍矿浸出液共沉淀法除杂新工艺研究[J].稀有金属,2015,39(5):468-472. 被引量:3

9梁飞,赵汀,王登红,刘超,王安建.中国铍资源供需预测与发展战略[J].中国矿业,2018,27(11):6-10. 被引量:11

10邓伟,颜世强,谭洪旗,杨耀辉,王昌良.我国铍矿资源概况及选矿技术研究现状[J].矿产综合利用,2023(1):148-154. 被引量:2

1刘晓文,毛小西,刘庄,华燕莉.羟硅铍石型铍矿的工艺矿物学研究[J].矿物学报,2010,30(S1):61-63. 被引量:8

2朱薇,刘志强,陈怀杰.从某低品位稀有、稀土复合矿浸出液中萃取铍的实验研究[J].材料研究与应用,2010,4(4):387-390. 被引量:5

3张玉玺,孙继朝,黄冠星,刘景涛,荆继红,向小平,陈玺,王金翠,崔海炜.珠江三角洲地区浅层地下水铍的分布及成因探讨[J].中国地质,2011,38(1):197-203. 被引量:6

4孙芳,孙卫玲.曝气生物滤池处理高氨氮含铍废水研究[J].环境科学与技术,2012,35(4):153-157. 被引量:7

5刘珍珍,刘勇,刘牡丹.溶剂萃取法从含铍溶液中分离铍[J].有色金属:冶炼部分,2012(5):37-39. 被引量:2

6彭明生,刘晓文,刘羽,杨志军.工艺矿物学近十年的主要进展[J].矿物岩石地球化学通报,2012,31(3):210-217. 被引量:65

7高诗佳,白峰.硅铍石的包裹体及其形成条件研究[J].岩石矿物学杂志,2013,32(2):180-188.

8肖超,李婕,吴海国.硫酸法提取铍工艺中铝杂质分离的研究现状[J].稀有金属与硬质合金,2013,41(3):8-10. 被引量:3

9刘爽,鲁力,柳德华,康健,黄鹏.我国稀有及稀散金属综合利用技术综述[J].矿产综合利用,2013(5):10-12. 被引量:6

10毕献武,董少花.我国矿产资源高效清洁利用进展与展望[J].矿物岩石地球化学通报,2014,33(1):14-22. 被引量:25

1刘世友.美国铍工业应用现状与展望[J].有色金属与稀土应用,1998(1):31-34. 被引量:1

2刘世友.美国铍工业概况[J].上海有色金属,1999,20(1):30-35. 被引量:7

3孟斌.铍[J].有色与稀有金属国外动态,1997(12):18-19.

4田春霞.铍[J].有色与稀有金属国外动态,1998(12):11-13.

5刘世友.日本铍工业生产、应用与展望[J].有色矿冶,1999,15(2):60-62. 被引量:5

6郭景阳.铍铜工业近况[J].上海金属:有色分册,1989,10(3):47-52. 被引量:3

7孟斌.铍[J].有色与稀有金属国外动态,1995(12):15-16.

8李复民,赖声伟.铍工业进展[J].上海金属:有色分册,1989,10(2):41-46.

9杨守春.铍[J].现代材料动态,2004(12):13-13.

10李子全.铍2001年需求降低[J].现代材料动态,2002(6):18-18.

Basic Information:

DOI:

Chinese Library Classification Number:F416.32[经济管理—产业经济]

Citation Information:

The article introduces the distribution of mineral resource and reserve of beryllium and present status of Be production of main manufacturers in the world. It describes in details theapplication and development of Be-metal、Be-Cu、Be-alloys and Be-oxides in all the fields. Finally it analyzes and forecasts the supply and demand of Be up to 2000 year.

quote

GB/T 7714-2015 [1] LIU Shi-you. Present Status of Beryllium Production and its Development and Application[J]. Rare Metals and Cemented Carbides, 1998(4): 56-61.
MLA [1] LIU Shi-you. "Present Status of Beryllium Production and its Development and Application." Rare Metals and Cemented Carbides, no. 4, 1998, pp. 56-61.
APA [1] LIU Shi-you. (1998). Present Status of Beryllium Production and its Development and Application. Rare Metals and Cemented Carbides(4), 56-61.
IEEE [1] LIU Shi-you, "Present Status of Beryllium Production and its Development and Application," Rare Metals and Cemented Carbides, no. 4, pp. 56-61, 1998. keywords: {beryllium industry, mineral resource production status, application and development market demand}