daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of Substituents with the Different Electron-Donating Abilities on Optoelectronic Properties of Bipolar Thioxanthone Derivatives Effect of Substituents with the Different Electron-Donating Abilities on Optoelectronic Properties of Bipolar Thioxanthone Derivatives AITranslate

Kaunas University of Technology; Kaunas University of Technology; Kaunas University of Technology; Kaunas University of Technology; Kaunas University of Technology; Kaunas University of Technology; Kaunas University of Technology;Department of Organic Chemistry, Center for Physical Sciences and Technology;Department of Organic Chemistry, Center for Physical Sciences and Technology; Kaunas University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The synthesis and optoelectronic properties of four simple-structure thioxanthone derivatives employing thioxanthone as an acceptor unit, coupled with moieties having very different electron-donating abilities such as phenoxazine, 3,6-di-tert-butylcarbazole, 3,7-di-tert-butylphenothiazine, or 2,7-di-tert-butyl-9,9-dimethylacridane, are reported. The compounds form molecular glasses with glass transition temperatures reaching 116 °C. Ionization potentials of the compounds estimated by photoelectron emission method range from 5.42 to 5.74 eV. Thioxanthone derivatives containing 3,6-tert-butylcarbazole or 2,7-di-tert-butyl-9,9-dimethylacridane moieties with weak electron-donating strengths were characterized by bipolar charge transport with relatively close hole and electron mobility values of 6.8 × 10–5/2.4 × 10–5 and 3.1 × 10–5/4.6 × 10–6 cm2/(V s) recorded at 3.6 × 105 V/cm. The other compounds demonstrated hole-transporting properties. The films of thioxanthones containing phenoxazine or 2,7-di-tert-butyl-9,9-dimethylacridane moieties showed efficient thermally activated delayed fluorescence with a photoluminescence quantum yield of up to 50% due to the solid-state luminescence enhancement. Organic-light-emitting diodes containing the synthesized compounds as emitters showed very different external quantum efficiencies (0.9–10.3%) and blue, sky blue, green, or yellow electroluminescence colors, thus reflecting the effects of donor substituents.

KeyWords AITranslate

thioxanthone carbazole phenothiazine acridane solidstate luminescence enhancement thermally activated delayed fluorescenceShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00092

Chinese Library Classification Number:

Citation Information:

The synthesis and optoelectronic properties of four simple-structure thioxanthone derivatives employing thioxanthone as an acceptor unit, coupled with moieties having very different electron-donating abilities such as phenoxazine, 3,6-di-tert-butylcarbazole, 3,7-di-tert-butylphenothiazine, or 2,7-di-tert-butyl-9,9-dimethylacridane, are reported. The compounds form molecular glasses with glass transition temperatures reaching 116 °C. Ionization potentials of the compounds estimated by photoelectron emission method range from 5.42 to 5.74 eV. Thioxanthone derivatives containing 3,6-tert-butylcarbazole or 2,7-di-tert-butyl-9,9-dimethylacridane moieties with weak electron-donating strengths were characterized by bipolar charge transport with relatively close hole and electron mobility values of 6.8 × 10–5/2.4 × 10–5 and 3.1 × 10–5/4.6 × 10–6 cm2/(V s) recorded at 3.6 × 105 V/cm. The other compounds demonstrated hole-transporting properties. The films of thioxanthones containing phenoxazine or 2,7-di-tert-butyl-9,9-dimethylacridane moieties showed efficient thermally activated delayed fluorescence with a photoluminescence quantum yield of up to 50% due to the solid-state luminescence enhancement. Organic-light-emitting diodes containing the synthesized compounds as emitters showed very different external quantum efficiencies (0.9–10.3%) and blue, sky blue, green, or yellow electroluminescence colors, thus reflecting the effects of donor substituents.

quote

GB/T 7714-2015 [1] Simas Macionis, Dalius Gudeika, Dmytro Volyniuk, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00092.
MLA [1] Simas Macionis, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00092.
APA [1] Simas Macionis, Dalius Gudeika, Dmytro Volyniuk, Malek Mahmoudi, Jurate Simokaitiene, Viktorija Andruleviciene, Murad Najafov, Rita Sadzeviciene, Sigitas Stoncius, & Juozas V. Grazulevicius. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00092
IEEE [1] Simas Macionis, Dalius Gudeika, Dmytro Volyniuk, Malek Mahmoudi, Jurate Simokaitiene, Viktorija Andruleviciene, Murad Najafov, Rita Sadzeviciene, Sigitas Stoncius, and Juozas V. Grazulevicius, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00092. keywords: {thioxanthone carbazole phenothiazine acridane solidstate luminescence enhancement thermally activated delayed fluorescenceShow More}