New Pulping and Scrubbing Equipment for Defluorination From Nb_2O_5 AITranslate
Abstract AITranslate
A new pulping and scrubbing unit for removal of fluorine ion impurity from Nb2O5 is recommended and described. By comparision with traditional open unit, tins equipment has the advantages of lower energy consumption, faster pulping and scrubbing, lower labour omtemsoty and much less repairing work. It can also be used for scrubbing operation in hydrometallurgy.
KeyWords AITranslate
1王青芬,张建辉.大型矿浆调浆搅拌槽的设计及工业应用[J].有色金属:选矿部分,2013(6):73-76. 被引量:8
2李济华,王新有.用工业硫酸作反铌液制取生产铌铁用的氢氧化铌试验研究[J].稀有金属与硬质合金,1991(3):13-14.
3李玲玲.低成本生产烧结钼粉的方法[J].中国钨业,1995,0(10):29-29.
4张新振.焙烧氰化冶炼系统银浸出试验研究[J].中国有色冶金,2015,44(3):71-74. 被引量:1
5曾宪明,唐德胜.微波技术在氢氧化铌干燥中的应用[J].稀有金属与硬质合金,2012,40(1):55-58.
6难浸金精矿的生物氧化——硫脲树脂矿浆法提金工艺[J].黄金科学技术,2006,14(1):9-9.
7付晨晓.刚果(金)某铜钴矿浸钴实验研究[J].才智,2013,0(12):312-313. 被引量:3
8李海涛,范红卫.刚果(金)MKM铜钴采冶工程基于物料平衡的逆流洗涤自动控制系统[J].有色金属工程,2014,4(2):73-75. 被引量:1
9叶跃威,杨建国.用锌粉从高铜铅含氰贵液中置换金银[J].湿法冶金,2007,26(3):150-153. 被引量:11
10张阳,王辉,王华鹏,肖围.从铜精炼炉渣中常压选择性浸出钴的研究[J].昆明理工大学学报:理工版,2009,34(5):14-17. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.602[冶金工程—有色金属冶金]
Citation Information:
A new pulping and scrubbing unit for removal of fluorine ion impurity from Nb2O5 is recommended and described. By comparision with traditional open unit, tins equipment has the advantages of lower energy consumption, faster pulping and scrubbing, lower labour omtemsoty and much less repairing work. It can also be used for scrubbing operation in hydrometallurgy.
quote
| GB/T 7714-2015 | [1] HU Yi-qing, ZHANG Yao-hua, XIAO Cheng-xi. New Pulping and Scrubbing Equipment for Defluorination From Nb_2O_5[J]. Rare Metals and Cemented Carbides, 1995(4): 29-33. |
| MLA | [1] HU Yi-qing, et al., "New Pulping and Scrubbing Equipment for Defluorination From Nb_2O_5." Rare Metals and Cemented Carbides, no. 4, 1995, pp. 29-33. |
| APA | [1] HU Yi-qing, ZHANG Yao-hua, & XIAO Cheng-xi. (1995). New Pulping and Scrubbing Equipment for Defluorination From Nb_2O_5. Rare Metals and Cemented Carbides(4), 29-33. |
| IEEE | [1] HU Yi-qing, ZHANG Yao-hua, and XIAO Cheng-xi, "New Pulping and Scrubbing Equipment for Defluorination From Nb_2O_5," Rare Metals and Cemented Carbides, no. 4, pp. 29-33, 1995. keywords: {fluorine ion, cyclone, pulping and scrubbing equipment} |