Controlled Growth of Semiconductor Alloy/Ferromagnetic Insulator (GeBi/Bi:Thulium Iron Garnet (TmIG)) Spin Heterojunction and Development of Quantum Logic Device Controlled Growth of Semiconductor Alloy/Ferromagnetic Insulator (GeBi/Bi:Thulium Iron Garnet (TmIG)) Spin Heterojunction and Development of Quantum Logic Device AITranslate
Abstract AITranslate
Replacing heavy metal and heavy metal alloy films with a semiconductor thin film, to form a semiconductor/ferromagnetic insulator spin heterojunction has always been an international research hotspot. This article reports on a Ge1–xBix/Bi:thulium iron garnet (TmIG) spin heterojunction. It was found that Ge1–xBix (x = 0.06–0.22) semiconductor alloy films and Bi3+-doped control Tm3–yBiyFe4.3Ga0.7O12 (Bi:TmIG, y = 0.2–1.0) films can enhance the spin–orbit coupling (SOC) strength, improving the abnormal spin Hall effect (ASHE) and the spin Hall magnetoresistance (RH) switch characteristics. As x varies from 0.06 to 0.22, it is noticed that the spin mixing conductance considerably increases. Because Bi ions have the ability to control the SOC strength, the 5–10 nm GeBi semiconductor thin film with the Bi-ion-doped Bi:TmIG film can realize a spin magnetic moment reversal and then drive the heterojunction magnetic moment switching effect, and the spin currents injected across this interface lead to deterministic magnetization reversal at an ultralow current density of 1.82 × 106 mA/cm2. This has significant practical applications in the design and implementation of spin quantum logic devices based on semiconductor processes, laying a material foundation for the development of quantum logic devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00413
Chinese Library Classification Number:
Citation Information:
Replacing heavy metal and heavy metal alloy films with a semiconductor thin film, to form a semiconductor/ferromagnetic insulator spin heterojunction has always been an international research hotspot. This article reports on a Ge1–xBix/Bi:thulium iron garnet (TmIG) spin heterojunction. It was found that Ge1–xBix (x = 0.06–0.22) semiconductor alloy films and Bi3+-doped control Tm3–yBiyFe4.3Ga0.7O12 (Bi:TmIG, y = 0.2–1.0) films can enhance the spin–orbit coupling (SOC) strength, improving the abnormal spin Hall effect (ASHE) and the spin Hall magnetoresistance (RH) switch characteristics. As x varies from 0.06 to 0.22, it is noticed that the spin mixing conductance considerably increases. Because Bi ions have the ability to control the SOC strength, the 5–10 nm GeBi semiconductor thin film with the Bi-ion-doped Bi:TmIG film can realize a spin magnetic moment reversal and then drive the heterojunction magnetic moment switching effect, and the spin currents injected across this interface lead to deterministic magnetization reversal at an ultralow current density of 1.82 × 106 mA/cm2. This has significant practical applications in the design and implementation of spin quantum logic devices based on semiconductor processes, laying a material foundation for the development of quantum logic devices.
quote
| GB/T 7714-2015 | [1] Shuaicheng Liu, Lichuan Jin, Qinghui Yang, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00413. |
| MLA | [1] Shuaicheng Liu, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00413. |
| APA | [1] Shuaicheng Liu, Lichuan Jin, Qinghui Yang, Xiangrong Wang, Dainan Zhang, & Huaiwu Zhang. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00413 |
| IEEE | [1] Shuaicheng Liu, Lichuan Jin, Qinghui Yang, Xiangrong Wang, Dainan Zhang, and Huaiwu Zhang, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00413. keywords: {Spin heterojunction liquid phase epitaxial garnet thin films anomalous spin Hall effect spin wave device nonmagnetic metal/ferromagnetic insulator} |