Ferromagnetic Cobalt Disulfide: A CVD Pathway Toward High-Quality and Phase-Pure Thin Films Ferromagnetic Cobalt Disulfide: A CVD Pathway Toward High-Quality and Phase-Pure Thin Films AITranslate
Abstract AITranslate
Pyrite-type cobalt disulfide (CoS2), which is one among other stable cobalt sulfide phases, exhibits interesting electronic and magnetic properties. Herein, we demonstrate a tailored metalorganic chemical vapor deposition (MOCVD) pathway for the growth of high-quality ferromagnetic CoS2 thin films. The influence of CVD process parameters on growth and quality of the films was investigated by complementary analyses. Superconducting quantum interference device (SQUID) measurements confirmed the existence of pure CoS2 with a magnetic moment of 0.85 μB and a Curie temperature of 128(5) K. Our findings could pave the way for large-area CoS2 to be used for different technological applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00685
Chinese Library Classification Number:
Citation Information:
Pyrite-type cobalt disulfide (CoS2), which is one among other stable cobalt sulfide phases, exhibits interesting electronic and magnetic properties. Herein, we demonstrate a tailored metalorganic chemical vapor deposition (MOCVD) pathway for the growth of high-quality ferromagnetic CoS2 thin films. The influence of CVD process parameters on growth and quality of the films was investigated by complementary analyses. Superconducting quantum interference device (SQUID) measurements confirmed the existence of pure CoS2 with a magnetic moment of 0.85 μB and a Curie temperature of 128(5) K. Our findings could pave the way for large-area CoS2 to be used for different technological applications.
quote
| GB/T 7714-2015 | [1] JanLucas Wree, JeanPierre Glauber, David Zanders, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00685. |
| MLA | [1] JanLucas Wree, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00685. |
| APA | [1] JanLucas Wree, JeanPierre Glauber, David Zanders, Detlef Rogalla, Malte Becher, Matthew B. E. Griffiths, Andreas Ostendorf, Seán T. Barry, Andreas Ney, & Anjana Devi. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00685 |
| IEEE | [1] JanLucas Wree, JeanPierre Glauber, David Zanders, Detlef Rogalla, Malte Becher, Matthew B. E. Griffiths, Andreas Ostendorf, Seán T. Barry, Andreas Ney, and Anjana Devi, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00685. keywords: {Cobalt disulfide MOCVD Raman spectroscopy SQUID ferromagnetism} |